摘要:
The invention relates to a process for preparing multifilament, wet-spun elastane threads with increased spinning output, which is achieved by largely removing entrained water from the filaments after leaving the spinning bath and then fixing the threads on at least two rollers at a temperature of at least 200.degree. C. for at least 3 seconds.
摘要:
The invention relates to a process for preparing multifilament, wet-spun elastane threads with increased spinning output, which is achieved by largely removing entrained water from the filaments after leaving the spinning bath and then fixing the threads on at least two rollers at a temperature of at least 200.degree. C. for at least 3 seconds.
摘要:
This invention relates to a new washing apparatus for the continuous production of elastane filaments which are produced by a wet-spinning process, which essentially consists of a stripping unit (10) and a washing unit (11) which are disposed in steps above the precipitation bath (1) of a wet-spinning device.
摘要:
The invention relates to a process for adjusting the viscosity of highly concentrated elastane solutions by reaction of the solution with secondary aromatic amines in order to produce spinning solutions for the dry or wet spinning of elastane fibres.
摘要:
The invention relates to a process for adjusting the viscosity of highly concentrated elastane solutions by reaction of the solution with secondary aromatic amines in order to produce spinning solutions for the dry or wet spinning of elastane fibers.
摘要:
An elastance spool is described which comprises a winding of elastane threads having a titre of greater than 160 dtex, particularly from 160 dtex to 1400 dtex, and a bobbin weight of elastane threads of at least 1.5 kg, in which the elastane threads have a ribbon-shaped fiber cross-section, wherein the ratio of the width of the elastane threads to the thickness of the elastane threads in cross-section is at least three to one. The elastane spool is used for the production of textile sheet products and for the production of disposable articles of hygiene.
摘要:
Described are a process for producing elastane yarn having a linear density of at least 2500 dtex by the wet spinning process and the thereby producible coarse linear density elastane yarn having a wide cross section and a low residual solvent content. The process comprises the steps of spinning an up to 35% strength by weight stable-viscosity elastane solution into a coagulation bath, washing and optionally drawing, drying by contact heating, setting, spin finishing and winding the yarn, the filaments leaving the coagulation bath passing around a diverting roller disposed just above the coagulation bath liquid, the as-spun filament linear density amounting to not more than 1% of the value of the final linear density, the jet stretch ratio being within the range from 0.5 to 50, the contact heating temperature being at least 220° C. and the contact time of the elastane yarn being at least 2 seconds.
摘要:
There is described a method for the storing of elastan filaments with a titre of at least 2,500 dtex in drums with a filament line length of at least 10 km with the use of a displacing device, in which the filaments are stored meandering in layers, and in which the filaments are inlaid into the drum at a speed of at least eight per cent above the production speed of the filaments.
摘要:
A spinning noxxle apparatus for the production of elastane filaments from spinning solutions by the wet spinning method comprising a feed line (7) for the spinning solution, a filter unit (1) having a mixer element (2) and a filter element element (3), a spinning nozzle (5) for immersion in a precipation bath (11), and a connection piece (8) for the direct connection of the filter unit (1) and spinning nozzle (5), wherein the spinning nozzle (5) is joined to the connection piece (8) by a quick-release coupling connection (4), particularly a bayonet coupling (4).
摘要:
Described are a process for producing elastane yarn having a linear density of at least 2500 dtex by the wet spinning process and the thereby producible coarse linear density elastane yarn having a wide cross section and a low residual solvent content. The process comprises the steps of spinning an up to 35% strength by weight stable-viscosity elastane solution into a coagulation bath, washing and optionally drawing, drying by contact heating, setting, spin finishing and winding the yarn, the filaments leaving the coagulation bath passing around a diverting roller disposed just above the coagulation bath liquid, the as-spun filament linear density amounting to not more than 1% of the value of the final linear density, the jet stretch ratio being within the range from 0.5 to 50, the contact heating temperature being at least 220° C. and the contact time of the elastane yarn being at least 2 seconds.