Abstract:
A composition comprising: a first polycarbonate comprising a poly(siloxane-carbonate); a second polycarbonate different from the first polycarbonate; and optionally, a third polycarbonate different from the first and second polycarbonate; wherein the first polycarbonate is present in an amount effective to provide the siloxane units of in the first polycarbonate in an amount of at least 0.3 wt %, and the second polycarbonate is present in an amount effective to provide the bromine of the second polycarbonate in an amount of at least 7.8 wt %; and further wherein an article molded from the composition has an OSU integrated 2 minute heat release test value of less than 65 kW-min/m2 and a peak heat release rate of less than 65 kW/m2, and an E662 smoke test Dmax value of less than 200.
Abstract:
This disclosure relates to polycarbonate compositions, methods, and articles of manufacture that at least meets certain electrical tracking resistance requirements. The compositions, methods, and articles of manufacture that meet these requirements contain at least a polycarbonate; a polysiloxane block co-polycarbonate; and a transition metal oxide, e.g. titanium dioxide.
Abstract:
A composition comprising: a first polymer comprising a poly(etherimide-siloxane) copolymer comprising (a) a repeating polyetherimide unit, and (b) a poly(siloxane) block unit, a second polymer different from the first polymer and comprising bromine; and optionally, a third polymer comprising a polycarbonate different from the first polymer and second polymer; wherein polysiloxane block units are present in the composition in an amount of at least 0.3 wt %, and bromine is present in the composition in an amount of at least 7.8 wt %, each based on the sum of the wt % of the first, second, and third polymers; and further wherein an article molded from the composition has an OSU integrated 2 minute heat release test value of less than 65 kW-min/m2 and a peak heat release rate of less than 65 kW/m2, and an E662 smoke test Dmax value of less than 200.
Abstract:
A poly(siloxane) copolymer composition comprising: a first polymer comprising a first repeating unit, and a poly(siloxane) block unit, a second polymer different from the first polymer and comprising of bromine; and optionally, one or more third polymers different from the first polymer and second polymer; wherein siloxane units are present in the composition in an amount of at least 0.3 wt%, and bromine is present in the composition in an amount of at least 7.8 wt%, each based on the sum of the wt% of the first, second, and optional one or more third polymers; and further wherein an article molded from the composition has an OSU integrated 2 minute heat release test value of less than 65 kW-min/m2 and a peak heat release rate of less than 65 kW/m2, and an E662 smoke test Dmax value of less than 200.
Abstract:
A composition comprising: a first polycarbonate comprising a poly(siloxane-carbonate); a second polycarbonate different from the first polycarbonate; and optionally, a third polycarbonate different from the first and second polycarbonate; wherein the first polycarbonate is present in an amount effective to provide the siloxane units of in the first polycarbonate in an amount of at least 0.3 wt %, and the second polycarbonate is present in an amount effective to provide the bromine of the second polycarbonate in an amount of at least 7.8 wt %; and further wherein an article molded from the composition has an OSU integrated 2 minute heat release test value of less than 65 kW-min/m2 and a peak heat release rate of less than 65 kW/m2, and an E662 smoke test Dmax value of less than 200.
Abstract:
A poly(siloxane) copolymer composition comprising: a first polymer comprising a first repeating unit, and a poly(siloxane) block unit, a second polymer different from the first polymer and comprising of bromine; and optionally, one or more third polymers different from the first polymer and second polymer; wherein siloxane units are present in the composition in an amount of at least 0.3 wt %, and bromine is present in the composition in an amount of at least 7.8 wt %, each based on the sum of the wt % of the first, second, and optional one or more third polymers; and further wherein an article molded from the composition has an OSU integrated 2 minute heat release test value of less than 65 kW-min/m2 and a peak heat release rate of less than 65 kW/m2, and an E662 smoke test Dmax value of less than 200.