OXYNITRIDE FLUORESCENT POWDER AND METHOD FOR MANUFACTURING SAME
    2.
    发明申请
    OXYNITRIDE FLUORESCENT POWDER AND METHOD FOR MANUFACTURING SAME 审中-公开
    氧化物荧光粉及其制造方法

    公开(公告)号:US20160272886A1

    公开(公告)日:2016-09-22

    申请号:US14777611

    申请日:2014-03-19

    IPC分类号: C09K11/77 C01B21/068

    摘要: An oxynitride phosphor powder includes an α-sialon fluorescent body having a fluorescent peak wavelength of 605-615 nm, and the external quantum efficiency of the oxynitride phosphor powder is greater than the conventional art. The oxynitride phosphor powder includes an α-sialon represented by the formula Cax1Eux2Si12-(y+z)Al(y+z)OzN16-z (where x1, x2, y, and z satisfy the expressions 1.10≦x1+x2≦1.70, 0.18≦x2/x1≦0.47, and 2.6≦y≦3.6, 0.0≦z≦1.0).

    摘要翻译: 氮氧化物荧光体粉末包括具有605-615nm的荧光峰值波长的α-赛隆荧光体,并且氮氧化物荧光体粉末的外部量子效率大于常规技术。 氮氧化物荧光体粉末包括由式Cax1Eux2Si12-(y + z)Al(y + z)OzN16-z(其中x1,x2,y和z满足表达式1.10≤x1+x2≤1.70)表示的α-赛隆, 0.18≤x2/x1≤0.47,2.6≤y≤3.6,0.0≤z≤1.0)。

    Oxynitride phosphor powder
    3.
    发明授权
    Oxynitride phosphor powder 有权
    氧氮化钠荧光粉

    公开(公告)号:US09382477B2

    公开(公告)日:2016-07-05

    申请号:US14387886

    申请日:2013-03-28

    IPC分类号: C09K11/77 H01L33/50

    摘要: An oxynitride phosphor power has a fluorescence peak wavelength of 580 to 605 nm, the oxynitride phosphor having a higher external quantum efficiency than ever before. The oxynitride phosphor powder is an oxynitride phosphor powder containing α-SiAlON and aluminum nitride, represented by composition formula: Cax1Eux2Si12−(y+z)Al(y+z)OzN16−z wherein x1, x2, y and z are 0

    摘要翻译: 氧氮化物荧光粉功率的荧光峰值波长为580〜605nm,氧氮化物荧光体具有比以往更高的外部量子效率。 氮氧化物荧光体粉末是由以下组成式表示的α-SiAlON和氮化铝的氮氧化物荧光体粉末:Cax1Eux2Si12-(y + z)Al(y + z)OzN16-z其中x1,x2,y和z分别为0

    OXYNITRIDE PHOSPHOR POWDER AND METHOD FOR PRODUCING SAME

    公开(公告)号:US20170174986A1

    公开(公告)日:2017-06-22

    申请号:US15115943

    申请日:2015-02-02

    IPC分类号: C09K11/77 H01L33/50 C09K11/08

    摘要: An oxynitride phosphor powder has a fluorescence peak wavelength of 587 to 630 nm and a high external quantum efficiency. A method of producing the oxynitride phosphor powder containing Li at 50 to 10,000 ppm includes mixing silicon nitride powder, a substance serving as an aluminum source, a substance serving as a calcium source and a substance serving as an europium source; firing the mixture at 1500 to 2000° C. in an inert gas atmosphere or a reducing gas atmosphere to obtain a fired oxynitride phosphor composed mainly of Ca-containing α-SiAlON, as an intermediate; and heat treating the fired oxynitride phosphor at a temperature of 1450° C. to less than the firing temperature, in an inert gas atmosphere or in a reducing gas atmosphere in the presence of Li.

    OXYNITRIDE PHOSPHOR POWDER
    8.
    发明申请
    OXYNITRIDE PHOSPHOR POWDER 有权
    氧化磷粉

    公开(公告)号:US20150044471A1

    公开(公告)日:2015-02-12

    申请号:US14387886

    申请日:2013-03-28

    IPC分类号: C09K11/77

    摘要: An oxynitride phosphor power has a fluorescence peak wavelength of 580 to 605 nm, the oxynitride phosphor having a higher external quantum efficiency than ever before. The oxynitride phosphor powder is an oxynitride phosphor powder containing α-SiAlON and aluminum nitride, represented by composition formula: Cax1Eux2Si12−(y+z)Al(y+z)OzN16−z wherein x1, x2, y and z are 0

    摘要翻译: 氧氮化物荧光粉功率的荧光峰值波长为580〜605nm,氧氮化物荧光体具有比以往更高的外部量子效率。 氮氧化物荧光体粉末是由以下组成式表示的α-SiAlON和氮化铝的氮氧化物荧光体粉末:Cax1Eux2Si12-(y + z)Al(y + z)OzN16-z其中x1,x2,y和z分别为0

    Oxynitride phosphor powder and method for producing same

    公开(公告)号:US10125313B2

    公开(公告)日:2018-11-13

    申请号:US15115943

    申请日:2015-02-02

    摘要: An oxynitride phosphor powder has a fluorescence peak wavelength of 587 to 630 nm and a high external quantum efficiency. A method of producing the oxynitride phosphor powder containing Li at 50 to 10,000 ppm includes mixing silicon nitride powder, a substance serving as an aluminum source, a substance serving as a calcium source and a substance serving as an europium source; firing the mixture at 1500 to 2000° C. in an inert gas atmosphere or a reducing gas atmosphere to obtain a fired oxynitride phosphor composed mainly of Ca-containing α-SiAlON, as an intermediate; and heat treating the fired oxynitride phosphor at a temperature of 1450° C. to less than the firing temperature, in an inert gas atmosphere or in a reducing gas atmosphere in the presence of Li.