摘要:
A process for obtaining aromatic sulfide polymer which has a markedly high molecular weight and can be readily formed into films, fibers, and other structures. The process comprises heating, in an aprotic solvent to a temperature of 100.degree. to 250.degree. C., (i) a dihaloaromatic compound and (ii) substantially anhydrous fine powder of the sulfide of an alkali or alkaline earth metal in the presence of (iii) substantially anhydrous fine powder of the carbonate of an alkali or alkaline earth metal, or of a mixture thereof with a hygroscopic inorganic salt and (iv) a strictly controlled very small amount of water dissolved in or solvated with the solvent.
摘要:
Disclosed herein are (1) a composition which is prepared by combining 0.2 to 90 parts by weight of a cross-linked polyarylene thioether having a melt viscosity of 5.times.10.sup.5 to 1.times.10.sup.9 poise, which becomes gel under melting, with 100 parts by weight of a resin consisting of polyarylene thioether, which has a repeating unit of ##STR1## as the main constituent, having a melt viscosity of 10 to 5.times.10.sup.4 poise and (2) a composition of polyarylene thioether for molding, which is prepared by combining not more than 400 parts by weight of a fibrous filler and/or an inorganic filler with 100 parts by weight of the above-mentioned composition (1), is excellent in an antiflash property, is high in a mechanical strength and a thermal stability and is easily processed on melt molding and can easily recycle its molded scraps.
摘要:
The improvement in a process for producing an aromatic sulfide polymer from (A) hydrous sulfide of an alkali or alkaline earth metal and (B) a dihalo-aromatic compound is disclosed. The improvement is concerned with how the hydrous sulfide is dehydrated and comprises dehydrating the hydrous sulfide by the action thereon of (C) an alkaline earth metal oxide before substantial formation of the aromatic sulfide polymer.
摘要:
A process for obtaining an aromatic sulfide polymer which has a markedly high molecular weight and can be readily formed into films, fibers, and other structures. The process comprises heating, to a temperature of 100.degree. to 270.degree. C. in an organic solvent under the coexistence of a very small amount of water, a dihaloaromatic compound and a substantially anhydrous amorphous vitreous compound composed of (i) S.sup.2- anions and other inorganic salt-forming anions and (ii) ions of an alkali metal and/or an alkaline earth metal.
摘要:
The invention provides a stretch blow molded container formed from a thermoplastic resin material which comprises polyglycolic acid having(a) a repeating unit represented by the following formula (1): ##STR1## (b) a melt viscosity, .eta.* [as measured at a temperature of (the melting point, Tm of the polymer+20.degree. C.) and a shear rate of 100/sec] of 500-100,000 Pa.s;(c) a melting point, Tm of at least 180.degree. C.;(d) a melt enthalpy, .DELTA.Hm of at least 20 J/g; and(e) a density of at least 1.50 g/cm.sup.3 as measured in an unoriented, crystallized form,wherein the stretch blow molded container has tensile strength (in a circumferential direction) of at least 100 MPa and a carbon dioxide permeability (as measured at a temperature of 23.degree. C. and 80% relative humidity; in terms of the thickness of 50 .mu.m) of 300 cc/m.sup.2.day.atm or smaller at the body sidewall thereof, and a production process thereof.
摘要:
The invention provides a stretch blow molded container formed from a thermoplastic resin material which comprises polyglycolic acid having(a) a repeating unit represented by the following formula (1): ##STR1## (b) a melt viscosity, .eta.* [as measured at a temperature of (the melting point, Tm of the polymer+20.degree. C.) and a shear rate of 100/sec] of 500-100,000 Pa.multidot.s;(c) a melting point, Tm of at least 180.degree. C.;(d) a melt enthalpy, .DELTA.Hm of at least 20 J/g; and(e) a density of at least 1.50 g/cm.sup.3 as measured in an unoriented, crystallized form,wherein the stretch blow molded container has tensile strength (in a circumferential direction) of at least 100 MPa and a carbon dioxide permeability (as measured at a temperature of 23.degree. C. and 80% relative humidity; in terms of the thickness of 50 .mu.m) of 300 cc/m.sup.2 .multidot.day.multidot.atm or smaller at the body sidewall thereof, and a production process thereof.
摘要翻译:本发明提供一种由热塑性树脂材料形成的拉伸吹塑成型容器,该容器包含聚乙醇酸,该聚乙醇酸具有(a)由下式(1)表示的重复单元:(b)熔体粘度eta * [在 (熔点,聚合物的Tm + 20℃)和100 /秒的剪切速率]为500-10000Pax; (c)熔点Tm为至少180℃。 (d)熔体焓,至少20J / g的DELTA Hm; 和(e)以非取向的结晶形式测量的至少1.50g / cm 3的密度,其中拉伸吹塑成型容器的拉伸强度(在圆周方向)为至少100MPa,二氧化碳渗透性(测量 在23℃和80%相对湿度的温度下,在其体侧壁为300cc / m 2×day×atm以下的厚度为50μm),及其制造方法。
摘要:
A controlled release pharmaceutical composition comprises (a) at least one pharmaceutically active substance having a water contact angle (θ) such that cos θ is between +0.9848 and −0.9848, (b) a first intelligent polymer component; and (c) a second intelligent polymer component having opposite wettability characteristics to the first intelligent polymer component, the first and second polymer components being present in a ratio in the range of about 1:100 to about 100:1 by weight. The polymer components are effective for controlled release of the pharmaceutically active substance from the composition.
摘要:
The invention provides an injection-molded product of polyglycolic acid obtainable by molding a thermoplastic resin material at an injection temperature ranging from the melting point, Tm of the polymer to 255° C., wherein the thermoplastic resin material comprises polyglycolic acid having a repeating unit represented by the following formula (1): and the following physical properties: (a) the melt viscosity, &eegr;* [as measured at a temperature of (the melting point, Tm of the polymer+20° C.) and a shear rate of 1,000/sec] being 30-10,000 Pa·s; (b) the melting point, Tm being at least 150° C.; (c) the melt enthalpy, &Dgr;Hm being at least 20 J/g; and (d) the density being at least 1.50 g/cm3 as measured in an unoriented, crystallized form, and a production process thereof.
摘要:
The invention provides an oriented polyglycolic acid film formed from a thermoplastic resin material which comprises polyglycolic acid having a repeating unit represented by the following formula (1): ##STR1## and the following physical properties: (a) the melt viscosity, .rho.* �as measured at a temperature of (the melting point, Tm of the polymer+20.degree. C.) and a shear rate of 100/sec! being 500-100,000 Pa.s; (b) the melting point, Tm being at least 150.degree. C.; (c) the melt enthalpy, .DELTA.Hm being at least 20 J/g; and (d) the density being at least 1.50 g/cm.sup.3 as measured in an unoriented, crystallized form, wherein the film has tensile strength of at least 150 MPa, and production processes thereof.
摘要:
Disclosed herein are an aromatic thioether ketone/thioether sulfone random copolymer comprising phenylene thioether ketone recurring units (I) and phenylene thioether sulfone recurring units (II), (a) the compositional ratio (I:II) of the recurring units (I) to the recurring units (II) ranging from 98:2 to 65:35, (b) the solution viscosity (.eta..sub.inh) being at least 0.3 dl/g, (c) the melt crystallization time (f) being at least 3 minutes, (d) the melting point (Tm) being 300.degree.-350.degree. C., (e) the glass transition temperature being at least 125.degree. C., (f) the retention (400.degree. C./20 min) of melt crystallization enthalpy (.DELTA.Hmc) being at least 60%, and (g) the average particle size being at least 0.1 mm, and the production process thereof.