Methods for doping and coating nickel hydroxide
    3.
    发明授权
    Methods for doping and coating nickel hydroxide 失效
    掺杂和涂覆氢氧化镍的方法

    公开(公告)号:US6015538A

    公开(公告)日:2000-01-18

    申请号:US98407

    申请日:1998-06-16

    摘要: The process precipitates additives onto nickel hydroxide seeds in an ammonia solution. Then introducing at least one metallic additive into the aqueous solution creates a slurry having a reducing potential. The additive is selected from the group consisting of aluminum, cadmium, cobalt, indium, iron, manganese and zinc. Introducing oxygen into the additive-containing slurry at a controlled rate maintains the reducing potential of the solution. At least one of the additives dissolves into the aqueous solution in excess of the slurry's solution solubility to precipitate the additive in the form of a hydroxide on the nickel hydroxide seeds.

    摘要翻译: 该方法在氨溶液中将添加剂沉淀在氢氧化镍晶种上。 然后将至少一种金属添加剂引入水溶液中产生具有还原电位的浆料。 添加剂选自铝,镉,钴,铟,铁,锰和锌。 以受控的速率将氧气引入含添加剂的浆料中维持溶液的还原电位。 至少一种添加剂溶解在水溶液中超过浆料的溶液溶解度,以将氢氧化物形式的添加剂沉淀在氢氧化镍晶种上。

    Process for producing nickel hydroxide from elemental nickel
    4.
    发明授权
    Process for producing nickel hydroxide from elemental nickel 失效
    从元素镍生产氢氧化镍的方法

    公开(公告)号:US5824283A

    公开(公告)日:1998-10-20

    申请号:US847715

    申请日:1997-04-28

    IPC分类号: C01G53/04 C01B13/14 C01G53/00

    摘要: This process produces nickel hydroxide from elemental nickel. Introducing elemental nickel into at least a 4N aqueous ammonia solution forms a mixture. Activating the nickel powder of this mixture allows the nickel to react with oxygen in the solution. This results in the dissolving of the nickel, producing a loaded solution containing nickel and hydroxyl ions. The redox potential of the solution remains negative during the dissolution of nickel. Distilling the loaded solution to vaporize the aqueous ammonia solution results in the precipitating of nickel hydroxide.

    摘要翻译: 该方法从元素镍产生氢氧化镍。 将元素镍引入至少4N氨水溶液中形成混合物。 激活该混合物的镍粉使镍与溶液中的氧反应。 这导致镍的溶解,产生含有镍和羟基离子的负载溶液。 在溶解镍期间溶液的氧化还原电位保持不变。 蒸馏装载的溶液以蒸发氨水溶液导致氢氧化镍的沉淀。

    Method for removal of Mn from cobalt sulfate solutions
    8.
    发明申请
    Method for removal of Mn from cobalt sulfate solutions 有权
    从硫酸钴溶液中除去Mn的方法

    公开(公告)号:US20050120828A1

    公开(公告)日:2005-06-09

    申请号:US10729911

    申请日:2003-12-09

    IPC分类号: C22B47/00

    摘要: The present invention provides a method for the removal of substantially all the amount of Mn contained in cobalt containing solution thereby to obtain purified cobalt solution with Mn content of 10 ppm or less and specifically a method for removing Mn from cobalt sulfate solution comprising the steps of adjusting pH of the solution within the range of 3-6 and then adding the NaOCl to the solution to obtain an oxidation-reduction potential in the range of 1100 to 1300 mV, with respect to standard hydrogen electrode (SHE); and removing Mn precipitate from thus treated solution.

    摘要翻译: 本发明提供了一种除去含钴溶液中所含的基本上所有量的Mn的方法,从而得到Mn含量为10ppm以下的纯化钴溶液,具体地说是从硫酸钴溶液中除去Mn的方法,包括以下步骤: 将溶液的pH调节到3-6范围内,然后将NaOCl加入到溶液中,以获得相对于标准氢电极(SHE)在1100至1300mV范围内的氧化还原电位; 并从这样处理的溶液中除去Mn沉淀物。

    Process for cobalt recovery from mixed sulfides
    9.
    发明授权
    Process for cobalt recovery from mixed sulfides 失效
    从混合硫化物中回收钴的方法

    公开(公告)号:US4401630A

    公开(公告)日:1983-08-30

    申请号:US298208

    申请日:1981-08-31

    CPC分类号: C22B23/0415 C22B23/0492

    摘要: The metal content of nickel-cobalt mixed sulfide slurries is recovered by atmospheric oxidation leaching, thereafter removing dissolved copper by metathesis with further mixed sulfide feed, treating the filtrate after liquid-solids separation with ammonia to selectively precipitate cobalt, separating the cobalt precipitate and working up the resulting filtrate to recover nickel.

    摘要翻译: 通过大气氧化浸出回收镍钴混合硫化物浆料的金属含量,然后通过复分解进一步混合硫化物进料除去溶解的铜,在用氨固液分离后处理滤液以选择性沉淀钴,分离钴沉淀物和加工 使所得滤液回收镍。

    Method for removal of Mn from cobalt sulfate solutions
    10.
    发明授权
    Method for removal of Mn from cobalt sulfate solutions 有权
    从硫酸钴溶液中除去Mn的方法

    公开(公告)号:US07052528B2

    公开(公告)日:2006-05-30

    申请号:US10729911

    申请日:2003-12-09

    IPC分类号: C22B47/00

    摘要: The present invention provides a method for the removal of substantially all the amount of Mn contained in cobalt containing solution thereby to obtain purified cobalt solution with Mn content of 10 ppm or less and specifically a method for removing Mn from cobalt sulfate solution comprising the steps of adjusting pH of the solution within the range of 3–6 and then adding the NaOCl to the solution to obtain an oxidation-reduction potential in the range of 1100 to 1300 mV, with respect to standard hydrogen electrode (SHE); and removing Mn precipitate from thus treated solution.

    摘要翻译: 本发明提供了一种除去含钴溶液中所含的基本上所有量的Mn的方法,从而得到Mn含量为10ppm以下的纯化钴溶液,具体地说是从硫酸钴溶液中除去Mn的方法,包括以下步骤: 将溶液的pH调节到3-6范围内,然后将NaOCl加入到溶液中,以获得相对于标准氢电极(SHE)在1100至1300mV范围内的氧化还原电位; 并从这样处理的溶液中除去Mn沉淀物。