Abstract:
A coated article has: a metallic substrate (22); a bondcoat (30); and a thermal barrier coating (TBC) (28). The bondcoat has a first layer (32) and a second layer (34), the first layer having a lower Cr content than the second layer.
Abstract:
A coated article has: a metallic substrate (22); a bondcoat (30); and a thermal barrier coating (TBC) (28). The bondcoat has a first layer (32) and a second layer (34), the first layer having a lower Cr content than the second layer.
Abstract:
The present disclosure relates to an improved low-cost metallic coating to be deposited on gas turbine engine components. The metallic coating consists of 1.0 to 18 wt % cobalt, 3.0 to 18 wt % chromium, 5.0 to 15 wt % aluminum, 0.01 to 1.0 wt % yttrium, 0.01 to 0.6 wt % hafnium, 0.0 to 0.3 wt % silicon, 0.0 to 1.0 wt % zirconium, 0.0 to 10 wt % tantalum, 0.0 to 9.0 wt % tungsten, 0.0 to 10 wt % molybdenum, 0.0 to 43.0 wt % platinum, and the balance nickel.
Abstract:
A method for coating a turbine engine component comprises the steps of: providing a turbine engine component having at least one sacrificial attachment on a first side; grasping the turbine engine component via the at least one sacrificial attachment to position a first surface of the turbine engine component relative to a source of coating material; and applying a coating to said first side.
Abstract:
A coated article has: a metallic substrate; a bondcoat; and a thermal barrier coating (TBC). The bondcoat has an MCrAlY first layer and an MCrAlY second layer, the second layer having a lower Cr content than the first layer.
Abstract:
A process for improving the adherence of a thermal barrier coating to a substrate includes the steps of providing a substrate, depositing a masking layer of aluminum, an aluminum alloy, or titanium alloy, or titanium on a surface of the substrate, depositing a non-thermally grown oxide layer of alumina or titania on the masking layer, and depositing a thermal barrier coating on the oxide layer.
Abstract:
The present disclosure relates to an improved low-cost metallic coating to be deposited on gas turbine engine components. The metallic coating consists of 1.0 to 18 wt % cobalt, 3.0 to 18 wt % chromium, 5.0 to 15 wt % aluminum, 0.01 to 1.0 wt % yttrium, 0.01 to 0.6 wt % hafnium, 0.0 to 0.3 wt % silicon, 0.0 to 1.0 wt % zirconium, 0.0 to 10 wt % tantalum, 0.0 to 9.0 wt % tungsten, 0.0 to 10 wt % molybdenum, 0.0 to 43.0 wt % platinum, and the balance nickel.
Abstract:
A process for improving the adherence of a thermal barrier coating to a substrate includes the steps of providing a substrate, depositing a masking layer of aluminum, an aluminum alloy, or titanium alloy, or titanium on a surface of the substrate, depositing a non-thermally grown oxide layer of alumina or titania on the masking layer, and depositing a thermal barrier coating on the oxide layer.
Abstract:
A coated article has: a metallic substrate (22); a bondcoat (30); and a thermal barrier coating (TBC) (28). The bondcoat has a first layer (32) and a second layer (34), the first layer having a lower Cr content than the second layer.
Abstract:
The thermal barrier coating system comprises a matrix of a first chemistry with multiple embedded second phases of a second chemistry. The matrix comprises a stabilized zirconia. The second regions comprise at least 40 mole percent of oxides having the formula Ln2O3, where Ln is selected from the lanthanides La through Lu, Y, Sc, In, Ca, and Mg with the balance zirconia (ZrO2), hafnia (HfO2), titania (TiO2), or mixtures thereof. The second phases have a characteristic thickness (T6) of less than 2.0 micrometers (μm). The spacing between second phases has a characteristic thickness (T5) of less than 8.0 micrometers (μm).