Abstract:
The present invention relates to a substrate (1) coated with a porous layer (2), to the processes for manufacturing the layer and to its applications. The porous layer (2) is mainly inorganic and of sol-gel type having a series of closed pores with at least the smallest characteristic dimension which is, on average, greater than or equal to 20 nm and less than or equal to 100 nm.
Abstract:
A synthetic fire opal and a process for its preparation. Synthetic fire opals have similar physical and chemical properties as natural fire opals. Synthetic fire opals are colored, hard, and transparent. The process of preparation of synthetic fire opal includes; mixing TEOS with absolute ethanol (99.9%), distilled water, concentrated nitric acid, and an inorganic salt to form a clear sol, storing the clear sol to obtain a gel, drying the gel and sintering the dried gel to obtain a synthetic fire opal.
Abstract:
본 발명은 태양전지 모듈 제조에 사용되는 유리에 코팅을 하여 투과율을 증대시켜 주는 코팅액의 제조방법과 상기 방법에 의하여 제조된 코팅액 조성물에 관한 것이다. 종래에 빛의 투과를 증가시키기 위해 고굴절률 층과 저굴절율의 층을 교대로 적층하거나 반사방지용 광촉매 코팅을 하거나 알콕시 실란의 다공성 구조를 이용하였으나 정밀한 적층이 어렵거나 원가가 비싸거나 코팅액의 저장안정성이 제한되는 등의 단점이 있어 사용이 어려웠다. 본 발명은 이러한 단점을 극복하기 위하여 안출된 것으로서, 수십에서 수백 나노의 무기 입자를 충진 형태로 배열을 하여 다공성 구조와 유사한 배열을 가지도록 하되 다공성 구조가 가지는 투과율 증대의 특성을 유지하면서 충진물의 기계적인 특성으로 경도를 향상시키도록 한다.
Abstract:
L'invention a trait à un procédé de préparation d'une solution sol-gel stable comprenant successivement les étapes suivantes : a) préparer une solution sol-gel par mise en contact d'un ou plusieurs précurseurs moléculaires de métal et/ou de métalloïde avec un milieu comprenant un solvant organique; b) ajouter à la solution obtenue en a) au moins un composé mercaptoorganosilane ; c) hydrolyser la solution obtenue en b) ; d) ajouter à la solution obtenue en c) un ou plusieurs agents complexants choisis parmi les acides carboxyliques, les composés β-dicétones, les composés hydroxamates . Utilisation de cette solution pour constituer des matériaux de revêtements de substrats métalliques, en particulier de substrat à base d'argent, tel que les miroirs.
Abstract:
Ein bekanntes Verfahren zur Herstellung eines Quarzglasbauteils mit hoher thermischer Stabilität umfasst das Bereitstellen eines Basiskörpers, dessen Oberflache mindestens teilweise mit einer Schicht versehen wird, die ein Kristallisationspromotor-lon in einer Silicatverbindung enthält, wobei durch Erhitzen beim bestimmungsgemassen Einsatz des Quarzglasbauteils von der Schicht eine Cristobalitbildung ausgeht. Um dieses Verfahren hinsichtlich seiner Reproduzierbarkeit and Wirtschaftlichkeit zu verbessern, wird erfindungsgemäss vorgeschlagen, class durch Hydrolyse einer das Kristallisationspromotor-Ion and eine hydrolysierbare Siliciumverbindung enthaltenden Lösung ein Sol gebildet wird, in weichem kolloidale Teilchen der hydrolysierten Siliciumverbindung and des Kristallisationspromotor-Ions vorliegen, dass das Sol unter Bildung der Schicht auf der Basiskörper-Oberfläche aufgetragen wird, and class anschliessend durch Kondensation der hydrolysierten Siliciumverbindung unter Vernetzung der kolloidalen Teilchen eine Silicatbildung in der Schicht erfolgt.
Abstract:
The present invention relates to a method for preparing a coating liquid for increasing the transmittance of glass used in the manufacture of a solar cell module when coated on said glass, and to a coating solution composition prepared by the method. In the prior art, in order to increase light transmittance, high and low refractive index layers are alternately stacked, an antireflection optical catalyst coating is implemented, or a porous alkoxysilane structure is used. However, these methods are difficult to employ because of the drawbacks thereof, such as the difficulty in precision stacking, high costs, or the limited storage stability of the coating liquid. Therefore, the present invention is proposed to overcome such drawbacks by filling and arranging inorganic particles, the size of which is several tens to several hundreds of nanometers, such that the inorganic particles form an array structure similar to a porous structure in order to exhibit the property of a porous structure of improving transmittance, while improving hardness due to the mechanical features of the filled inorganic particles.
Abstract:
La présente invention porte sur un substrat revêtu(1)d une couche poreuse (2), les procédés de fabrication de la couche et ses applications. La couche poreuse (2) estessentiellement minérale et de type sol-gel présentant une série de pores fermés avec au moins la plus petite dimension caractéristique qui est, en moyenne, supérieure ou égale à 20 nm et inférieure ou égale à 100 nm.
Abstract:
The invention concerns a method for preparing a stable sol-gel solution including the following successive steps: a) preparing a sol-gel solution by contacting one or more metal and/or metalloid precursors with a medium comprising an organic solvent; b) adding to the solution obtained at a) at least one mercaptoorganosilane compound; c) hydrolyzing the solution obtained at b); d) adding to the solution obtained at c) one or more complexing agents selected among carboxylic acids, ß-diketone compounds, hydroxamate compounds. The invention also concerns the use of said solution for forming coating materials for metal substrates, in particular silver-based substrate, such as mirrors.
Abstract:
Es wird ein Verfahren angegeben, das die wirtschaftliche Herstellung eines Rohlings für ein Bauteil aus laseraktivem Quarzglas in beliebiger Form und Abmessung ermöglicht. Das Verfahren umfasst die folgenden Verfahrensschritte: a) Bereitstellen einer Dispersion mit einem Feststoffgehalt von mindestens 40 Gew.-%, die Si0 2 -Nanopulver sowie Dotierstoffe umfassend ein Kation der Seltenerdmetalle und der Übergangsmetalle in einer Flüssigkeit enthält, b) Granulation durch Bewegen der Dispersion unter Entzug von Feuchtigkeit bis zur Bildung eines dotierten Si0 2 -Granulats aus sphärischen, porösen Granulatkörnern mit einem Feuchtigkeitsgehalt von weniger als 35 Gew.-% und mit einer Dichte von mindestens 0,95 g/cm 3 , c) Trocknen und Reinigen des Si0 2 -Granulats durch Aufheizen auf eine Temperatur von mindestens 1000 °C unter Bildung einer dotierten, porösen Si0 2 Körnung mit einem OH-Gehalt von weniger als 10 ppm; und d) Sintern oder Erschmelzen der dotierten SiO 2 -Körnung in einer reduzierend wirkenden Atmosphäre unter Bildung des Rohlings aus dotiertem Quarzglas.