公开(公告)号:US10457836B2
公开(公告)日:2019-10-29
申请号:US15895643
申请日:2018-02-13
Applicant: Motorola Mobility LLC
Inventor: Richard W. Brotzman , Ernest Sirois , Deborah Paskiewicz
IPC: C09D183/04 , H05K1/18 , C09D183/08 , H05K3/28 , C08G77/24 , C08G77/00
Abstract: A polysiloxane film comprises Si—O bonds and has a thickness of 0.3 to 1.5 microns. Adjacent electrodes coated with the polysiloxane film have a leakage current of at most 0.01 mA at 10 V after contact with water. An electrode coated with the polysiloxane film has a contact resistance of at least 0.01 ohms at 1.0 mm of pogo pin compression under a 1.0 N load. The polysiloxane film provides IPx7 protection from ingress of water.
-
公开(公告)号:US20180171176A1
公开(公告)日:2018-06-21
申请号:US15895643
申请日:2018-02-13
Applicant: Motorola Mobility LLC
Inventor: Richard W. Brotzman , Ernest Sirois , Deborah Paskiewicz
IPC: C09D183/04 , H05K1/18
CPC classification number: C09D183/04 , C08G77/24 , C08G77/80 , C09D183/08 , H05K1/18 , H05K3/282 , H05K3/285 , H05K2201/0162 , H05K2201/09872 , H05K2201/10015 , H05K2201/10022 , H05K2203/095
Abstract: A polysiloxane film comprises Si—O bonds and has a thickness of 0.3 to 1.5 microns. Adjacent electrodes coated with the polysiloxane film have a leakage current of at most 0.01 mA at 10 V after contact with water. An electrode coated with the polysiloxane film has a contact resistance of at least 0.01 ohms at 1.0 mm of pogo pin compression under a 1.0 N load. The polysiloxane film provides IPx7 protection from ingress of water.
-
公开(公告)号:US20170257950A1
公开(公告)日:2017-09-07
申请号:US15059682
申请日:2016-03-03
Applicant: Motorola Mobility LLC
Inventor: Richard W. Brotzman , Ernest Sirois , Deborah Paskiewicz
IPC: H05K3/28 , C23C16/505 , B05D1/00 , C09D183/04
CPC classification number: H05K3/28 , B05D1/62 , B05D5/08 , C08G77/24 , C08G77/80 , C09D183/04 , C09D183/08 , C23C16/30 , C23C16/505 , H05K3/281
Abstract: A method of forming a polysiloxane film on a substrate comprises polymerizing a siloxane monomer in a reaction chamber containing the substrate. The polymerization is catalyzed by a 30-60 W radio frequency plasma, the pressure in the reaction chamber during the polymerization is 100-400 mTorr, the residence time of the siloxane monomer in the reaction chamber is 5-120 minutes, the siloxane monomer is heated to 30-200° C. before entering the reaction chamber, and the polymerization is carried out at a temperature of 30-100° C.
-
公开(公告)号:US20170358771A1
公开(公告)日:2017-12-14
申请号:US15181722
申请日:2016-06-14
Applicant: Motorola Mobility LLC
Inventor: Richard W. Brotzman , Ernest Sirois , Daniel Thorstenson
Abstract: A dispersion comprised of at least 49 wt % of additive particles, a polymerizable monomer, a dispersant and a solvent. Upon polymerization the dispersion forms a hard coat with a haze of at most 0.5% and a transmission of at least 90%. A hard coat comprises at least 49 wt % of additive particles dispersed in a polymer. A method of making a hard coat comprises forming a dispersion, applying the dispersion to one side of a substrate, and polymerizing the dispersion. The hard coat has a haze of at most 0.5% and a transmission of at least 90%.
-
公开(公告)号:US20170253765A1
公开(公告)日:2017-09-07
申请号:US15059665
申请日:2016-03-03
Applicant: Motorola Mobility LLC
Inventor: Richard W. Brotzman , Ernest Sirois , Deborah Paskiewicz
IPC: C09D183/04 , H05K1/18
CPC classification number: C09D183/04 , C08G77/24 , C08G77/80 , C09D183/08 , H05K1/18 , H05K3/282 , H05K3/285 , H05K2201/0162 , H05K2201/09872 , H05K2201/10015 , H05K2201/10022 , H05K2203/095
Abstract: A polysiloxane film comprises Si—O bonds and has a thickness of 0.3 to 1.5 microns. Adjacent electrodes coated with the polysiloxane film have a leakage current of at most 0.01 mA at 10 V after contact with water. An electrode coated with the polysiloxane film has a contact resistance of at least 0.01 ohms at 1.0 mm of pogo pin compression under a 1.0 N load. The polysiloxane film provides IPx7 protection from ingress of water.
-
-
-
-