Polyesters with low molecular weight additives for improved gas barrier properties
    3.
    发明授权
    Polyesters with low molecular weight additives for improved gas barrier properties 有权
    具有低分子量添加剂的聚酯以改善气体阻隔性能

    公开(公告)号:US08377530B2

    公开(公告)日:2013-02-19

    申请号:US13023184

    申请日:2011-02-08

    IPC分类号: B29D22/00 B29D23/00 B32B1/08

    摘要: Disclosed is a polyester polymer composition comprising at least one polyethylene terephthalate polyester in an amount ranging from 94.0 weight percent to 99.5 weight percent and at least one additive in an amount ranging from 0.5 weight percent to 6 weight percent, each based on the total weight of the polyester composition. The at least one additive comprises a diamide molecule. The composition of the present invention is useful in producing shaped articles such as, for example, sheeting, films, tubes, bottles, preforms, and profiles. These articles can exhibit improved gas barrier properties. The process for making the polymer composition and the shaped articles is also disclosed.

    摘要翻译: 公开了一种聚酯聚合物组合物,其包含至少一种量为94.0重量%至99.5重量%的聚对苯二甲酸乙二醇酯聚酯和至少一种量为0.5重量%至6重量%的添加剂,各自基于 聚酯组合物。 所述至少一种添加剂包含二酰胺分子。 本发明的组合物可用于制造成形制品,例如片材,薄膜,管,瓶,预成型件和型材。 这些制品可以表现出改进的阻气性能。 还公开了制备聚合物组合物和成型制品的方法。

    Non-precipitating alkali/alkaline earth metal and aluminum solutions made with polyhydroxyl ether solvents
    7.
    发明申请
    Non-precipitating alkali/alkaline earth metal and aluminum solutions made with polyhydroxyl ether solvents 有权
    用多羟基醚溶剂制成的非沉淀碱/碱土金属和铝溶液

    公开(公告)号:US20080027208A1

    公开(公告)日:2008-01-31

    申请号:US11495870

    申请日:2006-07-28

    IPC分类号: C08G63/00

    摘要: A stable catalyst solution suitable for catalyzing the polycondensation of reactants to make polyester polymers comprising: (i) M, wherein M is represented by an alkaline earth metal or alkali metal and (ii) aluminum metal and (iii) a polyhydroxyl ether solvent, wherein the molar ratio of M:Al ranges from 0.2:1 to 4:1 or less. The catalyst solution is desirably a solution which does not precipitate upon standing over a period of at least one week at room temperature (25° C.-40° C.), even at molar ratios of M:Al approaching 1:1. There is also provided a method for the manufacture of the solution, its feed to and use in the manufacture of a polyester polymer, and polyester polymers obtained by combining certain ingredients or containing the residues of these ingredients in the composition.

    摘要翻译: 一种稳定的催化剂溶液,其适用于催化反应物的缩聚以制备聚酯聚合物,其包含:(i)M,其中M由碱土金属或碱金属代表,和(ii)铝金属和(iii)多羟基醚溶剂,其中 M:Al的摩尔比范围为0.2:1至4:1或更低。 催化剂溶液理想地是即使在接近1:1的M:Al的摩尔比下,在室温(25℃-40℃)下在至少一周的时间内静置时也不沉淀的溶液。 还提供了一种用于制造溶液,其用于制造聚酯聚合物的原料和通过组合某些成分或将组合物中含有这些成分的残余物而获得的聚酯聚合物的方法。

    Non-precipitating alkali/alkaline earth metal and aluminum solutions made with polyhydroxyl ether solvents
    10.
    发明授权
    Non-precipitating alkali/alkaline earth metal and aluminum solutions made with polyhydroxyl ether solvents 有权
    用多羟基醚溶剂制成的非沉淀碱/碱土金属和铝溶液

    公开(公告)号:US07709595B2

    公开(公告)日:2010-05-04

    申请号:US11495870

    申请日:2006-07-28

    IPC分类号: C08G63/00 C08G64/02

    摘要: A stable catalyst solution suitable for catalyzing the polycondensation of reactants to make polyester polymers comprising: (i) M, wherein M is represented by an alkaline earth metal or alkali metal and (ii) aluminum metal and (iii) a polyhydroxyl ether solvent, wherein the molar ratio of M:Al ranges from 0.2:1 to 4:1 or less. The catalyst solution is desirably a solution which does not precipitate upon standing over a period of at least one week at room temperature (25° C.-40° C.), even at molar ratios of M:Al approaching 1:1. There is also provided a method for the manufacture of the solution, its feed to and use in the manufacture of a polyester polymer, and polyester polymers obtained by combining certain ingredients or containing the residues of these ingredients in the composition.

    摘要翻译: 一种稳定的催化剂溶液,其适用于催化反应物的缩聚以制备聚酯聚合物,其包含:(i)M,其中M由碱土金属或碱金属代表,和(ii)铝金属和(iii)多羟基醚溶剂,其中 M:Al的摩尔比范围为0.2:1至4:1或更低。 催化剂溶液理想地是即使在接近1:1的M:Al的摩尔比下,在室温(25℃-40℃)下在至少一周的时间内静置时也不沉淀的溶液。 还提供了一种用于制造溶液,其用于制造聚酯聚合物的原料和通过组合某些成分或将组合物中含有这些成分的残余物而获得的聚酯聚合物的方法。