HYDROTHERMAL SYNTHESIS OF ALKALI PROMOTED MOS2-BASED CATALYST
    6.
    发明申请
    HYDROTHERMAL SYNTHESIS OF ALKALI PROMOTED MOS2-BASED CATALYST 审中-公开
    碱性促进的基于MOS2的催化剂的氢热合成

    公开(公告)号:WO2016070161A8

    公开(公告)日:2017-02-23

    申请号:PCT/US2015058526

    申请日:2015-10-31

    IPC分类号: B01J23/28

    摘要: Certain embodiments are directed to method for making and using an alkali promoted transition metal sulfide Fischer Tropsch catalyst. Certain embodiments are directed to alkali promoted transition metal sulfide Fischer Tropsch catalyst synthesized using steps comprising (i) mixing an ammonium tetrathiomolybdate (ATM) precursor compound with an alkali metal compound and molybdenium disulfide in deionized water to form a reaction mixture, (ii) heating the reaction mixture at a temperature of at least 200, 250, 300, 350, 400C at a pressure of at lease 900, 1000, 1100, 1500, 2000 psi for more than 0.5 1, 1.5, 2.0, 3 or more hours to form a reaction product, (iii) filtering, washing, and drying the reaction product.

    摘要翻译: 某些实施方案涉及制备和使用碱促进的过渡金属硫化物费 - 托催化剂的方法。 某些实施方案涉及使用以下步骤合成的碱促进的过渡金属硫化物费 - 托催化剂:(i)将四硫代钼酸铵(ATM)前体化合物与碱金属化合物和二硫化钼在去离子水中混合以形成反应混合物,(ii)加热 所述反应混合物在至少200,250,300,350,400℃的温度下在900,1000,1001,500,500psi的压力下超过0.5,1,1.5,2.0,3或更多小时以形成 反应产物,(iii)过滤,洗涤和干燥反应产物。

    HYDROTHERMAL SYNTHESIS OF ALKALI PROMOTED MOS2-BASED CATALYST
    9.
    发明申请
    HYDROTHERMAL SYNTHESIS OF ALKALI PROMOTED MOS2-BASED CATALYST 审中-公开
    碱性促进的基于MOS2的催化剂的氢热合成

    公开(公告)号:WO2016070161A1

    公开(公告)日:2016-05-06

    申请号:PCT/US2015/058526

    申请日:2015-10-31

    IPC分类号: B01J23/28

    摘要: Certain embodiments are directed to method for making and using an alkali promoted transition metal sulfide Fischer Tropsch catalyst. Certain embodiments are directed to alkali promoted transition metal sulfide Fischer Tropsch catalyst synthesized using steps comprising (i) mixing an ammonium tetrathiomolybdate (ATM) precursor compound with an alkali metal compound and molybdenium disulfide in deionized water to form a reaction mixture, (ii) heating the reaction mixture at a temperature of at least 200, 250, 300, 350, 400C at a pressure of at lease 900, 1000, 1100, 1500, 2000 psi for more than 0.5 1, 1.5, 2.0, 3 or more hours to form a reaction product, (iii) filtering, washing, and drying the reaction product.

    摘要翻译: 某些实施方案涉及制备和使用碱促进的过渡金属硫化物费 - 托催化剂的方法。 某些实施方案涉及使用以下步骤合成的碱促进的过渡金属硫化物费 - 托催化剂:(i)将四硫代钼酸铵(ATM)前体化合物与碱金属化合物和二硫化钼在去离子水中混合以形成反应混合物,(ii)加热 所述反应混合物在至少200,250,300,350,400℃的温度下在900,1000,1001,500,500psi的压力下超过0.5,1,1.5,2.0,3或更多小时以形成 反应产物,(iii)过滤,洗涤和干燥反应产物。