Elastane package
    6.
    发明授权
    Elastane package 失效
    弹性包装

    公开(公告)号:US06774064B1

    公开(公告)日:2004-08-10

    申请号:US09958422

    申请日:2002-01-11

    IPC分类号: B32B100

    摘要: An elastance spool is described which comprises a winding of elastane threads having a titre of greater than 160 dtex, particularly from 160 dtex to 1400 dtex, and a bobbin weight of elastane threads of at least 1.5 kg, in which the elastane threads have a ribbon-shaped fiber cross-section, wherein the ratio of the width of the elastane threads to the thickness of the elastane threads in cross-section is at least three to one. The elastane spool is used for the production of textile sheet products and for the production of disposable articles of hygiene.

    摘要翻译: 描述了一种弹性卷轴,其包括具有大于160dtex,特别是160dtex至1400dtex的滴定度的弹性纱线的卷绕和至少1.5kg的弹性纤维纱线的筒管重量,其中弹性纤维线具有带 形纤维横截面,其中弹性纤维丝的宽度与弹性纤维线的横截面的厚度之比至少为三比一。 弹性线轴用于生产纺织片材产品和生产一次性卫生用品。

    Process of making elastane yarn
    7.
    发明授权
    Process of making elastane yarn 失效
    制造弹性纱线的工艺

    公开(公告)号:US06602453B1

    公开(公告)日:2003-08-05

    申请号:US09720708

    申请日:2000-12-29

    IPC分类号: D01D506

    摘要: Described are a process for producing elastane yarn having a linear density of at least 2500 dtex by the wet spinning process and the thereby producible coarse linear density elastane yarn having a wide cross section and a low residual solvent content. The process comprises the steps of spinning an up to 35% strength by weight stable-viscosity elastane solution into a coagulation bath, washing and optionally drawing, drying by contact heating, setting, spin finishing and winding the yarn, the filaments leaving the coagulation bath passing around a diverting roller disposed just above the coagulation bath liquid, the as-spun filament linear density amounting to not more than 1% of the value of the final linear density, the jet stretch ratio being within the range from 0.5 to 50, the contact heating temperature being at least 220° C. and the contact time of the elastane yarn being at least 2 seconds.

    摘要翻译: 描述了通过湿法纺丝法制造线密度为2500dtex的弹性纤维的方法,从而生产出具有宽截面和低残留溶剂含量的粗制线性密度弹性纤维纱。 该方法包括以下步骤:将高达35%的重量比的稳定粘度的丙烯腈溶液旋转到凝固浴中,洗涤并任选地拉伸,通过接触加热,凝固,旋涂和卷绕纱线干燥,离开凝固浴的长丝 围绕设置在凝固浴液体正上方的转向辊,所述纺丝长丝线密度为不超过最终线密度值的1%,喷射拉伸比在0.5至50的范围内, 接触加热温度至少为220℃,弹性纤维的接触时间为至少2秒。

    Elastane yarn having a linear density of at least 2500 dtex and a cross-sectional width to height ratio of at least 4:1
    8.
    发明授权
    Elastane yarn having a linear density of at least 2500 dtex and a cross-sectional width to height ratio of at least 4:1 失效
    线密度为2500dtex,截面宽高比至少为4:1的弹性纤维纱

    公开(公告)号:US06844060B2

    公开(公告)日:2005-01-18

    申请号:US10425457

    申请日:2003-04-29

    IPC分类号: D01F6/70 D01G6/00 D01G3/00

    摘要: Described are a process for producing elastane yarn having a linear density of at least 2500 dtex by the wet spinning process and the thereby producible coarse linear density elastane yarn having a wide cross section and a low residual solvent content. The process comprises the steps of spinning an up to 35% strength by weight stable-viscosity elastane solution into a coagulation bath, washing and optionally drawing, drying by contact heating, setting, spin finishing and winding the yarn, the filaments leaving the coagulation bath passing around a diverting roller disposed just above the coagulation bath liquid, the as-spun filament linear density amounting to not more than 1% of the value of the final linear density, the jet stretch ratio being within the range from 0.5 to 50, the contact heating temperature being at least 220° C. and the contact time of the elastane yarn being at least 2 seconds.

    摘要翻译: 弹性纤维横截面宽,残留溶剂含量低,线密度至少为2500dtex。