Abstract:
An apparatus that includes a near field transducer, the near field transducer including silver (Ag) and at least one other element or compound, wherein the at least one other element or compound is selected from: copper (Cu), palladium (Pd), gold (Au), zirconium (Zr), zirconium oxide (ZrO), platinum (Pt), geranium (Ge), nickel (Ni), tungsten (W), cobalt (Co), rhodium (Rh), ruthenium (Ru), tantalum (Ta), chromium (Cr), aluminum (Al), vanadium (V), iridium (Ir), titanium (Ti), magnesium (Mg), iron (Fe), molybdenum (Mo), silicon (Si), or combinations thereof oxides of V, Zr, Mg, calcium (Ca), Al, Ti, Si, cesium (Ce), yttrium (Y), Ta, W or thorium (Th), Co, or combinations thereof; or nitrides of Ta, Al, Ti, Si, indium (In), Fe, Zr, Cu, W, boron (B), halfnium (Hf), or combinations thereof.
Abstract:
A device including a near field transducer (NFT); a write pole; at least one dielectric material positioned between the NFT and the write pole; and an adhesion layer positioned between the NFT and the at least one dielectric material.
Abstract:
A device including a near field transducer (NFT); a write pole; at least one dielectric material positioned between the NFT and the write pole; and an adhesion layer positioned between the NFT and the at least one dielectric material.
Abstract:
A device including a near field transducer (NFT); a write pole; at least one dielectric material positioned between the NFT and the write pole; and an adhesion layer positioned between the NFT and the at least one dielectric material.
Abstract:
Methods of forming a layer of magnetic material on a substrate, the method including: configuring a substrate in a chamber; controlling the temperature of the substrate at a substrate temperature, the substrate temperature being at or below about 250° C.; and introducing one or more precursors into the chamber, the one or more precursors including: cobalt (Co), nickel (Ni), iron (Fe), or combinations thereof, wherein the precursors chemically decompose at the substrate temperature, and wherein a layer of magnetic material is formed on the substrate, the magnetic material including at least a portion of the one or more precursors, and the magnetic material having a magnetic flux density of at least about 1 Tesla (T).
Abstract:
An apparatus that includes a near field transducer, the near field transducer including silver (Ag) and at least one other element or compound, wherein the at least one other element or compound is selected from: copper (Cu), palladium (Pd), gold (Au), zirconium (Zr), zirconium oxide (ZrO), platinum (Pt), geranium (Ge), nickel (Ni), tungsten (W), cobalt (Co), rhodium (Rh), ruthenium (Ru), tantalum (Ta), chromium (Cr), aluminum (Al), vanadium (V), iridium (Ir), titanium (Ti), magnesium (Mg), iron (Fe), molybdenum (Mo), silicon (Si), or combinations thereof oxides of V, Zr, Mg, calcium (Ca), Al, Ti, Si, cesium (Ce), yttrium (Y), Ta, W or thorium (Th), Co, or combinations thereof; or nitrides of Ta, Al, Ti, Si, indium (In), Fe, Zr, Cu, W, boron (B), halfnium (Hf), or combinations thereof.
Abstract:
Methods of forming a layer of magnetic material on a substrate, the method including: configuring a substrate in a chamber; controlling the temperature of the substrate at a substrate temperature, the substrate temperature being at or below about 250° C.; and introducing one or more precursors into the chamber, the one or more precursors including: cobalt (Co), nickel (Ni), iron (Fe), or combinations thereof, wherein the precursors chemically decompose at the substrate temperature, and wherein a layer of magnetic material is formed on the substrate, the magnetic material including at least a portion of the one or more precursors, and the magnetic material having a magnetic flux density of at least about 1 Tesla (T).
Abstract:
Methods of forming a layer of magnetic material on a substrate, the method including: configuring a substrate in a chamber; controlling the temperature of the substrate at a substrate temperature, the substrate temperature being at or below about 250° C.; and introducing one or more precursors into the chamber, the one or more precursors including: cobalt (Co), nickel (Ni), iron (Fe), or combinations thereof, wherein the precursors chemically decompose at the substrate temperature, and wherein a layer of magnetic material is formed on the substrate, the magnetic material including at least a portion of the one or more precursors, and the magnetic material having a magnetic flux density of at least about 1 Tesla (T).
Abstract:
A device including a near field transducer (NFT); a write pole; at least one dielectric material positioned between the NFT and the write pole; and an adhesion layer positioned between the NFT and the at least one dielectric material.
Abstract:
A device including a magnetoresistive sensor; a top shield; and a bottom shield, wherein the magnetoresistive sensor is positioned between the top shield and the bottom shield, and wherein at least one of the bottom shield and the top shield include NiFeX, wherein X is chosen from Nb, Mo, Ta, or W.