公开(公告)号:US10226766B2
公开(公告)日:2019-03-12
申请号:US14366712
申请日:2012-12-20
Applicant: SHELL OIL COMPANY
Inventor: Wiebe Sjoerd Kijlstra , Ferry Winter
IPC: B01J37/20 , C10G47/20 , B01J37/02 , B01J29/08 , B01J27/051 , B01J23/883 , B01J29/14 , B01J29/16 , B01J37/00
Abstract: A process for the preparation of a naphtha-selective hydrocracking catalyst comprising of from 3 to 4.8% wt of molybdenum, calculated as metal, and of from 1.5 to 3% wt of nickel, calculated as metal, which comprises loading a refractory oxide support comprising an alumina binder component and a zeolite Y component in a content of from 65 to 75 wt % based on the total weight of the catalyst, with nickel and molybdenum in the presence of citric acid, wherein the zeolite Y component has a unit cell size in the range of from 24.42 to 24.52 Å, a SAR in the range of from 8 to 15, and a surface area of from 850 to 1020 m2/g.
-
公开(公告)号:US20150273447A1
公开(公告)日:2015-10-01
申请号:US14428496
申请日:2013-09-16
Applicant: SHELL OIL COMPANY
Inventor: Hermanus Jongkind , Wiebe Sjoerd Kijlstra , Bart Pelgrim , Marcello Stefano Rigutto , Ferry Winter
IPC: B01J29/16 , B01J31/06 , B01J23/888 , C10G47/20 , B01J37/04 , B01J37/08 , B01J37/20 , B01J37/02 , B01J35/00 , B01J21/04
CPC classification number: B01J29/166 , B01J21/04 , B01J23/883 , B01J23/888 , B01J23/8885 , B01J29/146 , B01J31/06 , B01J35/0006 , B01J37/0203 , B01J37/0205 , B01J37/0213 , B01J37/04 , B01J37/08 , B01J37/20 , B01J2229/16 , B01J2229/186 , B01J2229/42 , C10G47/20
Abstract: This invention relates to a process for the preparation of a hydrocracking catalyst and its use. A zeolite Y having specifically defined properties is mixed with an alumina binder component and a first metals-containing solution that is extruded to form an extruded mixture. The extruded mixture is dried and calcined. The dried and calcined mixture is then impregnated with a second metals-containing solution.
Abstract translation: 本发明涉及一种制备加氢裂化催化剂的方法及其用途。 具有特定定义性质的沸石Y与氧化铝粘合剂组分和第一含金属溶液混合,挤出形成挤出混合物。 将挤出的混合物干燥并煅烧。 然后将干燥和煅烧的混合物用第二含金属溶液浸渍。
-
3.
公开(公告)号:US20150126791A1
公开(公告)日:2015-05-07
申请号:US14366712
申请日:2012-12-20
Inventor: Wiebe Sjoerd Kijlstra , Ferry Winter
IPC: B01J37/20 , C10G47/20 , B01J37/02 , B01J29/08 , B01J27/051
CPC classification number: B01J37/20 , B01J23/883 , B01J27/0515 , B01J29/084 , B01J29/146 , B01J29/166 , B01J37/0009 , B01J37/0036 , B01J37/0213 , B01J2229/186 , B01J2229/36 , B01J2229/37 , B01J2229/42 , C10G47/20
Abstract: A process for the preparation of a naphtha-selective hydrocracking catalyst comprising of from 3 to 4.8% wt of molybdenum, calculated as metal, and of from 1.5 to 3% wt of nickel, calculated as metal, which comprises loading a refractory oxide support comprising an alumina binder component and a zeolite Y component in a content of from 65 to 75 wt % based on the total weight of the catalyst, with nickel and molybdenum in the presence of citric acid, wherein the zeolite Y component has a unit cell size in the range of from 24.42 to 24.52 Å, a SAR in the range of from 8 to 15, and a surface area of from 850 to 1020 m2/g.
Abstract translation: 一种制备石脑油选择性加氢裂化催化剂的方法,其包含以金属计算的3至4.8重量%的钼,以金属计算为1.5-3重量%的镍,其包括负载耐火氧化物载体,其包括: 氧化铝粘合剂组分和沸石Y组分,其含量为催化剂总重量的65至75重量%,在柠檬酸存在下为镍和钼,其中沸石Y组分具有单位晶胞尺寸 范围为24.42至24.52埃,SAR范围为8至15,表面积为850至1020平方米/克。
-
-