Apparatus and foam electroplating process
    3.
    发明申请
    Apparatus and foam electroplating process 失效
    仪器和泡沫电镀工艺

    公开(公告)号:US20070278105A1

    公开(公告)日:2007-12-06

    申请号:US11407655

    申请日:2006-06-05

    IPC分类号: C25D3/12 C25C7/02

    摘要: An improved apparatus and method of producing metal foam is provided which involves optimizing the natural convection of electrolyte through a foam being electroplated by inclining the foam during plating. A diagonal flow of electrolyte though the foam enhances electrolyte turnover within the foam while increasing electroplating efficiency. Further increases in plating efficiency are provided by shifting current density from higher plating zones to lower plating zones.

    摘要翻译: 提供了一种改进的制造金属泡沫的装置和方法,其涉及通过在电镀期间使泡沫倾斜而电镀的泡沫来优化电解质的自然对流。 通过泡沫的电解质对角线流动可提高泡沫内的电解质周转率,同时提高电镀效率。 电镀效率的进一步提高是通过将电流密度从较高的镀层转移到较低的镀层区域来提供的。

    Process for producing nickel hydroxide from elemental nickel
    4.
    发明授权
    Process for producing nickel hydroxide from elemental nickel 失效
    从元素镍生产氢氧化镍的方法

    公开(公告)号:US5824283A

    公开(公告)日:1998-10-20

    申请号:US847715

    申请日:1997-04-28

    IPC分类号: C01G53/04 C01B13/14 C01G53/00

    摘要: This process produces nickel hydroxide from elemental nickel. Introducing elemental nickel into at least a 4N aqueous ammonia solution forms a mixture. Activating the nickel powder of this mixture allows the nickel to react with oxygen in the solution. This results in the dissolving of the nickel, producing a loaded solution containing nickel and hydroxyl ions. The redox potential of the solution remains negative during the dissolution of nickel. Distilling the loaded solution to vaporize the aqueous ammonia solution results in the precipitating of nickel hydroxide.

    摘要翻译: 该方法从元素镍产生氢氧化镍。 将元素镍引入至少4N氨水溶液中形成混合物。 激活该混合物的镍粉使镍与溶液中的氧反应。 这导致镍的溶解,产生含有镍和羟基离子的负载溶液。 在溶解镍期间溶液的氧化还原电位保持不变。 蒸馏装载的溶液以蒸发氨水溶液导致氢氧化镍的沉淀。

    Methods for doping and coating nickel hydroxide
    8.
    发明授权
    Methods for doping and coating nickel hydroxide 失效
    掺杂和涂覆氢氧化镍的方法

    公开(公告)号:US6015538A

    公开(公告)日:2000-01-18

    申请号:US98407

    申请日:1998-06-16

    摘要: The process precipitates additives onto nickel hydroxide seeds in an ammonia solution. Then introducing at least one metallic additive into the aqueous solution creates a slurry having a reducing potential. The additive is selected from the group consisting of aluminum, cadmium, cobalt, indium, iron, manganese and zinc. Introducing oxygen into the additive-containing slurry at a controlled rate maintains the reducing potential of the solution. At least one of the additives dissolves into the aqueous solution in excess of the slurry's solution solubility to precipitate the additive in the form of a hydroxide on the nickel hydroxide seeds.