Abstract:
Disclosed are: a polyalkylene terephthalate resin composition comprising (A) a polyalkylene terephthalate resin and (B) an acrylic-based core-shell polymer which has an average particle size of 2 μm or greater and in which an amount of the core layer component is more than 80% by mass but less than 100% by mass relative to a total mass of the core layer component and a shell layer component; and a molded article which is obtained by molding the polyalkylene terephthalate resin composition.
Abstract:
A resin composition including an aromatic polyester resin and having high levels of hydrolysis resistance and moldability is provided. The resin composition includes an aromatic polyester resin having a terminal carboxyl group content of not more than 30 eq/ton (component A), a cyclic carbodiimide compound having at least two carbodiimide rings, each having only one carbodiimide group (component B), and a polyvalent hydroxyl group-containing compound having a hydroxyl value of not less than 200 (component C).
Abstract:
Provided is a means for obtaining a polybutylene terephthalate resin composition that exhibits excellent hydrolysis resistance and high fluidity in a molten state. A carbodiimide compound (B) and a polyhydric hydroxyl group-containing compound (C) are added to a polybutylene terephthalate resin (A) having a terminal carboxyl group content of 30 meq/kg or lower. The polyhydric hydroxyl group-containing compound (C) that is used has a hydroxyl group value of 200 or higher. It is preferable for the polybutylene terephthalate resin (A) to have an intrinsic viscosity of 0.6 dL/g or higher.
Abstract:
A polybutylene terephthalate resin composition in which it is possible to effectively suppress discoloration without lowering the heat shock resistance. The polybutylene terephthalate resin composition is part of a molded article having a lightness L* value of 80 or higher as measured using a color difference meter, and includes a polybutylene terephthalate resin having a terminal carboxyl group content of 30 meq/kg or less, a carbodiimide compound, and a phosphite compound; and the phosphite compound content is 0.05-0.15 parts by mass per 100 parts by mass of polybutylene terephthalate resin.
Abstract:
Disclosed are: a polyalkylene terephthalate resin composition comprising (A) a polyalkylene terephthalate resin and (B) an acrylic-based core-shell polymer which has an average particle size of 2 μm or greater and in which an amount of the core layer component is more than 80% by mass but less than 100% by mass relative to a total mass of the core layer component and a shell layer component; and a molded article which is obtained by molding the polyalkylene terephthalate resin composition.
Abstract:
A polybutylene terephthalate resin composition which is free from bleeding and other problems, and improves the flowability (melt-flowability) while maintaining the characteristics such as mechanical strength or toughness. To 100 parts by weight of a composition composed of 50 to 90% by weight of (A) a polybutylene terephthalate resin and 10 to 50% by weight of (B) inorganic filler, is blended 0.05 to 5 parts by weight of (C) a glycerin fatty acid ester being composed of glycerin and/or a dehydrated condensate thereof and a fatty acid having 12 or more carbon atoms and having 200 or more hydroxyl value determined by a method specified in the description.
Abstract:
A resin composition including an aromatic polyester resin and having high levels of hydrolysis resistance and moldability is provided. The resin composition includes an aromatic polyester resin having a terminal carboxyl group content of not more than 30 eq/ton (component A), a cyclic carbodiimide compound having at least two carbodiimide rings, each having only one carbodiimide group (component B), and a polyvalent hydroxyl group-containing compound having a hydroxyl value of not less than 200 (component C).