Abstract:
Extruded or molded profiles comprising a polyolefin composition consisting of 85% by weight or more of a copolymer of 1-butene with ethylene (A) having an ethylene copolymerized content up to 18% by mol, and having Mw/Mn lower than 3, hardness shore A (measured according to ISO 868) lower than 90, no melting point (TmII) detectable at the DSC after cancelling the thermal history, melting enthalpy (ΔHf), measured by DSC after 10 days of aging at room temperature, comprised between 4 and 15 J/g; and up to 15% by weight of a propylene copolymer or a composition of copolymers of propylene (B) having a melting point from about 126° C. to 200° C., isotactic index greater than 90%.
Abstract:
The present disclosure relates to highly filled polyolefin compositions with improved balance of properties particularly for applications where puncture and tear resistance is requested comprising a flexible heterophasic polyolefin composition (I), consisting of a crystalline polymer fraction (A) consisting of a copolymer of propylene with ethylene having a fraction insoluble in xylene at 25° C. of at least 90% by weight, and an elastomeric fraction (B) consisting of a copolymer or blend of copolymers of ethylene with propylene; the copolymer or blend containing units derived from ethylene in a quantity lower than 40% by weight. The fraction soluble in xylene at 25° C. of the polyolefin composition having an IVgpc lower than 2.5 dl/g, a broad molecular weight distribution Mw/Mn (GPC) equal to or higher than 4, and a Mz/Mw (GPC) equal to or higher than 2.5.
Abstract:
A method for the production of metal-plated articles, including the step of
depositing an electrically-conductive metallic layer on a surface of an article comprising a polymer composition comprising by weight:
a) 40-60% of a propylene homopolymer, or propylene copolymer containing up to 5% by weight of ethylene and/or another C4-C10 α-olefin, and having a melting temperature of 155° C. or higher and/or a fraction soluble in xylene at 25° C. of 10% by weight or less; b) 10-20% of an ethylene-based elastoplastic copolymer, optionally, a copolymer of ethylene with C4-C10 α-olefin; c) 2-6% of a styrene block copolymer; d) optionally, up to 3% of a propylene homopolymer having a Melt Flow Rate (230° C./2.16 kg) of 500 g/10 min. or more; e) 15-50% of a filler; and f) optionally, up to 6% of a color pigment.
Abstract:
Liner for CIPP rehabilitation comprising a layer of thermoplastic polymer material, a resin absorbent layer, thermosetting hot curing-resin impregnating the absorbent layer; wherein said thermoplastic is a heterophasic polyolefin composition (I) having flexural modulus equal to or lower than 200 MPa, and comprising a crystalline propylene homopolymer (a); and a copolymer or a composition of copolymers of ethylene with other alpha-olefins (b) containing from 15% by weight to less than 40% by weight of ethylene.
Abstract:
Flexible highly filled polyolefin compositions with improved balance of properties particularly for applications where softness and ductility at low temperature is requested comprising a soft heterophasic polyolefin composition the fraction soluble in xylene at 25° C. of said polyolefin composition having IVgpc lower than 2.5 dl/g. Mw/Mn (GPC) equal to or higher than 4. Mz/Mw (GPC) equal to or higher than 2.5. Said polyolefin composition further comprising an inorganic filler (II) selected from flame-retardant inorganic fillers and inorganic oxides or salts and a further elastomeric polymer or polymer composition component (c) having flexural modulus (ISO 178) lower than 60 MPa, Shore A (ISO 868) lower than 90 and Tg (DMTA) lower than −20° C.
Abstract translation:柔性高填充聚烯烃组合物具有改善的性能平衡,特别是对于要求低温柔软性和延展性的应用,包括柔软的多相聚烯烃组合物,所述聚烯烃组合物在25℃下可溶于二甲苯的馏分具有低于2.5dl / g 。 Mw / Mn(GPC)等于或高于4.Mz / Mw(GPC)等于或高于2.5。 所述聚烯烃组合物还包含选自阻燃无机填料和无机氧化物或盐的无机填料(II)以及弹性体聚合物或聚合物组合物组分(c),其弯曲模量(ISO 178)低于60MPa,肖氏A( ISO 868)低于90,Tg(DMTA)低于-20℃
Abstract:
A method for the production of metal-plated articles, including the step of depositing an electrically-conductive metallic layer on a surface of an article comprising a polymer composition comprising by weight: a) 40-60% of a propylene homopolymer, or propylene copolymer containing up to 5% by weight of ethylene and/or another C4-C10 α-olefin, and having a melting temperature of 155° C. or higher and/or a fraction soluble in xylene at 25° C. of 10% by weight or less; b) 10-20% of an ethylene-based elastoplastic copolymer, optionally, a copolymer of ethylene with C4-C10 α-olefin; c) 2-6% of a styrene block copolymer; d) optionally, up to 3% of a propylene homopolymer having a Melt Flow Rate (230° C./2.16 kg) of 500 g/10 min. or more; e) 15-50% of a filler; and f) optionally, up to 6% of a color pigment.
Abstract:
Extruded or molded profiles comprising a polyolefin composition consisting of 85% by weight or more of a copolymer of 1-butene with ethylene (A) having an ethylene copolymerized content up to 18% by mol, and having Mw/Mn lower than 3, hardness shore A (measured according to ISO 868) lower than 90, no melting point (TmII) detectable at the DSC after cancelling the thermal history, melting enthalpy (ΔHf), measured by DSC after 10 days of aging at room temperature, comprised between 4 and 15 J/g; and up to 15% by weight of a propylene copolymer or a composition of copolymers of propylene (B) having a melting point from about 126° C. to 200° C., isotactic index greater than 90%.