Styrene resin and resin composition comprising the same
    1.
    发明授权
    Styrene resin and resin composition comprising the same 有权
    苯乙烯树脂及其组合物

    公开(公告)号:US06376605B1

    公开(公告)日:2002-04-23

    申请号:US09245065

    申请日:1999-02-05

    IPC分类号: C08F800

    摘要: A styrene resin is disclosed having excellent moldability and physical properties and is suited for recycling; and a thermoplastic polycarbonate composition with the styrene resin. The styrene resin contains 50 to 90 wt. % of a continuous phase component (S) composed of a copolymer of a styrene monomer, an unsaturated nitrile monomer; and 10 to 50 wt. % of a dispersed phase component on which said monomers have been grafted and which has occluded said copolymer. In the styrene resin, no triple chain unit AAA is detected from the unsaturated nitrite monomer component (A) in the continuous phase component (S) and a double chain unit AA amounts to 3% or less based on the whole units (A) detected.

    摘要翻译: 公开了具有优异的成型性和物理性能并且适于再循环的苯乙烯树脂; 和具有苯乙烯树脂的热塑性聚碳酸酯组合物。 苯乙烯树脂含有50〜90wt。 %的由苯乙烯单体,不饱和腈单体的共聚物组成的连续相组分(S) 和10〜50wt。 %的所述单体已经在其上接枝并且已经封闭所述共聚物的分散相组分。 在苯乙烯树脂中,连续相成分(S)中不饱和亚硝酸酯单体成分(A)不检测到三链单元AAA,双链单元AA相对于检测到的全部单元(A)为3%以下 。

    Method for removing volatile materials from a polymer composition
    2.
    发明授权
    Method for removing volatile materials from a polymer composition 失效
    从聚合物组合物中除去挥发性物质的方法

    公开(公告)号:US6124426A

    公开(公告)日:2000-09-26

    申请号:US160061

    申请日:1998-09-24

    IPC分类号: C08F6/00 C08F6/28

    CPC分类号: C08F6/28 C08F6/005

    摘要: A method for removing volatile materials, comprises adding a blowing aid to a polymer composition containing volatile materials, mixing them in a static mixing apparatus, and extruding the resultant mixture by an extruding apparatus into a devolatilizing tank, thereby the mixture is made to be blown, to cause removal of the volatile materials. First, the blowing aid (6) is discharged with an addition nozzle apparatus (2), in a direction opposite to the direction of the flow of the polymer composition (1), to be added, and the polymer composition is introduced into the static mixing apparatus (3), at a pressure at which the blowing does not take place, thereby mixing them. Then, using the extruding apparatus (11), the resultant mixture is extruded into the devolatilizing tank (4), so that the polymer is made into a blown product at such a temperature and a pressure that the blowing coefficient B is 1.4 or more, thereby causing the removal of volatile materials.B=A'/A Expression (1)wherein A represents the cross-sectional area of an extruding apparatus, and A' represents the average cross-sectional area of the polymer composition in a direction perpendicular to the vertical direction of the blown polymer composition, at a point where the polymer composition is dropped from the lower part of an opening section of the extruding apparatus vertically 50 cm to 1 m. The method can give a polymer composition having residual volatile materials in very small amounts, by removing volatile materials continuously with high efficiency.

    摘要翻译: 一种除去挥发性物质的方法,包括向含有挥发性物质的聚合物组合物中加入发泡助剂,将其混合在静态混合装置中,并通过挤出装置将所得混合物挤出到脱挥发分槽中,从而将混合物吹制 ,以除去挥发性物质。 首先,用添加喷嘴装置(2)沿着与聚合物组合物(1)的流动方向相反的方向排出吹塑助剂(6),并将聚合物组合物引入静态 混合装置(3)在不发生吹塑的压力下进行混合。 然后,使用挤出装置(11)将所得混合物挤出到脱挥发分槽(4)中,使得在吹塑系数B为1.4以上的温度和压力下将聚合物制成吹塑制品, 从而导致挥发性物质的去除。B = A'/ A表达式(1)其中A表示挤出装置的横截面积,A'表示聚合物组合物在垂直于...的方向上的平均横截面积 在聚合物组合物从挤出设备的开口部分的下部垂直延伸50cm至1μm的点处,吹塑聚合物组合物的垂直方向。 该方法可以通过以高效率连续除去挥发性物质,得到非常少的具有残留挥发性物质的聚合物组合物。

    Production process of ABS resin, ABS resin, and ABS-polycarbonate resin composition making use of the same
    3.
    发明授权
    Production process of ABS resin, ABS resin, and ABS-polycarbonate resin composition making use of the same 失效
    ABS树脂,ABS树脂和ABS-聚碳酸酯树脂组合物的生产工艺使用相同

    公开(公告)号:US06391965B1

    公开(公告)日:2002-05-21

    申请号:US08861657

    申请日:1997-05-22

    IPC分类号: C08F27904

    摘要: A process is disclosed for the continuous production of an ABS resin. The polymerization step comprises at least two substeps, one being a first-stage substep of forming particles of the rubbery polymer and the other a second-stage substep of adjusting the particle sizes of the particles. The first-stage substep is conducted in a polymerization system making use of a plug flow reactor or a batch polymerization reactor, and conducts polymerization at least until the particles are formed in the polymerization mixture. The second-stage substep increases a converted amount of the monomer component into the polymer compared with that in the particle forming substep and makes the particles smaller. A polycarbonate-ABS resin composition is also disclosed.

    摘要翻译: 公开了用于连续生产ABS树脂的方法。 聚合步骤包括至少两个子步骤,一个是形成橡胶状聚合物颗粒的第一阶段子步骤,另一个是调整颗粒的粒度的第二阶段子步骤。 第一级子步骤在使用活塞流反应器或间歇式聚合反应器的聚合系统中进行,并进行至少直至聚合混合物中形成颗粒的聚合。 第二级子步骤将单体组分转化成聚合物,与颗粒形成子步骤相比,使颗粒更小。 还公开了一种聚碳酸酯-ABS树脂组合物。

    Rubber dispersed copolymer resin
    4.
    发明授权
    Rubber dispersed copolymer resin 失效
    橡胶分散共聚树脂

    公开(公告)号:US4808661A

    公开(公告)日:1989-02-28

    申请号:US899867

    申请日:1986-08-25

    摘要: The invention provides a rubber dispersed copolymer resin having excellent heat resistance, impact strength and moldability and composed of (1) a dispersed phase formed of a rubbery polymer and copolymerized styrene-type, acrylonitrile-type and maleimide-type monomers, said rubbery polymer specifically controlled occluding the copolymer of monomers, being grafted with the copolymer and/or forming a multicomponent gel together with copolymers, and (2) a continuous phase formed at least of a specifically controlled copolymer of the styrenetype, acrylonitrile-type and maleimide-type monomers. The resin is useful as a molding material for electric appliances, electronic equipment and cars.

    摘要翻译: 本发明提供了具有优异的耐热性,冲击强度和成型性的橡胶分散共聚物树脂,它由(1)由橡胶状聚合物和共聚苯乙烯型丙烯腈 - 型马来酰亚胺型单体形成的分散相组成,所述橡胶状聚合物特别 控制阻塞共聚物与共聚物接枝和/或与共聚物一起形成多组分凝胶,和(2)至少形成苯乙烯类,丙烯腈型和马来酰亚胺型单体的特异性控制共聚物的连续相 。 该树脂可用作电器,电子设备和汽车的成型材料。

    Continuous bulk polymerization reactor
    5.
    发明授权
    Continuous bulk polymerization reactor 失效
    连续本体聚合反应器

    公开(公告)号:US4460278A

    公开(公告)日:1984-07-17

    申请号:US337765

    申请日:1982-01-07

    摘要: Disclosed is a continuous bulk polymerization reactor comprising a cylindrical reaction vessel elongated in the direction of the reacting fluid and a shaft installed within the reaction vessel. A plurality of flow of double helical-ribbon agitators are attached to the shaft in such a way that they face in the same direction, and a plurality of baffles having a relative open area of 5 to 40% based on the cross-sectional area of the internal space of the reaction vessel, are disposed between any adjacent ones of the agitators. Thus the formation of stagnant fluid pockets is avoided and excellent piston flow properties are achieved.

    摘要翻译: 公开了一种连续本体聚合反应器,其包括在反应流体的方向上延伸的圆柱形反应容器和安装在反应容器内的轴。 多个双螺旋带搅拌器的流动以这样的方式附接到轴上,使得它们面向相同的方向,并且多个挡板的相对开口面积为5至40%,基于横截面积 反应容器的内部空间设置在任何相邻的搅拌器之间。 因此避免了滞留流体袋的形成,并且实现了优异的活塞流动特性。

    Colored styrenic resin composition
    6.
    发明授权
    Colored styrenic resin composition 失效
    着色苯乙烯树脂组合物

    公开(公告)号:US5434204A

    公开(公告)日:1995-07-18

    申请号:US960766

    申请日:1992-10-14

    CPC分类号: C08K5/57

    摘要: A colored styrenic resin composition comprises 100 parts by weight of a styrenic resin, 0.1 to 5 parts by weight of titanium oxide and 0.05 to 2.5 parts by weight of an organo-tin compound and in which the amount of the organo-tin compound is not less than 10% by weight on the basis of the amount of the titanium oxide. The resin composition ensures the production of injection-molded articles free of black streaks and, therefore, the articles formed from the resin composition of the invention have high commercial value. The colored styrenic resin composition is useful as a material for the production of housings of, for example, a variety of electric appliances and office machinery and equipment as well as miscellaneous goods.

    摘要翻译: 有色苯乙烯树脂组合物包含100重量份苯乙烯树脂,0.1至5重量份氧化钛和0.05至2.5重量份有机锡化合物,其中有机锡化合物的量不是 基于氧化钛的量小于10重量%。 树脂组合物确保了没有黑色条纹的注塑制品的生产,因此,由本发明的树脂组合物形成的制品具有很高的商业价值。 有色苯乙烯树脂组合物可用作生产例如各种电器,办公机器和设备以及杂货的外壳的材料。

    Continuous process for preparing rubber modified high impact resin
    7.
    发明授权
    Continuous process for preparing rubber modified high impact resin 失效
    制备橡胶改性高冲击树脂的连续工艺

    公开(公告)号:US5210132A

    公开(公告)日:1993-05-11

    申请号:US961026

    申请日:1992-10-14

    IPC分类号: C08F279/02 C08F291/02

    CPC分类号: C08F291/02 C08F279/02

    摘要: A process for preparing rubber modified high impact resins by dissolving a rubbery polymer in a monomer containing an aromatic vinyl monomer or a mixture of an aromatic vinyl monomer and a vinyl cyanide monomer followed by polymerizing the monomer, the two steps being carried out in at least two polymerization reactors with a particle disperser placed between the first and second reactors. High impact resins having excellent surface properties are obtained with a savings in a power consumption by controlling:(1) the relationship between the concentration of the polymerized monomer and the content of the rubbery polymer in the first reactor;(2) the relationship between the volume occupied by the polymerizing liquid in the first reactor and the inner volume of the particle disperser; and(3) the peripheral linear velocity of a shearing stirrer in the particle disperser.

    摘要翻译: 通过将橡胶状聚合物溶解在含有芳族乙烯基单体或芳香族乙烯基单体和乙烯基氰单体的混合物的单体中,然后使单体聚合,制备橡胶改性的高冲击性树脂的方法,这两个步骤至少进行 两个具有放置在第一和第二反应器之间的分散器的聚合反应器。 通过控制:(1)聚合单体的浓度与第一反应器中橡胶状聚合物的含量之间的关系,可以节省功耗,获得具有优异表面性能的高冲击性树脂; (2)第一反应器中的聚合液体占据的体积与粒子分散器的内体积之间的关系; 和(3)粒子分散器中的剪切搅拌器的外围线速度。

    Quality control method for ABS-based resin and molding of the ABS-based
resin
    10.
    发明授权
    Quality control method for ABS-based resin and molding of the ABS-based resin 失效
    ABS基树脂的质量控制方法和ABS基树脂的成型

    公开(公告)号:US5552494A

    公开(公告)日:1996-09-03

    申请号:US361489

    申请日:1994-12-22

    摘要: A molding of an ABS-based resin is described. Rubber particles located at a depth of 0.5-1.5 .mu.m from a surface of the molding morphologically comprise at least the following two types of particles:(1) A particles having an a/b ratio not greater than 1.5, wherein a and b represent a major axis and a minor axis, respectively, and(2) B particles having an a/b ratio not smaller than 5, wherein a and b have the same meanings as defined abovewhen a section extending at the depth in parallel with the surface of the molding is observed in an electron micrograph taken by the ultrathin sectioning technique. Assuming that the total area of the rubber particles as observed in the electron micrograph is 100%, the total area of the A particles accounts for at least 10% and that of the B particles is in a range of 0.01-90%.