摘要:
A metal back-attached phosphor screen comprises a metal back layer that has a high-reflectance, high-resistance layer consisting of an In-, Sn- or Bi-oxide layer. The metal back layer of the metal back-attached phosphor screen may have a laminate structure including a high-reflectance layer formed on a phosphor layer side and a high-resistance layer formed on that layer. The high-reflectance layer may be formed of Al, In, Sn or Bi. The high-resistance layer may be formed of an Al-, In-, Sn-, Bi- or Si-oxide or nitride. A high-brightness metal back-attached phosphor screen is provided that prevents the destruction or the deterioration of an electron emission element and a phosphor screen by discharging.
摘要:
A transfer film comprising a base film (11), a parting-agent layer (12), a protective film (13), and a metal film (14), the latter three being formed on the base film (11) in order, wherein the protective film (13) contains a softening agent such as a phosphate, an aliphatic monobasic acid ester, an aliphatic dibasic acid ester, or a dihydric alcohol ester. By using such a transfer film, a metal back layer is formed. Since the transfer layer of the transfer film has a surface resistivity of as high as 102–108 Ω/, the surface resistivity of the formed metal back layer is high, and discharge is suppressed.
摘要:
A transfer film comprising a base film (11), a parting-agent layer (12), a protective film (13), and a metal film (14), the latter three being formed on the base film (11) in order, wherein the protective film (13) contains a softening agent such as a phosphate, an aliphatic monobasic acid ester, an aliphatic dibasic acid ester, or a dihydric alcohol ester. By using such a transfer film, a metal back layer is formed. Since the transfer layer of the transfer film has a surface resistivity of as high as 102-108 Ω/, the surface resistivity of the formed metal back layer is high, and discharge is suppressed.
摘要:
A transfer film comprising a base film (11), a parting-agent layer (12), a protective film (13), and a metal film (14), the latter three being formed on the base film (11) in order, wherein the protective film (13) contains a softening agent such as a phosphate, an aliphatic monobasic acid ester, an aliphatic dibasic acid ester, or a dihydric alcohol ester. By using such a transfer film, a metal back layer is formed. Since the transfer layer of the transfer film has a surface resistivity of as high as 102-108 Ω/, the surface resistivity of the formed metal back layer is high, and discharge is suppressed.
摘要:
An electron source device includes a porous layer (for example, porous alumina layer) which is composed of an insulator and has many microscopic holes provided in a direction perpendicular to a main surface, and first and second conductor layers placed on both sides of the porous layer, and is characterized in that the current density I/S is 1 μA/cm2 or higher when a direct-current voltage is applied between the second conductor layer and the fist conductor layer while using the second conductor layer as an anode. In this case, S represents the overlapping area of the first conductor layer, the second conductor layer and the porous layer. Consequently, an electron source device having a high electron emission ability and a long life even when the degree of vacuum is low can be obtained at low cost, and hence, a display having a high luminous efficiency and high reliability can be realized.
摘要翻译:电子源装置包括由绝缘体构成的多孔层(例如,多孔氧化铝层),在与主表面垂直的方向上具有许多微小的孔,以及设置在多孔层的两侧的第一和第二导体层 并且其特征在于当在第二导体层和第一导体层之间施加直流电压时,电流密度I / S为1μA/ cm 2以上,同时使用第二导体层 导体层作为阳极。 在这种情况下,S表示第一导体层,第二导体层和多孔层的重叠面积。 因此,可以以低成本获得具有高电子发射能力和长寿命的电子源器件,因此可以实现具有高发光效率和高可靠性的显示器。
摘要:
This dispersion liquid composition for black matrix comprises; manganese oxide having an average particle diameter in the range of 50 to 2000 nm, or solid solution of manganese oxide and ferric oxide having an average particle diameter in the range of 50 to 2000 nm and a manganese content in the range of 15 to 70% by weight; at least one kind of dispersing agent selected from a group of water-soluble acrylic resin, sodium salt, ammonium salt or potassium salt of water-soluble acrylic resin, and sodium salt, ammonium salt or potassium salt of polycarboxylic acid or ligninsulfonic acid or bisphenolsulfonic acid; and water, or a solvent mixture of water and an organic solvent compatible with water. By employing such a dispersion liquid composition for black matrix, light reflectivity of a light absorption layer of an interface with a panel is remarkably reduced. Accordingly, in a display device such as a color cathode ray tube, a display surface in which superposition of ambient light is difficult to occur is realized.
摘要:
A coating solution composition for forming a glass gel thin film, contains at least one material selected from the group consisting of a metal alkoxide and a polycondensate of the metal alkoxide, a coloring material, an alcohol solvent, and a dispersant having an adsorption material for the coloring material, soluble in the alcohol solvent, and having miscibility with the metal alkoxide, wherein the coloring material has an average particle size of 3 nm to 300 nm. A glass gel thin film obtained by sintering this composition at a temperature of 100.degree. to 300.degree. C. is excellent in water resistance, durability and has a high strength.
摘要:
An ink composition having a pigment in its droplets, which are adhered onto the surface such as glass, ceramics or polyester resins of a base material, always dispersed uniformly is ejected from a nozzle by an ink-jet method to directly form a prescribed pattern of a colored layer of a color filter on the surface of the base material.
摘要:
A coating solution composition for forming a glass gel thin film, contains at least one material selected from the group consisting of a metal alkoxide and a polycondensate of the metal alkoxide, a coloring material, an alcohol solvent, and a dispersant having an adsorption material for the coloring material, soluble in the alcohol solvent, and having miscibility with the metal alkoxide, wherein the coloring material has an average particle size of 3 nm to 300 nm. A glass gel thin film obtained by sintering this composition at a temperature of 100.degree. to 300.degree. C. is excellent in water resistance, durability and has a high strength.
摘要:
An electroluminescent phosphor comprising particles of a phosphor and particles of an electron-emitting material not originating from atoms constituting the host material of the phosphor and an activator. The particles of the electron-emitting material is contained inside the phosphor particles or included between the phosphor particles in close contact with the phosphor particles. An electroluminescent element has a light emitting layer containing the electroluminescent phosphor. Another electroluminescent element has a light emitting layer containing particles of a phosphor and particles of an electron-emitting material composed of a conductive compound not originating from the atoms constituting the host material of the phosphor and the activator. The proportion of the electron-emitting material to the light emitting layer is 1-75 weight %. A high-luminous efficiency and high-luminance electroluminescent element can be produced.