公开(公告)号:US20250066546A1
公开(公告)日:2025-02-27
申请号:US18724373
申请日:2022-12-20
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Keshavaraja Alive , Mark Erik Nelson
IPC: C08G63/91 , B29C48/00 , B29K267/00 , C08G63/183
Abstract: In an aspect, a method for reducing the molecular weight of a polyester, comprises mixing a composition comprising a polyester oligomer and a polyester in a molten state to form a modified polyester; wherein the mixing occurs at a temperature of 230 to 330° C.; wherein the polyester oligomer is present in an amount of 0.1 to 50 weight percent based on 5 the total weight of the composition; wherein the polyester comprises a C2-12 alkyl phthalate polyester having a weight average molecular weight, Mwi, of 15,000 to 100,000 g/mol determined using gel permeation chromatography based on polystyrene standards; and wherein the modified polyester has a weight average molecular weight, Mwf, of at least 5% less than the weight average molecular weight of the polyester.
-
公开(公告)号:US20190338071A1
公开(公告)日:2019-11-07
申请号:US16474616
申请日:2017-12-06
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Prashant Kumar , Husnu Alp Alidedeoglu , Keshavaraja Alive
IPC: C08G63/181 , C08G63/82 , B01J21/06
Abstract: The present invention relates to a process for the production of a thermoplastic polyester using a reaction mixture comprising a dicarboxylic acid having a melting temperature of ≥200° C. wherein the dicarboxylic acid is introduced to the process in the form of particles having an average particle diameter of ≥100 μm. Such process results in a reduction of the polymerisation time. Furthermore, it allows for the production of thermoplastic polyesters having a desired balance of intrinsic viscosity and carboxylic end group content at a reduced polymerisation time.
-
公开(公告)号:US20250059322A1
公开(公告)日:2025-02-20
申请号:US18724356
申请日:2022-12-19
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Keshavaraja Alive , Robert Russell Gallucci
IPC: C08G63/78 , C08G63/183 , C08J3/12 , C08J3/20 , C08K5/053
Abstract: In an aspect, a method for reducing the molecular weight of a polyester comprises extruding a composition comprising a chain scission agent and a polyester in a molten state to form a modified polyester. The chain scission agent can comprise a C2-12 diol and can be present in an amount of 0.1 to 5 weight percent based on the total weight of the composition. The polyester can comprise a C2-12 alkyl phthalate polyester having a weight average molecular weight, Mwi, of 15,000 to 100,000 g/mol based on polystyrene standards. The modified polyester can have a weight average molecular weight, Mwf, of at least 5% less than the weight average molecular weight of the polyester.
-
公开(公告)号:US11021570B2
公开(公告)日:2021-06-01
申请号:US16474616
申请日:2017-12-06
Applicant: SABIC GLOBAL TECHNOLOGIES B.V.
Inventor: Prashant Kumar , Husnu Alp Alidedeoglu , Keshavaraja Alive
IPC: C08G63/181 , B01J21/06 , C08G63/82
Abstract: The present invention relates to a process for the production of a thermoplastic polyester using a reaction mixture comprising a dicarboxylic acid having a melting temperature of ≥200° C. wherein the dicarboxylic acid is introduced to the process in the form of particles having an average particle diameter of ≥100 μm. Such process results in a reduction of the polymerisation time. Furthermore, it allows for the production of thermoplastic polyesters having a desired balance of intrinsic viscosity and carboxylic end group content at a reduced polymerisation time.
-
-
-