公开(公告)号:US07137276B2
公开(公告)日:2006-11-21
申请号:US10362313
申请日:2001-08-20
CPC分类号: C03C17/3417 , C03C17/2453 , C03C17/2456 , C03C2217/211 , C03C2217/212 , C03C2217/23 , C03C2217/71 , C03C2217/91 , C03C2218/15
摘要: A process for the production of durable photocatalytically active self-cleaning coating on glass by contacting a hot glass surface with a fluid mixture of titanium chloride, a source of oxygen and a tin precursor. The coating preferably comprises less than 10 atom % tin in the bulk of the coating and preferably there is a greater atomic percent tin in the surface of the coating than there is in the bulk of the coating. Preferably, the coating is durable to abrasion and humidity cycling.
摘要翻译: 通过使热玻璃表面与氯化钛,氧源和锡前体的流体混合物接触来在玻璃上生产耐久的光催化活性自清洁涂层的方法。 该涂层优选包含在涂层主体中小于10原子%的锡,并且优选地,涂层表面中的原子百分比比在涂层主体中更大。 优选地,涂层耐磨损和湿度循环。
-
公开(公告)号:US20110287178A1
公开(公告)日:2011-11-24
申请号:US12452150
申请日:2008-07-04
IPC分类号: B05D5/06
CPC分类号: C23C16/453 , C03C17/245 , C03C2217/213 , C03C2218/152
摘要: Anti reflective silica coatings are deposited on the glass ribbon produced during a float glass or a rolled glass production process using a flame pyrolysis deposition process which is preferably a combustion chemical vapour deposition process. The temperature of the ribbon is greater than 200° C. The process may be carried out in the gap between the float bath or rollers and the annealing lehr. The durability of the coating may be increased by sintering. The equipment preferably comprises an extraction unit positioned adjacent to each burner head. In a further embodiment additional oxygen is introduced to the vapour deposition process in order produce a coating having a lower effective refractive index.
摘要翻译: 防反射二氧化硅涂层沉积在使用火焰热解沉积工艺(最好是燃烧化学气相沉积工艺)的浮法玻璃或轧制玻璃生产过程中产生的玻璃带上。 带的温度大于200℃。该过程可以在浮浴或辊之间的间隙和退火炉中进行。 通过烧结可以提高涂层的耐久性。 该设备优选地包括与每个燃烧器头相邻设置的提取单元。 在另外的实施方案中,将额外的氧气引入到气相沉积工艺中,以便产生具有较低有效折射率的涂层。
-
公开(公告)号:US06929862B2
公开(公告)日:2005-08-16
申请号:US10144010
申请日:2002-05-13
IPC分类号: C03C17/245 , C03C17/34 , C23C16/40 , B32B9/00
CPC分类号: B01J35/004 , B01J21/063 , B01J37/0215 , B32B17/10036 , B32B17/10174 , B32B17/10761 , C03C17/2456 , C03C17/3417 , C03C2217/212 , C03C2217/71 , C03C2218/152 , C23C16/405
摘要: A coated substrate, especially a glass substrate, such coated substrate having high photocatalytic activity and low visible light reflection as well as being highly abrasion resistant. Preferably, the coating is a titanium oxide coating, the photolytic activity is greater than 5×10−3 cm−1min−1, and coating side visible light reflection is 35% or lower.
摘要翻译: 涂布的基材,特别是玻璃基材,具有高光催化活性和低可见光反射以及高耐磨性的涂布基材。 优选地,涂层是氧化钛涂层,光解活性大于5×10 -3 cm -1 min -1以下,涂层侧 可见光反射率为35%以下。
-
公开(公告)号:US20120040175A1
公开(公告)日:2012-02-16
申请号:US13138690
申请日:2010-03-19
申请人: Simon James Hurst , Troy Manning , Peter Dobson , Steve Sheard , Peter Bishop , Ivan Parkin
发明人: Simon James Hurst , Troy Manning , Peter Dobson , Steve Sheard , Peter Bishop , Ivan Parkin
CPC分类号: C03C1/008 , C03C17/008 , C03C2217/72 , C23C18/1216 , C23C18/1229 , C23C18/1258 , C23C18/127 , Y10T428/25
摘要: Methods for coating a substrate are disclosed, the methods comprising providing a substrate, providing pre-formed nanoparticles of an inorganic material, providing at least one precursor of a first metal oxide, and depositing a coating on at least one surface of the substrate by contacting the surface with the precursor of the metal oxide and pre-formed nanoparticles. Also disclosed are substrates coated using such a method. The coated substrates are coloured. Preferably the metal oxide is a doped metal oxide to modify the thermal properties of the coating. The preferred nanoparticles are of platinum group metals or coinage metals.
摘要翻译: 公开了涂覆基材的方法,所述方法包括提供基材,提供无机材料的预先形成的纳米颗粒,提供至少一种第一金属氧化物的前体,以及通过接触将沉积在基材的至少一个表面上的涂层 表面与金属氧化物的前体和预形成的纳米颗粒。 还公开了使用这种方法涂覆的基材。 涂覆的基材是着色的。 优选地,金属氧化物是掺杂的金属氧化物以改变涂层的热性能。 优选的纳米颗粒是铂族金属或造币金属。
-
公开(公告)号:US20130160640A1
公开(公告)日:2013-06-27
申请号:US13820281
申请日:2011-09-02
摘要: An armour system, comprising at least two elements, wherein said elements are arranged at an angle(α)°, characterised wherein said at least two elements comprise a plurality of perforations.
摘要翻译: 一种装甲系统,包括至少两个元件,其中所述元件以角度(α)°布置,其特征在于,所述至少两个元件包括多个穿孔。
-
公开(公告)号:US09470481B2
公开(公告)日:2016-10-18
申请号:US13820281
申请日:2011-09-02
摘要: An armor system, comprising at least two elements, wherein the elements are arranged at an angle, characterized wherein the at least two elements include a plurality of perforations.
摘要翻译: 一种装甲系统,包括至少两个元件,其中所述元件以一定角度布置,其特征在于,所述至少两个元件包括多个穿孔。
-
公开(公告)号:US06840061B1
公开(公告)日:2005-01-11
申请号:US09587970
申请日:2000-06-06
CPC分类号: C23C16/405 , C03C17/2456 , C03C17/3417 , C03C2217/212 , C03C2217/71 , C03C2218/152
摘要: A process for the production of a photocatalytically active self-cleaning coated substrate, especially a glass substrate, which comprises depositing a titanium oxide coating on the surface of the substrate by contacting it with a fluid mixture containing a source of titanium and a source of oxygen, the substrate being at a temperature of at least 600° C. The coated surface has good durability, a high photocatalytic activity and a low visible light reflection. Most preferably the deposition temperature is in the range 645° C. to 7200° C. which provides especially good durability. The fluid mixture preferably contains titanium chloride and an ester, especially ethyl acetate. Also disclosed is a self cleaning coated substrate, especially a glass substrate, having high photocatalytic activity and low visible light reflection and a durable self-cleaning coated glass.
摘要翻译: 一种用于制备光催化活性自清洁涂覆的基材,特别是玻璃基材的方法,其包括通过使其与含有钛源和氧源的流体混合物接触来沉积氧化钛涂层在基材的表面上 基板处于至少600℃的温度。涂覆表面具有良好的耐久性,高的光催化活性和低的可见光反射。 最优选地,沉积温度在645℃至7200℃的范围内,这提供了特别好的耐久性。 流体混合物优选含有氯化钛和酯,特别是乙酸乙酯。 还公开了具有高光催化活性和低可见光反射的自清洁涂覆的基材,特别是玻璃基材,以及耐久的自洁涂层玻璃。
-
-
-
-
-
-