摘要:
A process for copper coating printed circuit boards is disclosed. The process includes a treating step in which a metal surface is contacted with an adhesion promotion composition material. The adhesion promotion material includes 0.1 to 20% by weight hydrogen peroxide, an inorganic acid, an organic corrosion inhibitor and a surfactant.
摘要:
An improved process for forming a zinc phosphate coating on a zinc surface comprises contacting the surface with an aqueous nitrate and ammonia-free solution containing zinc, phosphate, nickel or cobalt, and hydrogen peroxide.
摘要:
A COMPOSITION AND PROCESS FOR THE TREATMENT OF FERROUS METAL SURFACES UTILIZING A NITRITE ACCELERATED ZINC PHOSPHATE TREATING SOLUTION, WHEREIN UNDESIRED CONCENTRATIONS OF FERRO-NITROSO COMPLEXES ARE PREVENTED BY INCORPORATING IN THE PHOSPHATING BATH A PEROXIDE CONTAINING SULFUR OXYGEN COMPOUND. EXEMPLARY OF PREFERRED COMPOUNDS WHICH MAY BE USED ARE NA2S2O8 AND H2SO5.
摘要:
An acidic phosphating solution for coating metal surfaces comprising (1) zinc phosphate (2) an acid radical derived from peroxy disulphuric acid, peroxy diphosphoric acid, peroxy diboric acid or peroxy dicarbonic acid and (3) a conventional phosphating accelerator.
摘要:
The invention relates to a coating agent for coating acid-sensitive metal surfaces, which is an aqueous solution of an acidic phosphate binder, the coating agent comprising a peroxo compound and being free of chromium (VI) salts. The invention further relates to a method of coating a metal surface with such a coating agent, and to the use of such a coating agent for increasing the corrosion resistance of metal components in various industrial fields.
摘要:
A zinc phosphate-type conversion film having microfine-sized crystals is formed on metal surfaces using a conversion treatment bath that contains zinc ions and phosphate ions along with 50 to 1500 ppm of an organoperoxide conversion accelerator, and optionally surfactant. Surface-conditioning treatments can be omitted from this method. The presence of the surfactant makes possible simultaneous execution of surface cleaning and conversion treatment
摘要:
A continuous process for coating ferrous or zinciferous metal substrates using an acidic coating solution of zinc phosphate in the presence of hydrogen peroxide wherein (a) the molar ratio ortho phosphate/zinc in solution is maintained in the range 0.5-3.7, and (b) the coating solution is replenished with hydrogen peroxide, replenishment feed (i) (comprising zinc, ortho phosphate and anion N.sup.n-), and replenishment feed (ii) (comprising alkali), the ratio of the quantities of (i) and (ii) being defined. The acid H.sub.n N has a pK.sub.a value not greater than 3.
摘要:
A method for the treatment or pre-treatment of surfaces of metal objects by means of an acidic, aqueous solution containing zinc and phosphate. The phosphating solution contains between 0.1-10 g/L, zinc, 4-50 g/L phosphate calculated as PO4, between 0.03-3 g/L, of at least one guanidine compound comprising at least one nitro group calculated as nitroguanidine, and between 0.001-0.9 g/L hydrogen peroxide and has a temperature of less than 80° C. The corresponding acidic, aqueous composition and finished products are also disclosed.
摘要:
The invention relates to a phosphating solution and a process for the phosphating of metallic surfaces with aqueous, acidic phosphating solutions that comprise zinc and phosphate ions, at least one source of peroxide and one or more aliphatic chelating carboxylic acids containing 2 to 7 carbon atoms; the phosphating solution having a free acid content of one point or less.
摘要:
The invention relates to a method for the treatment or pre-treatment of surfaces of metal objects by means of an acidic, aqueous solution containing zinc and phosphate. Said invention is characterised in that the phosphating solution contains between 0.1-10 g/L zinc, 4-50 g/L phosphate calculated as PO4, between 0.03-3 g/L of at least one guanidine compound comprising at least one nitro group calculated as nitroguanidine, and between 0.001-0.9 g/L hydrogen peroxide and has a temperature of less than 80° C. The invention also relates to a corresponding acidic, aqueous composition.