摘要:
A (Li, Na, K)(Nb, Ta)O3 based piezoelectric/electrostrictive porcelain composition obtained by adding a slight amount of a Mn compound to a perovskite type oxide containing Li, Na and K as A-site elements and contains at least Nb out of Nb and Ta as B-site elements, where a ratio of a total number of atoms of the A-site elements to a total number of atoms of the B-site elements is not smaller than 1. A composition of the perovskite type oxide as a principal component is represented by a general formula: {Liy(Na1-xKx)1-y}a(Nb1-zTaz)O3. The A/B ratio “a” preferably satisfies 1
摘要翻译:通过向含有Li,Na和K的钙钛矿型氧化物中添加少量的Mn化合物作为A位元素而至少含有(Li,Na,K)(Nb,Ta)O 3的压电/电致伸缩瓷组合物 Nb中的Nb和Ta作为B位元素,其中A位元素的总原子数与B位元素的总原子数的比率不小于1.钙钛矿的组成 氧化物作为主要成分的通式为:{Liy(Na1-xKx)1-y} a(Nb1-zTaz)O3。 A / B比“a”优选满足1
摘要:
A (Li, Na, K)(Nb, Ta)O3 based piezoelectric/electrostrictive porcelain composition obtained by adding a slight amount of a Mn compound to a perovskite type oxide containing Li, Na and K as A-site elements and contains at least Nb out of Nb and Ta as B-site elements, where a ratio of a total number of atoms of the A-site elements to a total number of atoms of the B-site elements is not smaller than 1. A composition of the perovskite type oxide as a principal component is represented by a general formula: {Liy(Na1-xKx)1-y}a(Nb1-zTaz)O3. The A/B ratio “a” preferably satisfies 1
摘要翻译:通过向含有Li,Na和K的钙钛矿型氧化物中添加少量的Mn化合物作为A位元素而至少含有(Li,Na,K)(Nb,Ta)O 3的压电/电致伸缩瓷组合物 Nb中的Nb和Ta作为B位元素,其中A位元素的总原子数与B位元素的总原子数的比率不小于1.钙钛矿的组成 氧化物作为主要成分的通式为:{Liy(Na1-xKx)1-y} a(Nb1-zTaz)O3。 A / B比“a”优选满足1
摘要:
A (Li, Na, K)(Nb, Ta)O3-based piezoelectric/electrostrictive ceramic composition having a large field-induced distortion during application of a high electric field is provided. After synthesizing a perovskite oxide containing Li (lithium), Na (sodium) and K (potassium) as A-site elements and containing at least Nb (niobium) out of the Nb and Ta (tantalum) as B-site elements, a ratio of total number of atoms of the A-site elements to total number of atoms of the B-site elements being higher than 1, a Bi (bismuth) compound is added to the perovskite oxide and the perovskite oxide is reacted with the Bi compound. An addition amount of the Bi compound with respect to 100 molar parts of the perovskite oxide is preferably equal to or greater than 0.01 molar part and equal to or smaller than 0.1 molar part in terms of Bi atoms.
摘要:
A piezoelectric/electrostrictive device which exhibits an excellent piezoelectric characteristic and which has only a small dependence on a temperature is provided. The piezoelectric/electrostrictive device includes a piezoelectric/electrostrictive portion made of a piezoelectric ceramic, and electrodes electrically connected to the piezoelectric/electrostrictive portion. The piezoelectric ceramic reversibly transits to a tetragonal phase and an orthorhombic phase at a phase transition point as a boundary. The piezoelectric/electrostrictive portion is formed by a polarization treatment performed under the conditions that a treatment temperature ranges from a first temperature which exceeds the phase transition point of the piezoelectric ceramic to a second temperature which is 50° C. higher than the first temperature.
摘要:
A (Li, Na, K)(Nb, Ta)O3-based piezoelectric/electrostrictive ceramic composition having a large field-induced distortion during application of a high electric field is provided. After synthesizing a perovskite oxide containing Li (lithium), Na (sodium) and K (potassium) as A-site elements and containing at least Nb (niobium) out of the Nb and Ta (tantalum) as B-site elements, a ratio of total number of atoms of the A-site elements to total number of atoms of B-site elements being higher than 1, a Bi (bismuth) compound is added to the perovskite oxide and the perovskite oxide is reacted with the Bi compound. An addition amount of the Bi compound with respect to 100 molar parts of the perovskite oxide is preferably equal to or greater than 0.01 molar part and equal to or smaller than 0.1 molar part in terms of Bi atoms.
摘要:
There is disclosed a piezoelectric/electrostrictive device which exhibits an excellent piezoelectric characteristic and which has an only small dependence on a temperature so that the piezoelectric characteristic does not easily change with the temperature. A piezoelectric/electrostrictive device includes a piezoelectric/electrostrictive portion made of a piezoelectric ceramic, and electrodes electrically connected to the piezoelectric/electrostrictive portion. The piezoelectric ceramic can reversibly transit to a tetragonal phase and an orthorhombic phase at a phase transition point as a boundary, and the piezoelectric/electrostrictive portion is formed by a polarization treatment performed on conditions that a treatment temperature ranges from a temperature which exceeds the phase transition point of the piezoelectric ceramic to a temperature which is 50° C. higher than the temperature.
摘要:
A monomorph type piezoelectric/electrostrictive device includes a piezoelectric/electrostrictive body, which is composed of a non-lead based piezoelectric/electrostrictive crystalline body containing at least Nb, Ta, and one or more types of alkali metal element, which has a cubic crystal structure at a temperature higher than the phase transition point and at least any one of tetragonal and orthorhombic crystal structures at a temperature lower than the phase transition point, and which is curved to a large extent by a polarization treatment to take on a curved shape at a temperature lower than the phase transition point without application of a voltage after the polarization treatment. In the polarization treatment, an electric field is increased at a speed of from 0.1 (kV/mm)/sec or more to 5 (kV/mm)/sec or less, with applying the maximum electric field of from 2 kV/mm or more to 1.0 kV/mm or less.
摘要:
A monomorph type piezoelectric/electrostrictive device includes a piezoelectric/electrostrictive body, which is composed of a non-lead based piezoelectric/electrostrictive crystalline body containing at least Nb, Ta, and one or more types of alkali metal element, which has a cubic crystal structure at a temperature higher than the phase transition point and at least any one of tetragonal and orthorhombic crystal structures at a temperature lower than the phase transition point, and which is curved to a large extent by a polarization treatment to take on a curved shape at a temperature lower than the phase transition point without application of a voltage after the polarization treatment. In the polarization treatment, an electric field is increased at a speed of from 0.1 (kV/mm)/sec or more to 5 (kV/mm)/sec or less, with applying the maximum electric field of from 2 kV/mm or more to 1.0 kV/mm or less.
摘要:
Disclosed are piezoelectric materials in which electrical properties are improved, and manufacturing methods of the same. In (Li, Na, K, Bi)(Nb, Ta)O3 based piezoelectric materials, the surface microstructures of sintered bodies are constituted of microscopic grains having grain diameters of less than 5 μm, intermediate grains having grain diameters of 5 μm or more and less than 15 μm, and coarse grains having grain diameters of 15 μm or more and 100 μm or less.
摘要:
An alkali niobate-based piezoelectric/electrostrictive ceramics sintered body including, as a main crystal phase, a perovskite type oxide containing at least one type of element selected from the group consisting of Li, Na and K as A site constituent elements and at least one type of element selected from the group consisting of Nb and Ta as B site constituent elements. The number of lattice-strained layers of the piezoelectric/electrostrictive ceramics sintered body is preferably small. A diffuse scattering intensity ratio, which is a ratio of an intensity of diffuse scattering by a lattice-strained layer present near a domain wall to a sum of an X-ray diffraction intensity of a first lattice plane and that of a second lattice plane different in interplanar spacing from the first lattice plane due to crystallographic symmetry reduction is preferably 0.5 or lower.