Abstract:
The present invention relates to a method for fractionating lignin, wherein the method comprises the following steps: (i) dissolving lignin into a mixture containing organic solvent and water; and (ii) ultrafiltrating the mixture formed in step (i) through one or more filtration membranes for producing a predetermined number of lignin fractions, wherein each fraction contains lignin with a molecular weight within a predetermined range. The present invention further relates to a lignin fraction and to the uses thereof.
Abstract:
The invention relates to a method for treating lignin, wherein the method comprises the following steps: a) dissolving lignin into an aqueous composition, which contains a compound selected from the class of phenols, while keeping the temperature of the composition at 0-6° C.; and b) allowing the composition to react while keeping the temperature of the composition at 60-100° C. and the pH of the composition at a pH value of 6-14. The invention relates further to a method for producing a binder composition and to different applications thereof.
Abstract:
The present invention relates to a method for increasing the reactivity of lignin, wherein the method comprises the following steps: a) forming, under heating at a temperature of 71-94° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin.
Abstract:
The present invention relates to a method for producing a binder composition, wherein the method comprises the following steps: (i) forming an aqueous composition comprising reactant components including lignin molecules of 11-60 lignin units, lignin molecules of 1-10 lignin units, polymerizable substance and crosslinking agent in the presence of a catalyst; and (ii) cooking the composition at a temperature of 60-95° C. for polymerizing the reactant components until a binder composition with a predetermined viscosity value is formed.
Abstract:
The invention relates to a method for treating lignin, wherein the method comprises the following steps: a) dissolving lignin into an aqueous composition, which contains a compound selected from the class of phenols, while keeping the temperature of the composition at 0-16° C.; and b) allowing the composition to react while keeping the temperature of the composition at 60-100° C. and the pH of the composition at a pH valise of 6-14. The invention relates further to a method for producing a binder composition and to different applications thereof.
Abstract:
The present invention relates to a method for increasing the reactivity of lignin, wherein the method comprises the following steps: a) forming, under heating at a temperature of 71-94° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin.
Abstract:
The invention relates to a method for producing a fiber based product, wherein the method comprises the steps of: a) applying a binder composition over at least one surface of at least one fiber based substrate; b) determining the distribution of the applied binder composition over the entire at least one surface of the at least one fiber based substrate; and c) based on the determination in step b) either accepting the treated at least one fiber based substrate for the production of the fiber based product or rejecting the treated at least one fiber based substrate from the production of the fiber based product. The invention further relates to a method for producing a binder composition, to a binder composition and to a fiber based product.
Abstract:
The present invention relates to a method for increasing the reactivity of lignin, wherein the method comprises the following steps: a) forming, under heating at a temperature of 71-94° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin.
Abstract:
The present invention relates to a method for increasing the reactivity of lignin, wherein the method comprises the following steps: a) forming, under heating at a temperature of 30-70° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin.
Abstract:
The present invention relates to a method for increasing the reactivity of lignin, wherein the method comprises the following steps: a) forming, under heating at a temperature of 30-70° C., an aqueous dispersion comprising alkali and lignin, wherein the alkali comprises a hydroxide of an alkali metal; and b) heating the dispersion formed in step a) at a temperature of 50-95° C. for producing alkalated lignin.