Aluminum-lithium alloys having improved corrosion resistance containing
Mg and Zn
    1.
    发明授权
    Aluminum-lithium alloys having improved corrosion resistance containing Mg and Zn 失效
    含有Mg和Zn的具有改善的耐腐蚀性的铝 - 锂合金

    公开(公告)号:US4961792A

    公开(公告)日:1990-10-09

    申请号:US172506

    申请日:1988-03-24

    摘要: An aluminum base alloy wrought product having improved corrosion resistance in addition to combinations of strength and toughness. The product comprises 0.2 to 5.0 wt. % Li, 0.05 to 6.0 wt. % Mg, at least 2.45 wt. % Cu, 0.05 to 0.16 wt. % Zr, 0.05 to 12 wt. % Zn, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities and has the ability to develop improved combinations of strength and toughness in response to an aging treatment. Prior to an aging step, the product having imparted thereto a working effect equivalent to stretching so that after an aging step it has improved combinations of strength and toughness.

    摘要翻译: 除了强度和韧性的组合之外,还具有改进的耐腐蚀性的铝基合金锻造产品。 该产品包含0.2至5.0wt。 %Li,0.05〜6.0重量% %Mg,至少2.45wt。 %Cu,0.05〜0.16wt。 %Zr,0.05〜12wt。 %Zn,0.5wt。 最大% Fe,0.5wt。 最大% Si,余量为铝和偶然杂质,并且具有响应于时效处理而改进的强度和韧性组合的能力。 在老化步骤之前,产品赋予其相当于拉伸的作用效果,使得在老化步骤之后,其具有改善的强度和韧性的组合。

    Aluminum-lithium alloys
    2.
    发明授权
    Aluminum-lithium alloys 失效
    铝 - 锂合金

    公开(公告)号:US4832910A

    公开(公告)日:1989-05-23

    申请号:US812386

    申请日:1985-12-23

    IPC分类号: C22C21/00

    CPC分类号: C22C21/00

    摘要: Disclosed is an aluminum-lithium alloy containing a predetermined amount of lanthanides which provides the alloy with an improved combination of strength and fracture toughness relative to a baseline alloy not containing lanthanides but otherwise having the alloy's composition.

    摘要翻译: 公开了含有预定量的镧系元素的铝 - 锂合金,其相对于不含镧系元素但具有合金组成的基础合金,提供了强度和断裂韧性的改进组合。

    Aluminum-lithium alloys with hafnium
    3.
    发明授权
    Aluminum-lithium alloys with hafnium 失效
    铝合金与铪

    公开(公告)号:US4869870A

    公开(公告)日:1989-09-26

    申请号:US172504

    申请日:1988-03-24

    摘要: An aluminum base alloy suitable for forming into a wrought product having improved combinations of strength and fracture toughness is provided. The alloy is comprised of 0.2 to 5.0 wt. % Li, 0.05 to 6.0 wt. % Mg, 0.2 to 5.0 wt. % Cu, 0 to 2.0 wt. % Mn, 0 to 1.0 wt. % Zr, 0.05 to 12.0 wt. % Zn, 0.05 to 1.0 wt. % Hf, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities.

    摘要翻译: 提供了一种适合于形成具有改善的强度和断裂韧性组合的锻造产品的铝基合金。 该合金由0.2〜5.0重量% %Li,0.05〜6.0重量% %Mg,0.2〜5.0wt。 %Cu,0〜2.0重量% %Mn,0〜1.0wt。 %Zr,0.05〜12.0重量% %Zn,0.05〜1.0wt。 %Hf,0.5wt。 最大% Fe,0.5wt。 最大% Si,余量为铝和杂质。

    Aluminum-lithium alloys and method
    5.
    发明授权
    Aluminum-lithium alloys and method 失效
    铝锂合金及方法

    公开(公告)号:US4648913A

    公开(公告)日:1987-03-10

    申请号:US594344

    申请日:1984-03-29

    IPC分类号: C22C21/00 C22F1/00 C22F1/04

    CPC分类号: C22C21/00 C22F1/04

    摘要: An aluminum base alloy wrought product suitable for aging and having the ability to develop improved strength in response to an aging treatment without impairing fracture toughness properties is disclosed. The product is comprised of 0.5 to 4.0 wt. % Li, 0 to 5.0 wt. % Mg, up to 5.0 wt. % Cu, 0 to 1.0 wt. % Zr, 0 to 2.0 wt. % Mn, 0 to 7.0 wt. % Zn, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities. The product has imparted thereto, prior to an aging step, a working effect equivalent to stretching an amount greater than 3% in order that, after said aging, improved strength and fracture toughness combinations are obtained.

    摘要翻译: 公开了一种适用于老化的铝基合金锻造产品,并且具有在不损害断裂韧性的情况下响应于时效处理而产生改进的强度的能力。 该产品由0.5至4.0wt。 %Li,0〜5.0wt。 %Mg,最高5.0wt。 %Cu,0〜1.0wt。 %Zr,0〜2.0重量% %Mn,0〜7.0wt。 %Zn,0.5wt。 最大% Fe,0.5wt。 最大% Si,余量为铝和杂质。 在老化步骤之前,赋予产品相当于拉伸量大于3%的工作效果,以便在老化后获得改进的强度和断裂韧性组合。

    Aluminum-lithium alloys having improved corrosion resistance
    6.
    发明授权
    Aluminum-lithium alloys having improved corrosion resistance 失效
    具有改善的耐腐蚀性的铝 - 锂合金

    公开(公告)号:US4897126A

    公开(公告)日:1990-01-30

    申请号:US213722

    申请日:1988-06-30

    IPC分类号: C22C21/00 C22F1/00 C22F1/04

    CPC分类号: C22C21/00 C22F1/04

    摘要: An aluminum base alloy wrought product having improved corrosion resistance in addition to combinations of strength and toughness. The product comprises 2.2 to 3.0 wt. % Li, 0.4 to 2.0 wt. % Mg, 0.2 to 1.6 wt. % Cu, 0 to 2.0 wt. % Mn, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities and has the ability to develop improved combinations of strength and toughness in response to an aging treatment. Prior to an aging step, the product having imparted thereto a working effect equivalent to stretching so that after an aging step it has improved combinations of strength and toughness.

    摘要翻译: 除了强度和韧性的组合之外,还具有改进的耐腐蚀性的铝基合金锻造产品。 该产品包含2.2至3.0wt。 %Li,0.4〜2.0wt。 %Mg,0.2〜1.6wt。 %Cu,0〜2.0重量% %Mn,0.5wt。 最大% Fe,0.5wt。 最大% Si,余量为铝和偶然杂质,并且具有响应于时效处理而改进的强度和韧性组合的能力。 在老化步骤之前,产品赋予其相当于拉伸的作用效果,使得在老化步骤之后,其具有改善的强度和韧性的组合。

    Superplastic aluminum products and alloys
    7.
    发明授权
    Superplastic aluminum products and alloys 失效
    超塑性铝制品和合金

    公开(公告)号:US5055257A

    公开(公告)日:1991-10-08

    申请号:US414872

    申请日:1989-09-29

    IPC分类号: C22F1/04 C22F1/047 C22F1/053

    CPC分类号: C22F1/053 C22F1/04 C22F1/047

    摘要: Superplastic forming of aluminum work stock is improved by including therein about 0.05% to about 10% or 15% scandium together with up to 0.2 or 0.25% zirconium. In preferred practices, soluble elements such as magnesium are also included in the aluminum alloy. One or more of the elements from the group of scandium, yttrium, gadolinium, holminum, dysprosium, erbium, ytterbium, lutetium, and terbium, may be included in addition to or in lieu of scandium. Heat treatable aluminum alloys such as 7XXX alloys and 2XXX alloys can be made superplastic by including scandium and zirconium to provide very high strength in superplastically formed products.

    摘要翻译: 通过在其中包括约0.05%至约10%或15%的钪以及至多0.2或0.25%的锆来改善铝工作原料的超塑性成形。 在优选的实践中,铝合金中也包括可溶性元素如镁。 钪,钇,钆,茂金属,镝,铒,镱,镥,铽等元素中的一种或多种元素可以包含在钪中,也可以代替钪。 可热处理的铝合金如7XXX合金和2XXX合金可以通过包括钪和锆在超塑性产品中提供非常高的强度而被制成超塑性。

    Superplastic aluminum products and alloys
    8.
    发明授权
    Superplastic aluminum products and alloys 失效
    超塑性铝制品和合金

    公开(公告)号:US4874440A

    公开(公告)日:1989-10-17

    申请号:US085851

    申请日:1987-08-14

    IPC分类号: C22F1/04 C22F1/047 C22F1/053

    摘要: Superplastic forming of aluminum work stock is improved by including therein about 0.05% to about 10% or 15% scandium. In preferred practices, soluble elements such as magnesium are also included in the aluminum alloy. One or more of the elements from the group of scandium, yttrium, gadolinium, holminum, dysprosium, erbium, ytterbium, lutetium, and terbium, may be included in addition to or in lieu of scandium.

    摘要翻译: 通过在其中包括约0.05%至约10%或15%的钪来改善铝制工件的超塑性成形。 在优选的实践中,铝合金中也包括可溶性元素如镁。 钪,钇,钆,茂金属,镝,铒,镱,镥,铽等元素中的一种或多种元素可以包含在钪中,也可以代替钪。

    Aluminum-lithium alloys having improved corrosion resistance and method
    9.
    发明授权
    Aluminum-lithium alloys having improved corrosion resistance and method 失效
    具有改善的耐腐蚀性和方法的铝 - 锂合金

    公开(公告)号:US4797165A

    公开(公告)日:1989-01-10

    申请号:US685731

    申请日:1984-12-24

    IPC分类号: C22C21/00 C22F1/00 C22F1/04

    CPC分类号: C22F1/04 C22C21/00

    摘要: An aluminum base alloy wrought product having improved corrosion resistance in addition to combinations of strength and toughness. The product comprises 2.2 to 3.0 wt. % Li, 0.4 to 2.0 wt. % Mg, 0.2 to 1.6 wt. % Cu, 0 to 2.0 wt. % Mn, 0.5 wt. % max. Fe, 0.5 wt. % max. Si, the balance aluminum and incidental impurities and has the ability to develop improved combinations of strength and toughness in response to an aging treatment. Prior to an aging step, the product having imparted thereto a working effect equivalent to stretching so that after an aging step it has improved combinations of strength and toughness.

    摘要翻译: 除了强度和韧性的组合之外,还具有改进的耐腐蚀性的铝基合金锻造产品。 该产品包含2.2至3.0wt。 %Li,0.4〜2.0wt。 %Mg,0.2〜1.6wt。 %Cu,0〜2.0重量% %Mn,0.5wt。 最大% Fe,0.5wt。 最大% Si,余量为铝和偶然杂质,并且具有响应于时效处理而改进的强度和韧性组合的能力。 在老化步骤之前,产品赋予其相当于拉伸的作用效果,使得在老化步骤之后,其具有改善的强度和韧性的组合。