摘要:
A method and apparatus for analyzing the electrode impedance, in which an a.c. voltage with its frequency varied at intervals is applied between a pair of measuring electrodes dipped in the sample liquid, the complex a.c. impedance between the electrodes is measured at each frequency, the maximum value among absolute values of imaginary part of the measured impedance values is detected as the electrode polarization resistance, and the solution resistance of the liquid is calculated by subtracting the detected maximum value from the real part of the impedance corresponding to the maximum imaginary part.
摘要:
An air conditioning system for a building according to the present invention essentially has a first thermal storage tank as a cold thermal source which is installed at a high place in the building, a second thermal storage tank as a hot thermal source which is installed at a low place in the building, air conditioners which are installed at various levels between the first thermal storage tank and the second thermal storage tank, and heat pipes of a gravity type with which the air conditioners are connected to the first thermal storage tank and the second thermal storage tank. This system dispenses with passages for water, typically used as a thermal medium, at the places where air conditioners are installed. The system makes it possible to lower the capacities of the air conditioning equipment, especially the capacity of the regrigerator included in the cold thermal source equipment.
摘要:
The object of this invention is to provide a method for mitigating a stress corrosion cracking of reactor structural material which makes it possible to suppress the rise in the main steam line dose rate without secondary effects such as a rise in the concentration of radioactive cobalt-60, etc. in the reactor water. Hydrogen and a reductive nitrogen compound containing nitrogen having a negative oxidation number (for example, hydrazine) are injected into the core water of boiling water nuclear power plant. By injecting the reductive nitrogen compound containing nitrogen having a negative oxidation number into the core water, the stress corrosion cracking of structural material of reactor can be mitigated without side reactions such as a rise in the concentration of cobalt-60, etc.
摘要:
A method for surface modification of a fluorine resin by irradiating the surface of the fluorine resin containing a heat-resistant light-absorbing polymeric material and/or a light-absorbing material is with laser light. Surface properties of the fluorine resin molded articles, particularly adhesion and wetting properties, can be greatly improved by a simple operation with high efficiency.
摘要:
The object of this invention is to provide a method for mitigating a stress corrosion cracking of reactor structural material which makes it possible to suppress the rise in the main steam line dose rate without secondary effects such as a rise in the concentration of radioactive cobalt-60, etc. in the reactor water. Hydrogen and a reductive nitrogen compound containing nitrogen having a negative oxidation number (for example, hydrazine) are injected into the core water of boiling water nuclear power plant. By injecting the reductive nitrogen compound containing nitrogen having a negative oxidation number into the core water, the stress corrosion cracking of structural material of reactor can be mitigated without side reactions such as a rise in the concentration of cobalt-60, etc.
摘要:
The object of this invention is to provide a method for mitigating a stress corrosion cracking of reactor structural material which makes it possible to suppress the rise in the main steam line dose rate without secondary effects such as a rise in the concentration of radioactive cobalt-60, etc. in the reactor water. Hydrogen and a reductive nitrogen compound containing nitrogen having a negative oxidation number (for example, hydrazine) are injected into the core water of boiling water nuclear power plant. By injecting the reductive nitrogen compound containing nitrogen having a negative oxidation number into the core water, the stress corrosion cracking of structural material of reactor can be mitigated without side reactions such as a rise in the concentration of cobalt-60, etc.
摘要:
A head-lamp having an adjuster construction comprising a pivot portion and an adjusting screw portion, in which a ball joint is provided for at least one of said portions, a part of a carrying surface of the ball joint being formed of a soft elastic member which extends into the region of the ball joint.
摘要:
The present invention provides a base cloth for reinforcement produced by winding a weldable yarn on either one of a warp or weft or the both at a definite interval, arranging the warp and weft in the respective directions and then thermally welding the both yarns. According to this method, the fraying of warp or weft, particularly easy fluffing of carbon fibers, etc. can be prevented by winding the weldable yarn. And, it is sufficient for the weldable yarn to be present at the intersections between the warp and weft. Consequently, as compared with a case wherein the whole weft is impregnated with adhesives, penetration of the matrix resin can sufficiently be attained and thus, strength in the weft direction can be improved.
摘要:
The present invention provides a gypsum molded product having excellent waterproof properties without impaired strength by adding alkaline metal alkylsiliconates or phenylsiliconates together with calcium hydroxide or calcium oxide to gypsum; poly(.alpha.,.beta.-unsaturated carboxylic acid) may be used in combination with the above, if desired. According to the present invention, the preparation of a gypsum molded product, particularly a gypsum from desulfurization of exhaust gas, is contemplated.
摘要:
The object of this invention is to provide a method for mitigating a stress corrosion cracking of reactor structural material which makes it possible to suppress the rise in the main steam line dose rate without secondary effects such as a rise in the concentration of radioactive cobalt-60, etc. in the reactor water. Hydrogen and a reductive nitrogen compound containing nitrogen having a negative oxidation number (for example, hydrazine) are injected into the core water of boiling water nuclear power plant. By injecting the reductive nitrogen compound containing nitrogen having a negative oxidation number into the core water, the stress corrosion cracking of structural material of reactor can be mitigated without side reactions such as a rise in the concentration of cobalt-60, etc.