公开(公告)号:US12116466B2
公开(公告)日:2024-10-15
申请号:US17605095
申请日:2020-04-22
Inventor: Katsuyoshi Takeshita , Hideyuki Wakiyasu , Tomohiro Ito , Tomonori Miyamoto , Masayoshi Tokuda
IPC: C08J7/04 , B05D1/00 , B05D3/10 , B05D5/08 , C03C17/34 , C09D183/04 , G02B1/111 , G02B1/14 , G02B1/18
CPC classification number: C08J7/042 , B05D1/60 , B05D3/10 , B05D5/086 , C03C17/3405 , C09D183/04 , G02B1/111 , G02B1/14 , G02B1/18 , B05D2203/35 , B05D2506/10 , B05D2518/10 , C03C2217/73
Abstract: An object of the present invention is to provide a laminate which has a substrate, an intermediate layer, and a water-repellent layer laminated in this order, and has excellent abrasion resistance. The present invention is a laminate comprising: a substrate (s) having an anti-reflection layer; an intermediate layer (c) placed on the anti-reflection layer side of the substrate; and a water-repellent layer (r), in this order, wherein the intermediate layer (c) is a cured layer of a mixture composition (cc) of an organosilicon compound (C), or a vapor deposition layer of the organosilicon compound (C), the organosilicon compound (C) contains a silicon atom together with an amino group and/or an amine skeleton, the water-repellent layer (r) is a cured layer of a mixture composition (ca) of an organosilicon compound (A) in which a monovalent group having a perfluoropolyether structure is bound to a silicon atom through a linking group or without a linking group located therebetween, and a hydrolyzable group is bound to the silicon atom through a linking group or without a linking group located therebetween, and the laminate satisfies the following requirement (1),
(1) a water sliding angle is not larger than 50° after a abrasion resistance test in which a 200 g load per 1.5 cm×1.5 cm area is applied to a surface on the water-repellent layer (r) side of the laminate and the surface is rubbed 20,000 times.