摘要:
Embodiments disclosed herein relate to using cobalt (Co) to fine tune the magnetic properties, such as permeability and magnetic loss, of nickel-zinc ferrites to improve the material performance in electronic applications. The method comprises replacing nickel (Ni) with sufficient Co +2 such that the relaxation peak associated with the Co +2 substitution and the relaxation peak associated with the nickel to zinc (Ni/Zn) ratio are into near coincidence. When the relaxation peaks overlap, the material permeability can be substantially maximized and magnetic loss substantially minimized. The resulting materials are useful and provide superior performance particularly for devices operating at the 13.56 MHz ISM band.
摘要:
Embodiments disclosed herein relate to using cobalt (Co) to fine tune the magnetic properties, such as permeability and magnetic loss, of nickel-zinc ferrites to improve the material performance in electronic applications. The method comprises replacing nickel (Ni) with sufficient Co +2 such that the relaxation peak associated with the Co +2 substitution and the relaxation peak associated with the nickel to zinc (Ni/Zn) ratio are into near coincidence. When the relaxation peaks overlap, the material permeability can be substantially maximized and magnetic loss substantially minimized. The resulting materials are useful and provide superior performance particularly for devices operating at the 13.56 MHz ISM band.
摘要:
The invention concerns a ferrite magnet comprising a magnetoplumbite phase of formula M1-xRxFe12-yTyO19, wherein: M represents at least an element selected among the group consisting of: Sr, Ba, Ca and Pb; R represents at least an element selected among rare earths and Bi; T represents at least an element selected among Co, Mn, Ni, Zn; 0,15
摘要:
A ceramic composite is a mixed conducting oxide that has a perovskite type crystal structure of {Ln 1-a A a }{B x B' y B'' z }O (3-δ) where a, x, y, and z are within the range of 0.8 ≤ a ≤ 1, 0 x O (3-δ) , the composite formula is constituted, A is selected out of Ba, Sr, and Ca, and is within the range of 0.98 ≤ x ≤ 1.02, and δ denotes a value determined so as to meet the charge neutralization conditions.
摘要:
A method comprising the steps of mixing raw material powders to a composition comprising metal elements of Ca, La, Sr, Ba, Fe and Co, whose atomic ratios are represented by the general formula of Ca 1-x-y La x (Sr y' Ba 1-y' ) y Fe 2n-z Co z , wherein 1-x-y, x and y are values in a region defined by a coordinate a: (0.470, 0.297, 0.233), a coordinate b: (0.300, 0.392, 0.308), a coordinate c: (0.300, 0.300, 0.400), a coordinate d: (0.400, 0.200, 0.400) and a coordinate e: (0.470, 0.200, 0.330) in a ternary diagram of x, y, and 1-x-y; y' and z, and n representing a molar ratio meet 0.5 ≤ y' ≤ 1, 0.2 ≤ z 2 being added to the raw material powder mixture, the calcined body or the calcined powder; and 0-2% by mass (as CaO) of CaCO 3 being added to the calcined body or the calcined powder.
摘要翻译:一种方法,包括以下步骤:将原料粉末与包含Ca,La,Sr,Ba,Fe和Co的金属元素的组合物混合,其原子比由通式Ca 1-xy La x(Sr y Ba) 1-y')y Fe 2n-z Co z,其中1-xy,x和y是由坐标a:(0.470,0.27,0.233),坐标b:(0.300,0.392,0.308)定义的区域中的值 ),x,y和1-xy的三元图中的坐标c:(0.300,0.300,0.400),坐标d:(0.400,0.200,0.400)和坐标e:(0.470,0.200,0.330) ; y'和z,n表示摩尔比满足0.5‰¤‰¤1,0.2‰¤z <0.25和5.2
摘要:
Disclosed is a polycrystalline diamond or diamond-like element with greatly improved wear resistance without loss of impact strength. These elements are formed with a binder-catalyzing material in a high-temperature, high-pressure (HTHP) process. The PCD element has a body with a plurality of bonded diamond or diamond-like crystals forming a continuous diamond matrix that has a diamond volume density greater than 85 %. Interstices among the diamond crystals form a continuous interstitial matrix containing a catalyzing material. The diamond matrix table is formed and integrally bonded with a metallic substrate containing the catalyzing material during the HTHP process. The diamond matrix body has a working surface, where a portion of the interstitial matrix in the body adjacent to the working surface is substantially free of the catalyzing material, and the remaining interstitial matrix contains the catalyzing material. Typically, less than about 70 % of the body of the diamond matrix table is free of the catalyzing material.
摘要:
Die Erfindung betrifft einen modifizierten Strontiumferrit der allgemeinen chemischen Formel
Sr 1-x La x Fe 12-y CO y O 19
X = y = 0,01 - 1,00 bzw. X = 0,15 und y = x/1,6n bis = x/2,6n, wobei n das eingesetzte Verhältnis Fe 2 O 3 : SrO ist und 5-6 sein kann. Erfindungsgemäß werden Lanthan und Kobalt in einer Menge zugegeben, sodass gilt, 0,14 ≤ x ≤ 0,145 und 0,14 ≤ y ≤ 0,145. Der so hergestellte modifizierte Strontiumferrit hat ausgezeichnete magnetische Eigenschaften sowohl hinsichtlich der Remanenz B R , der Koerzitivfeldstärke H CJ als auch des Verhältnisses H K zu H CJ .
摘要翻译:改性锶铁氧体是新的。 式(Sr 1-x La x Fe 1 2 -yCo yO 9)的改性锶铁氧体是新的。 x,y:0.14-0.145,优选0.142。 还包括用于生产改性锶铁氧体的独立权利要求。