摘要:
A method of preserving a PEFC stack of the present invention is a method of preserving a PEFC stack that is provided with an oxidizing agent passage having an inlet and an outlet and extending through a cathode and a reducing agent passage having an inlet and an outlet and extending through an anode. The method comprises preserving the polymer electrolyte fuel cell stack in an uninstalled state under a condition in which an oxygen concentration within the oxidizing agent passage and within the reducing agent passage is lower than an oxygen concentration in atmospheric air.
摘要:
A preservation method of a polymer electrolyte membrane electrode assembly (MEA) which is capable of controlling its degradation that may be thereafter caused by the preservation is provided. A method of preserving a polymer electrolyte membrane electrode assembly including a polymer electrolyte membrane, a pair of catalyst layers disposed on both surfaces of the polymer electrolyte membrane, and a pair of gas diffusion electrodes disposed on outer surfaces of the pair of the catalyst layers, the method comprising the steps of causing the polymer electrolyte membrane electrode assembly to perform a power generation process just after the polymer electrolyte membrane electrode assembly is manufactured or within a time period in which degradation of the polymer electrolyte membrane electrode assembly due to influence of a solvent or impurities does not occur (step S1); and thereafter preserving the polymer electrolyte membrane electrode assembly (step S2).
摘要:
A method of preserving a PEFC stack of the present invention is a method of preserving a PEFC stack that is provided with an oxidizing agent passage having an inlet and an outlet and extending through a cathode and a reducing agent passage having an inlet and an outlet and extending through an anode. The method comprises preserving the polymer electrolyte fuel cell stack in an uninstalled state under a condition in which an oxygen concentration within the oxidizing agent passage and within the reducing agent passage is lower than an oxygen concentration in atmospheric air.
摘要:
A preservation assembly of a polymer electrolyte fuel cell stack is provided. The assembly includes an uninstalled polymer electrolyte fuel cell stack and sealing units. The uninstalled polymer electrolyte fuel cell stack is provided with an oxidizing agent passage having an inlet and an outlet and extending through a cathode and a reducing agent passage having an inlet and an outlet and extending through an anode. The sealing units include sealing plugs or containers and are configured to seal the inlet and the outlet of the oxidizing agent passage within which an oxygen concentration has been decreased and to seal the inlet and the outlet of the reducing agent passage within which the oxygen concentration has been decreased. The uninstalled polymer electrolyte fuel cell stack is in a state before an assembled polymer electrolyte fuel cell stack is incorporated into a fuel cell system.
摘要:
A preservation assembly of a PEFC stack which is capable of sufficiently inhibiting degradation of performance of the PEFC stack particularly during a time period that elapses from when the stack is placed in the uninstalled state until it is placed in the installation position and is practically used. The PEFC stack is provided with an oxidizing agent passage having an inlet and an outlet and extending through a cathode and a reducing agent passage having an inlet and an outlet and extending through an anode. The PEFC stack is preserved in an uninstalled state in such a manner that an interior of the oxidizing agent passage and an interior of the reducing agent passage are set in a pressure-reduced state.
摘要:
Provided is a method of preserving a PEFC stack, which is capable of controlling degradation of performance of the PEFC stack during a time period that elapses from when the stack is placed in an uninstalled state until it is placed in an installation position and is practically used. Provided is a preservation assembly of the PEFC stack which is capable of sufficiently inhibiting degradation of performance of the PEFC stack particularly during a time period that elapses from when the stack is placed in the uninstalled state until it is placed in the installation position and is practically used. A method of preserving a PEFC stack that is provided with an oxidizing agent passage (30) having an inlet and an outlet and extending through a cathode and a reducing agent passage (40) having an inlet and an outlet and extending through an anode, comprising preserving the PEFC (200) stack in an uninstalled state in such a manner that an interior of the oxidizing agent passage (30) and an interior of the reducing agent passage (40) are set in a pressure-reduced state.
摘要:
Provided is a method of preserving a PEFC stack, which is capable of controlling degradation of performance of the PEFC stack during a time period that elapses from when the stack is placed in an uninstalled state until it is placed in an installation position and is practically used. Provided is a preservation assembly of the PEFC stack which is capable of sufficiently inhibiting degradation of performance of the PEFC stack particularly during a time period that elapses from when the stack is placed in the uninstalled state until it is placed in the installation position and is practically used. A method of preserving a PEFC stack that is provided with an oxidizing agent passage (30) having an inlet and an outlet and extending through a cathode and a reducing agent passage (40) having an inlet and an outlet and extending through an anode, comprising preserving the PEFC (200) stack in an uninstalled state in such a manner that an interior of the oxidizing agent passage (30) and an interior of the reducing agent passage (40) are set in a pressure-reduced state.
摘要:
Provided is a method of preserving a PEFC stack, which is capable of controlling degradation of performance of the PEFC stack during a time period that elapses from when the stack is placed in an uninstalled state until it is placed in an installation position and is practically used. Provided is a preservation assembly of the PEFC stack which is capable of sufficiently inhibiting degradation of performance of the PEFC stack particularly during a time period that elapses from when the stack is placed in the uninstalled state until it is placed in the installation position and is practically used. A method of preserving a PEFC stack that is provided with an oxidizing agent passage (30) having an inlet and an outlet and extending through a cathode and a reducing agent passage (40) having an inlet and an outlet and extending through an anode, comprising preserving the PEFC (200) stack in an uninstalled state in such a manner that an interior of the oxidizing agent passage (30) and an interior of the reducing agent passage (40) are set in a pressure-reduced state.
摘要:
Provided is a method of preserving a PEFC stack, which is capable of controlling degradation of performance of the PEFC stack during a time period that elapses from when the stack is placed in an uninstalled state until it is placed in an installation position and is practically used. Provided is a preservation assembly of the PEFC stack which is capable of sufficiently inhibiting degradation of performance of the PEFC stack particularly during a time period that elapses from when the stack is placed in the uninstalled state until it is placed in the installation position and is practically used. A method of preserving a PEFC stack that is provided with an oxidizing agent passage (30) having an inlet and an outlet and extending through a cathode and a reducing agent passage (40) having an inlet and an outlet and extending through an anode, comprising preserving the PEFC (200) stack in an uninstalled state in such a manner that an interior of the oxidizing agent passage (30) and an interior of the reducing agent passage (40) are set in a pressure-reduced state.
摘要:
A preservation assembly of a PEFC stack which is capable of sufficiently inhibiting degradation of performance of the PEFC stack particularly during a time period that elapses from when the stack is placed in the uninstalled state until it is placed in the installation position and is practically used. The PEFC stack is provided with an oxidizing agent passage having an inlet and an outlet and extending through a cathode and a reducing agent passage having an inlet and an outlet and extending through an anode. The PEFC stack is preserved in an uninstalled state in such a manner that an interior of the oxidizing agent passage and an interior of the reducing agent passage are set in a pressure-reduced state.