Abstract:
A piece of jewelry having a copper-containing gold alloy consists of 58.5 to 58.7 wt. % gold, 26.9 to 32.6 wt. % copper, 5.7 to 10.7 wt. % silver, 1.0 to 3.0 wt. % palladium, and a remainder containing 0.7 to 2.2 wt. % zinc.
Abstract:
A castable, moldable, or extrudable magnesium-based alloy that includes one or more insoluble additives. The insoluble additives can be used to enhance the mechanical properties of the structure, such as ductility and/or tensile strength. The final structure can be enhanced by heat treatment, as well as deformation processing such as extrusion, forging, or rolling, to further improve the strength of the final structure as compared to the non-enhanced structure. The magnesium-based composite has improved thermal and mechanical properties by the modification of grain boundary properties through the addition of insoluble nanoparticles to the magnesium alloys. The magnesium-based composite can have a thermal conductivity that is greater than 180 W/m-K, and/or ductility exceeding 15-20% elongation to failure.
Abstract:
Eyewear and eyewear structures comprising bulk-solidifying amorphous alloys and methods of making eyewear structures from such bulk-solidifying amorphous alloys are described. The bulk-solidifying amorphous alloys provide form and shape durability, the minimum use of fasteners in the eyewear structure, high resistance to chemical and environmental effects, and low-cost net-shape fabrication for intricate eyewear design and shapes.
Abstract:
Disclosed are embodiments of a vessel configured to contain a secondary magnetic induction field therein for melting materials, and methods of use thereof. The vessel can be used in an injection molding apparatus having an induction coil positioned adjacent to the vessel. The vessel can have a tubular body configured to substantially surround and receive a plunger tip. Longitudinal slots or gaps extend through the thickness of the body to allow and/or direct eddy currents into the vessel during application of an RF induction field from the coil. The body also includes temperature regulating lines configured to flow a liquid within. The temperature regulating lines can be provided to run longitudinally within the wall(s) of the body between its inner bore and outer surface(s). A flange may be provided at one end of the body to secure the body within an injection molding apparatus.
Abstract:
A method for manufacturing a bioresorbable implant, wherein a magnesium alloy is formed into an implant. A melt is pressed into a die and gases in the die induce turbulence in the inflowing melt, thereby enclosing gas, so that the porous implant is formed with a porosity, which increases from outside inwardly. The surface of the implant is substantially free from open pores.
Abstract:
Described herein is a method of selectively depositing molten bulk metallic glass (BMG). In one embodiment, a continuous stream or discrete droplets of molten BMG is deposited to selected positions. The deposition can be repeated as needed layer by layer. One or more layers of non-BMG can be used as needed.
Abstract:
An amorphous and a manufacturing method thereof are provided. The amorphous alloy may have a formula of ZraCubAlcMdNe, M is at least one selected from the group consisting of Ni, Fe, Co, Mn, Cr, Ti, Hf, Ta, Nb and rare earth elements; N is at least one selected from a group consisting of Ca, Mg, and C; 40≦a≦70, 15≦b≦35, 5≦c≦15, 5≦d≦15, 0≦e≦2, and a+b+c+d+e=100.
Abstract:
A method comprising introducing a first casting material into a casting mold; applying directional solidification to the first casting material in the casting mold; introducing a second casting material into the casting mold, the second casting material having a different chemical composition than the first casting material; applying directional solidification to the second casting material in the casting mold; and forming a molded article, wherein the molded article comprises a first region.
Abstract:
Described herein is a crucible with a rod fused thereon to optimize pouring of molten material, and method of using the same. The crucible has a body configured for receipt of an amorphous alloy material in a vertical direction, and the rod extends in a horizontal direction from the body. The body of the crucible and the rod are formed from silica or quartz. The rod may be fused to the body of the crucible and provided off a center axis so that pouring molten material is improved when the crucible is rotated.
Abstract:
Disclosed herein is a device comprising: vacuum chamber; a stage configured to receive BMG in a molten state or a BMG feedstock, configured to spin, and located in the vacuum chamber; a heater configured to melt the BMG feedstock or to keep BMG in a molten state molten; wherein the stage comprises one or more conduits therein and the conduits are configured to accommodate a cooling fluid. Also disclosed herein is a method of forming a solid BMG sheet, the method comprising: disposing BMG in a molten state onto a stage; spreading the BMG in a molten state into a sheet of BMG in a molten state by spinning the stage; cooling the sheet of BMG in a molten state to form a solid BMG sheet.