Abstract:
A dielectric ceramic composition that contains, as its main constituent, (Ba1-x-yCaxSry)(Ti1-z-wZrzHfw)O3 (in the formula, 0≦x+y≦0.2, 0≦z+w≦0.1), and contains CuO and Bi2O3, and the dielectric ceramic composition has a feature that the total content of the CuO and Bi2O3 is 10 parts by weight or more with respect to 100 parts by weight of the main constituent, and the molar ratio CuO/(CuO+Bi2O3) is 0.5 or less.
Abstract translation:作为其主要成分的(Ba1-x-yCaxSry)(Ti1-z-wZrzHfw)O3(式中,0< nlE; x + y≦̸ 0.2,0≦̸ z + w≦̸ 0.1)的电介质陶瓷组合物, 含有CuO和Bi2O3,电介质陶瓷组合物的特征在于,相对于主要成分为100重量份,CuO和Bi 2 O 3的总含量为10重量份以上,CuO /(CuO + Bi2O3)为0.5以下。
Abstract:
A dielectric ceramic composition that contains, as its main constituent, (Ba1-x-yCaxSry)(Ti1-z-wZrzHfw)O3 (in the formula, 0≦x+y≦0.2, 0≦z+w≦0.1), and contains CuO and Bi2O3, and the dielectric ceramic composition has a feature that the total content of the CuO and Bi2O3 is 10 parts by weight or more with respect to 100 parts by weight of the main constituent, and the molar ratio CuO/(CuO+Bi2O3) is 0.5 or less.
Abstract translation:作为其主要成分的(Ba1-x-yCaxSry)(Ti1-z-wZrzHfw)O3(式中,0 @ x + y @ 0.2,0 @ z + w @ 0.1)的电介质陶瓷组合物和 含有CuO和Bi2O3,电介质陶瓷组合物的特征在于,相对于主要成分为100重量份,CuO和Bi 2 O 3的总含量为10重量份以上,CuO /(CuO + Bi2O3)为0.5以下。
Abstract:
A three-terminal capacitor includes a main body having a cylindrical or substantially cylindrical shape extending in a first direction and including first and second inner electrodes alternately laminated together with dielectric layers interposed therebetween, a pair of first outer electrodes on two end surfaces of the main body in the first direction and electrically connected to the first inner electrodes, and a second outer electrode electrically connected to the second inner electrodes. The main body includes a projecting portion projecting in a direction perpendicular or substantially perpendicular to the first direction at a position between the pair of first outer electrodes. The second outer electrode is provided on one surface of the projecting portion viewable when viewed in the first direction.
Abstract:
A dielectric ceramic that can be sintered at a sufficiently low temperature and has a desired specific resistance at a high temperature, and a multilayer ceramic electronic component (a multilayer ceramic capacitor and the like) using the dielectric ceramic are provided. The multilayer ceramic capacitor includes a multilayer body having a plurality of laminated dielectric ceramic layers, and a plurality of internal electrodes at interfaces between the dielectric ceramic layers; and external electrodes 8 and 9 on outer surfaces of the multilayer body. The composition of the multilayer body includes a perovskite-type compound containing Ba and Ti (where a part of Ba may be substituted by Ca, and a part of Ti may be substituted by Zr) as a primary ingredient, and further includes M (where M is at least one of Cu, Zn, Li, K, and Na) and Bi. The total content of M and Bi is equal to or greater than 3 molar parts when the total content of Ti and Zr is 100 molar parts. The crystal particle size of the dielectric ceramic is 30 nm or more and 150 nm or less.
Abstract:
A dielectric ceramic enabling low-temperature firing and exhibiting good dielectric characteristics, and a stack ceramic electronic component using the same are provided. The dielectric ceramic containing (Ba1-x-yCaxSry)m(Ti1-zZrz)O3 (1.005≦m≦1.2, 0≦x+y≦0.2, and 0≦z≦0.2) as a major component and an amount of Bi relative to 100 parts by mol of the major component which is 1.0 part by mol or more and 40 parts by mol or less.
Abstract translation:提供能够进行低温烧制并且具有良好的介电特性的电介质陶瓷,以及使用其的叠层陶瓷电子元件。 含有(Ba1-x-yCaxSry)m(Ti1-zZrz)O3(1.005 @ m @ 1.2,0 @ x + y @ 0.2和0 @ z @ 0.2)作为主要成分的电介质陶瓷和Bi相对量 至100摩尔份的主成分为1.0摩尔%以上且40摩尔份以下。
Abstract:
A dielectric ceramic that can be sintered at a sufficiently low temperature and has a desired specific resistance at a high temperature, and a multilayer ceramic electronic component (a multilayer ceramic capacitor and the like) using the dielectric ceramic are provided. The multilayer ceramic capacitor includes a multilayer body having a plurality of laminated dielectric ceramic layers, and a plurality of internal electrodes at interfaces between the dielectric ceramic layers; and external electrodes 8 and 9 on outer surfaces of the multilayer body. The composition of the multilayer body includes a perovskite-type compound containing Ba and Ti (where a part of Ba may be substituted by Ca, and a part of Ti may be substituted by Zr) as a primary ingredient, and further includes M (where M is at least one of Cu, Zn, Li, K, and Na) and Bi. The total content of M and Bi is equal to or greater than 3 molar parts when the total content of Ti and Zr is 100 molar parts. The crystal particle size of the dielectric ceramic is 30 nm or more and 150 nm or less.
Abstract:
A dielectric ceramic enabling low-temperature firing and exhibiting good dielectric characteristics, and a stack ceramic electronic component using the same are provided. The dielectric ceramic containing (Ba1-x-yCaxSry)m(Ti1-zZrz)O3 (1.005≦m≦1.2, 0≦x+y≦0.2, and 0≦z≦0.2) as a major component and an amount of Bi relative to 100 parts by mol of the major component which is 1.0 part by mol or more and 40 parts by mol or less.