摘要:
Provided is a method of continuous production of a biodegradable aliphatic polyester including continuously performing an esterification reaction of a mixture including an aliphatic dihydroxy compound and aliphatic dicarboxylic acid at a temperature of 185° C. or less to obtain an ester; continuously performing a first polycondensation reaction of the ester to obtain a preliminary polymer; and continuously performing a polycondensation reaction of the preliminary polymer. According to the method of production, an amount of the aliphatic dihydroxy compound used decreases, which is a starting material, thereby decreasing the manufacturing cost of the biodegradable aliphatic polyester.
摘要:
Provided is a method of continuous production of a biodegradable aliphatic polyester including continuously performing an esterification reaction of a mixture including an aliphatic dihydroxy compound and aliphatic dicarboxylic acid at a temperature of 185° C. or less to obtain an ester; continuously performing a first polycondensation reaction of the ester to obtain a preliminary polymer; and continuously performing a polycondensation reaction of the preliminary polymer. According to the method of production, an amount of the aliphatic dihydroxy compound used decreases, which is a starting material, thereby decreasing the manufacturing cost of the biodegradable aliphatic polyester.
摘要:
Provided is a hard capsule. The provided hard capsule includes water-soluble cellulose ether, about 0.5 parts by weight to about 1.5 parts by weight of a gelation agent based on 100 parts by weight of the water-soluble cellulose ether, and about 0 parts by weight to about 0.3 parts by weight of a gelation aid based on 100 parts by weight of the water-soluble cellulose ether, wherein the hard capsule comprises a body and a cap that seals the body, and a ratio of a maximum thickness to a minimum thickness of the body and the cap is each 2.5 or less.
摘要:
Provided is a method of continuous preparation of a biodegradable aliphatic/aromatic polyester copolymer, the method including: performing a first esterification reaction of an aliphatic dihydroxy compound and an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product obtained by the first esterification reaction; obtaining a pre-polymer by continuously performing a first polycondensation reaction of a reaction product obtained by the second esterification reaction; and continuously performing polycondensation reaction of the pre-polymer, wherein an aromatic carboxylic acid is added to a reactor in which the first esterification reaction or the second esterification reaction is performed, to prepare the biodegradable aliphatic/aromatic polyester copolymer. According to the method of continuous preparation of the biodegradable aliphatic/aromatic polyester copolymer as described above, the amount of the aliphatic dihydroxy compound used, which is a starting material, is reduced and accordingly, manufacturing costs are reduced.
摘要:
Provided is a hard capsule. The provided hard capsule includes water-soluble cellulose ether, about 0.5 parts by weight to about 1.5 parts by weight of a gelation agent based on 100 parts by weight of the water-soluble cellulose ether, and about 0 parts by weight to about 0.3 parts by weight of a gelation aid based on 100 parts by weight of the water-soluble cellulose ether, wherein the hard capsule comprises a body and a cap that seals the body, and a ratio of a maximum thickness to a minimum thickness of the body and the cap is each 2.5 or less.
摘要:
A continuous preparation method of a biodegradable aliphatic/aromatic polyester copolymer includes: performing a first esterification reaction of an aliphatic dihydroxy compound with an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product from the first esterification reaction; continuously performing a first polycondensation reaction of a reaction product from the second esterification reaction to obtain a prepolymer; continuously performing a second polycondensation reaction of the prepolymer to obtain a second polycondensation reaction product having a melting index from about 15 g/10 min to about 25 g/10 min; and continuously performing a third polycondensation reaction of the second polycondensation reaction product to prepare the biodegradable aliphatic/aromatic polyester copolymer, wherein the performing of the first esterification reaction or the continuously performing of the second esterification reaction includes adding an aromatic carboxylic acid.
摘要:
Provided is a method of continuous preparation of a biodegradable aliphatic/aromatic polyester copolymer, the method including: performing a first esterification reaction of an aliphatic dihydroxy compound and an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product obtained by the first esterification reaction; obtaining a pre-polymer by continuously performing a first polycondensation reaction of a reaction product obtained by the second esterification reaction; and continuously performing polycondensation reaction of the pre-polymer, wherein an aromatic carboxylic acid is added to a reactor in which the first esterification reaction or the second esterification reaction is performed, to prepare the biodegradable aliphatic/aromatic polyester copolymer. According to the method of continuous preparation of the biodegradable aliphatic/aromatic polyester copolymer as described above, the amount of the aliphatic dihydroxy compound used, which is a starting material, is reduced and accordingly, manufacturing costs are reduced.
摘要:
A continuous preparation method of a biodegradable aliphatic/aromatic polyester copolymer includes: performing a first esterification reaction of an aliphatic dihydroxy compound with an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product from the first esterification reaction; continuously performing a first polycondensation reaction of a reaction product from the second esterification reaction to obtain a prepolymer; continuously performing a second polycondensation reaction of the prepolymer to obtain a second polycondensation reaction product having an intrinsic viscosity from about 0.9 dl/g to about 1.0 dl/g; and continuously performing a third polycondensation reaction of the second polycondensation reaction product to prepare the biodegradable aliphatic/aromatic polyester copolymer, wherein the performing of the first esterification reaction or the continuously performing of the second esterification reaction includes adding an aromatic carboxylic acid. The biodegradable aliphatic/aromatic polyester copolymer prepared by control of the intrinsic viscosity of the second polycondensation reaction product may be improved in processibility, film formability, tensile/tearing strength, and blending ability with another polymer resin. Use of a less amount of the aliphatic dihydroxy compound as a starting material may reduce manufacturing costs.
摘要:
A continuous preparation method of a biodegradable aliphatic/aromatic polyester copolymer includes: performing a first esterification reaction of an aliphatic dihydroxy compound with an aliphatic dicarboxylic acid at a temperature of 185° C. or less; continuously performing a second esterification reaction of a reaction product from the first esterification reaction; continuously performing a first polycondensation reaction of a reaction product from the second esterification reaction to obtain a prepolymer having a weight average molecular weight of about 6,900 to about 14,000; continuously performing a second polycondensation reaction of the prepolymer to obtain a second polycondensation reaction product; and continuously performing a third polycondensation reaction of the second polycondensation reaction product to prepare the biodegradable aliphatic/aromatic polyester copolymer, wherein the performing of the first esterification reaction or the continuously performing of the second esterification reaction includes adding an aromatic carboxylic acid. The biodegradable aliphatic/aromatic polyester copolymer prepared by the continuous method may be improved in processibility, film formability, tensile/tearing strength, and blending ability with another polymer resin. Use of a less amount of the aliphatic dihydroxy compound as a starting material may reduce manufacturing costs.