Stretch packaging film
    4.
    发明专利
    Stretch packaging film 有权
    拉伸包装膜

    公开(公告)号:JP2012162074A

    公开(公告)日:2012-08-30

    申请号:JP2012001729

    申请日:2012-01-09

    IPC分类号: B32B27/32

    摘要: PROBLEM TO BE SOLVED: To provide a packaging film that is well suited for packaging machinery using an automatic packaging machine, in which slackening does not occur during long-term low temperature storage and in which high-stretch packaging does not cause whitening of the film.SOLUTION: A stretch packaging film formed by a laminate film comprising at least three layers, wherein both surface layers contain an ethylene-based resin (A) component as a primary component, and an interlayer includes, a propylene-based resin (B) component satisfying following conditions (1) and (2) and a propylene-based resin (C) component satisfying a following condition (3), wherein the crystallization heat is 10-60 J/g, and the storage modulus is 100 MPa-1 GPa. (1) The peak of the crystallization curve when measured with DSC is a single. (2) The crystallization peak temperature in (1) is ≥70°C and a heat amount of crystallization is ≤10J/g. (3) The value of the heat amount of crystallization when measured at DSC has a value larger than the heat amount of crystallization of the propylene resin (B).

    摘要翻译: 要解决的问题:提供一种非常适合于使用自动包装机的包装机械的包装膜,其中在长期低温储存期间不会发生松弛,并且其中高拉伸包装不会引起白化 的电影。 解决方案:由包含至少三层的层压膜形成的拉伸包装膜,其中两个表面层包含基于乙烯的树脂(A)成分作为主要成分,并且中间层包括丙烯类树脂( B)满足以下条件(1)和(2)的组分和满足以下条件(3)的丙烯类树脂(C)组分,其中结晶热为10-60J / g,储能模量为100MPa -1 GPa。 (1)用DSC测定结晶曲线的峰值为单峰。 (2)(1)中的结晶峰温度≥70℃,结晶热量≤10J/ g。 (3)DSC测定时的结晶热量的值比丙烯类树脂(B)的结晶热量大。 版权所有(C)2012,JPO&INPIT

    Resin molded product and electronic equipment using the same and method for treating resin molded product
    7.
    发明专利
    Resin molded product and electronic equipment using the same and method for treating resin molded product 审中-公开
    树脂模制产品和使用它的电子设备和处理树脂模制产品的方法

    公开(公告)号:JP2007106783A

    公开(公告)日:2007-04-26

    申请号:JP2005296071

    申请日:2005-10-11

    摘要: PROBLEM TO BE SOLVED: To provide a resin molded product capable of improving a biodegradable rate and electronic equipment using the molded product and to provide a method for treating the resin molded product in which biodegradable rate can be improved. SOLUTION: The resin molded product 10 comprises a molded base material 11 composed of a biodegradable resin, and a coated film 12 formed on the surface of the molded base material 11, wherein the coated film 12 comprises a petroleum-based coating material, a natural material and a proliferation promoter for promoting proliferation of microorganisms, e.g. a carbohydrate or an amino acid. The resin molded product 10 proliferates microorganisms in soil by the proliferation promoter and improves biodegradable rate of the resin molded product 10. COPYRIGHT: (C)2007,JPO&INPIT

    摘要翻译: 要解决的问题:提供能够提高生物降解速度的树脂成型体和使用该成型体的电子设备,提供可以提高生物降解率的树脂成型体的处理方法。 解决方案:树脂模制产品10包括由生物可降解树脂构成的模塑基材11和形成在模制基材11的表面上的涂膜12,其中涂膜12包括石油基涂料 ,天然物质和促进微生物增殖的增殖启动子,例如 碳水化合物或氨基酸。 树脂成型体10通过增殖促进剂在土壤中增殖微生物,提高树脂成型体10的生物降解率。(C)2007,JPO&INPIT

    多層賦形フィルム製品を形成するための単一パス方法
    8.
    发明专利
    多層賦形フィルム製品を形成するための単一パス方法 有权
    用于形成多层成形膜产品单遍方法

    公开(公告)号:JP2017504474A

    公开(公告)日:2017-02-09

    申请号:JP2016543679

    申请日:2014-12-23

    IPC分类号: B05D1/36 B05D1/26 B05D1/32

    摘要: 方法は、基材上にマスクを載置することと、マスクを通して液体フィルム形成組成物を基材へ送達することと、マスクを取り外して多層粗形状体を基材上に残すことと、多層粗形状体を硬化させて基材上に配された多層賦形フィルム製品を形成することと、を含む。マスクは、送達面と、対向面と、所望の賦形フィルム製品に対応する設計を有する少なくとも1つの開口部とを有する。フィルム形成組成物は、マルチストリームノズルを通して送達される。マスクの移動と第1及び第2の液体フィルム形成組成物のマスク開口部への送達は、空隙の容積に対応する体積流量の第1及び第2の液体フィルム形成組成物をマスク開口部へ提供するように制御される。ノズルは、マスクの送達面と接触している。

    摘要翻译: 该方法包括将掩模放置在衬底上,并且通过掩模的液体膜形成组合物递送到衬底上,并且通过去除所述掩模,多层粗离开基板上的多层粗糙度形状体 成型体被固化包括形成设置在所述衬底上的多层成形膜的产品,。 所述掩模具有一个输送表面,并且所述相对的表面,并具有对应于所期望的成形膜产品设计的至少一个开口。 膜形成组合物通过多流喷嘴输送。 输送到掩模开口运动,并且第一和第二液体膜形成掩模的组合物中,提供对应于所述空隙的体积与掩模开口的体积流率的第一和第二液体形成膜的组合物 它控制。 喷嘴与掩模的输送表面接触。