Method and Apparatus for Microplasma Spray Coating a Portion of a Turbine Vane in a Gas Turbine Engine
    2.
    发明申请
    Method and Apparatus for Microplasma Spray Coating a Portion of a Turbine Vane in a Gas Turbine Engine 有权
    在燃气轮机发动机中用于微喷涂的涡轮叶片的一部分的方法和装置

    公开(公告)号:US20130098879A1

    公开(公告)日:2013-04-25

    申请号:US13708945

    申请日:2012-12-08

    Abstract: A method and apparatus for microplasma spray coating a portion of a turbine vane without masking any portions thereof. The apparatus includes a microplasma gun with an anode, cathode, and an arc generator for generating an electric arc between the anode and cathode. An arc gas emitter injects gas through the electric arc. The electric arc is operable for ionizing the gas to create a plasma gas stream. A powder injector injects powdered material into a plasma stream. A localized area of the turbine vane is coated with the powdered material without having to mask the turbine vane.

    Abstract translation: 一种用于微观喷雾涂覆涡轮叶片的一部分而不遮盖其任何部分的方法和装置。 该装置包括具有阳极,阴极和电弧发生器的微型喷枪,用于在阳极和阴极之间产生电弧。 电弧气体发射器通过电弧喷射气体。 电弧可操作用于电离气体以产生等离子体气流。 粉末喷射器将粉末材料注入等离子体流中。 涡轮叶片的局部区域涂覆有粉末材料,而不必掩盖涡轮叶片。

    METHOD OF APPLYING A WEAR RESISTANT COATING
    5.
    发明申请
    METHOD OF APPLYING A WEAR RESISTANT COATING 审中-公开
    应用耐磨涂层的方法

    公开(公告)号:US20130316086A1

    公开(公告)日:2013-11-28

    申请号:US13962477

    申请日:2013-08-08

    Abstract: A method of applying a wear-resistant coating comprises mixing about 75% to about 85% by weight chromium carbide and about 15% to about 25% by weight nickel chromium to form a chromium carbide-nickel chromium mixture, and simultaneously heating the chromium carbide-nickel chromium mixture to about 1371 degrees Celsius to about 2204 degrees Celsius and applying the chromium carbide-nickel chromium mixture at a velocity in a range of about 305 meters feet per second to about 915 meters per second by high velocity oxygen fuel (HVOF) spraying.

    Abstract translation: 施加耐磨涂层的方法包括混合约75重量%至约85重量%的碳化铬和约15重量%至约25重量%的镍铬,以形成碳化铬 - 镍铬混合物,并同时加热碳化铬 镍镍混合物至约1371摄氏度至约2204摄氏度,并以高速氧燃料(HVOF)以约305米/秒至约915米每秒的速度施加碳化铬 - 镍铬混合物, 喷涂。