摘要:
A ceramic composite laminate includes a wavelength-converting layer and a non-emissive layer, wherein the ceramic composite laminate has a wavelength conversion efficiency (WCE) of at least 0.650. The ceramic composite laminate can also include a wavelength-converting ceramic layer comprising an emissive material and a scattering material, wherein the laminated composite has a total transmittance of between about 40% to about 85%. The wavelength-converting layer may be formed from plasma YAG:Ce powder.
摘要:
Disclosed herein are emissive ceramic materials having a dopant concentration gradient along a thickness of a yttrium aluminum garnet (YAG) region. The dopant concentration gradient may include a maximum dopant concentration, a half-maximum dopant concentration, and a slope at or near the half-maximum dopant concentration. The emissive ceramics may, in some embodiments, exhibit high internal quantum efficiencies (IQE). The emissive ceramics may, in some embodiments, include porous regions. Also disclosed herein are methods of make the emissive ceramic by sintering an assembly having doped and non-doped layers.
摘要:
Some embodiments provide luminescent ceramics which have a lower amount of dopant than conventional luminescent ceramics. In some embodiments, the luminescent ceramic comprises a host material comprising a rare earth element and at least one rare earth dopant, wherein the rare earth dopant may be about 0.01% to 0.5% of the rare earth atoms present in the material. Some embodiments provide luminescent ceramic comprising: a polycrystalline phosphor represented by the formula (A 1-x E x ) 3 B 5 O 12 . Some embodiments provide a light-emitting device comprising a luminescent ceramic disclosed herein.
摘要:
There is provided a photocatalyst sheet comprising a base material and a photocatalyst layer containing at least a photocatalyst, wherein the photocatalyst layer is firmly adhered to the base material. In an embodiment, there is provided a photocatalyst sheet comprising a base material; and a photocatalyst layer that contains at least a photocatalyst, and is formed on at least one surface of the base material through an aerosol deposition method. This photocatalyst sheet has an excellent photocatalytic activity and an excellent adhesion.
摘要:
Embodiments of the present invention include a filter element for decomposing contaminants including a substrate, and a photocatalytic composition comprising at least a photocatalyst. The embodiments of the present invention also includes a system for decomposing contaminants including a substrate, and a photocatalytic composition comprising at least a photocatalyst; and a method using the system.
摘要:
A method for forming an oxide coated substrate comprising heating a pre-coating mixture in the presence of a substrate to synthesize an oxide coating on the substrate. The pre-coating mixture comprises a solubilized reducing additive, a solubilized oxidizing additive, and the substrate. The heating is conducted at a temperature sufficiently high enough to exothermically react the solubilized reducing additive and solubilized oxidizing additive and low enough to control the phase and composition of the oxide.