摘要:
The present disclosure is directed to a plasticizer, polymeric compositions containing the plasticizer, and conductors coated with the polymeric composition. The plasticizer includes (i) an epoxidized fatty acid methyl ester, (ii) an epoxidized natural oil, and (iii) an epoxidized tallate ester. Polymeric compositions containing a polymeric resin and the plasticizer exhibit a weight loss less than 50 mg/cm2 after exposure to 100° C. for seven days. Conductors coated with the polymeric composition (containing the plasticizer) pass the low temperature unwind test of UL719 and exhibit a weight loss less than 50 mg/cm2 after exposure to 100° C. for seven days.
摘要翻译:本公开涉及含增塑剂的增塑剂,聚合物组合物和涂覆有聚合物组合物的导体。 增塑剂包括(i)环氧化脂肪酸甲酯,(ii)环氧化天然油,和(iii)环氧化的酯酸酯。 含有聚合物树脂和增塑剂的聚合物组合物在暴露于100℃下显示重量损失小于50mg / cm 2,持续7天。 用聚合物组合物(含增塑剂)涂覆的导体通过UL719的低温退火试验,并且在暴露于100℃下显示出低于50mg / cm 2的重量减少7天。
摘要:
The present disclosure is directed to a plasticizer, polymeric compositions containing the plasticizer, and conductors coated with the polymeric composition. The plasticizer includes (i) an epoxidized fatty acid methyl ester, (ii) an epoxidized natural oil, and (iii) an epoxidized tallate ester. Polymeric compositions containing a polymeric resin and the plasticizer exhibit a weight loss less than 50 mg/cm2 after exposure to 100° C. for seven days. Conductors coated with the polymeric composition (containing the plasticizer) pass the low temperature unwind test of UL719 and exhibit a weight loss less than 50 mg/cm2 after exposure to 100° C. for seven days.
摘要翻译:本公开涉及含增塑剂的增塑剂,聚合物组合物和涂覆有聚合物组合物的导体。 增塑剂包括(i)环氧化脂肪酸甲酯,(ii)环氧化天然油,和(iii)环氧化的酯酸酯。 含有聚合物树脂和增塑剂的聚合物组合物在暴露于100℃下显示重量损失小于50mg / cm 2,持续7天。 用聚合物组合物(含增塑剂)涂覆的导体通过UL719的低温退火试验,并且在暴露于100℃下显示出低于50mg / cm 2的重量减少7天。
摘要:
The disclosure is directed to a plasticizer system with improved electrical properties. The plasticizer system includes (a) a primary plasticizer consisting of an epoxidized vegetable oil and (b) a secondary plasticizer consisting of an epoxidized fatty acid ester, where the primary plasticizer is present in an amount greater than 50% by weight of the total plasticizer system weight.
摘要:
Processes for making a polyvinyl chloride (PVC) dry blend composition with a phthalate-free, bio-based plasticizer and filler, having a bulk density of greater than 0.67 g/cc and an extrusion rate of greater than 65 gm/minute for a single screw extruder of 0.75 in barrel diameter with a 25:1 L:D general purpose polyethylene screw at 75 rotations per minute screw speed, and compositions made by the processes are provided.
摘要:
Processes for making a polyvinyl chloride (PVC) dry blend composition with a phthalate-free, bio-based plasticizer and filler, having a bulk density of greater than 0.67 g/cc and an extrusion rate of greater than 65 gm/minute for a single screw extruder of 0.75 in barrel diameter with a 25:1 L:D general purpose polyethylene screw at 75 rotations per minute screw speed, and compositions made by the processes are provided.
摘要:
A composition comprising (A) at least one bisphenol-A polycarbonate resin, (B) at least one polypropylene, preferably a high crystallinity polypropylene, (C) at least one compatibilizer comprising an amine functionalized elastomeric polymer, (D) at least one organic phosphate flame retardant, preferably an organic phosphate that is liquid at room temperature, and, optionally, (E) one or more additives. These compositions are useful in the manufacture of wire insulation coatings of less than 0.2 mm with good scrape abrasion resistance.
摘要:
The present disclosure is directed to a halogen-free composition and conductors coated with the halogen-free composition. The halogen-free composition includes (A) from 70 wt % to 85 wt % of a polymeric component and (B) from 30 wt % to 15 wt % of a halogen-free flame retardant. The polymeric component (A) includes (i) a propylene homopolymer or a mini-random copolymer with greater than 40% crystallinity and (ii) an ethylene/a-olefin copolymer. The halogen-free composition has a density less than 1.15 g/cc. The halogen-free composition also has a scrape abrasion resistance of greater than or equal to 350 cycles as measured in accordance with ISO 6722.
摘要:
A composition comprising (A) at least one bisphenol-A polycarbonate resin, (B) at least one polypropylene, preferably a high crystallinity polypropylene, (C) at least one compatibilizer comprising an amine functionalized elastomeric polymer, (D) at least one organic phosphate flame retardant, preferably an organic phosphate that is liquid at room temperature, and, optionally, (E) one or more additives. These compositions are useful in the manufacture of wire insulation coatings of less than 0.2 mm with good scrape abrasion resistance.
摘要:
The present disclosure is directed to a halogen-free composition and conductors coated with the halogen-free composition. The halogen-free composition includes (A) from 70 wt % to 85 wt % of a polymeric component and (B) from 30 wt % to 15 wt % of a halogen-free flame retardant. The polymeric component (A) includes (i) a propylene homopolymer or a mini-random copolymer with greater than 40% crystallinity and (ii) an ethylene/α-olefin copolymer. The halogen-free composition has a density less than 1.15 g/cc. The halogen-free composition also has a scrape abrasion resistance of greater than or equal to 350 cycles as measured in accordance with ISO 6722.