1.
公开(公告)号:US20240402569A1
公开(公告)日:2024-12-05
申请号:US18804139
申请日:2024-08-14
Applicant: FUJIFILM Corporation
Inventor: Yasuyuki SASADA
Abstract: Provided are a base material for a metamaterial, in which a thermal dimensional change rate in a case of being allowed to stand in an environment of 90° C. for 24 hours is 0.01% or more and less than 10%; a metamaterial and a laminate including the base material for a metamaterial; and a manufacturing method of a metamaterial.
-
公开(公告)号:US20240228715A1
公开(公告)日:2024-07-11
申请号:US18615743
申请日:2024-03-25
Applicant: FUJIFILM Corporation
Inventor: Miyoko HARA , Takato SUZUKI , Yasuyuki SASADA , Akio TAMURA , Reiko INUSHIMA
IPC: C08J7/04
CPC classification number: C08J7/042 , C08J2333/10
Abstract: An object of the present invention is to provide a cover film in which chips during cutting are unlikely to be generated, voids during bonding to a substrate using an enclosing solution are unlikely to be generated, and adhesiveness with the substrate is excellent. The cover film of the present invention is used for covering a test subject on a substrate, the cover film including a support and a polymer layer containing a polymer, in which a fracture toughness value of the polymer layer is 0.2 MPa·m0.5 or more, an in-plane retardation of the support at a wavelength of 590 nm is 1,000 nm or less, and a requirement regarding a dissolution rate of the polymer layer in xylene and a requirement regarding a viscosity of a xylene solution of the polymer layer are satisfied.
-
公开(公告)号:US20230321958A1
公开(公告)日:2023-10-12
申请号:US18318708
申请日:2023-05-16
Applicant: FUJIFILM Corporation
Inventor: Yasuyuki SASADA
CPC classification number: B32B27/06 , B32B27/20 , B32B27/365 , B32B2250/02 , B32B2255/062 , B32B2305/55 , B32B2311/12 , B32B2367/00
Abstract: Provided are a liquid crystal polymer film or a polymer film, which has low dielectric loss tangent and has excellent breaking strength; and a laminate using the liquid crystal polymer film or the polymer film. The liquid crystal polymer film contains a liquid crystal polymer A and a compound having a melting point lower than a melting point of the liquid crystal polymer A and having a dielectric loss tangent of less than 0.01.
-
公开(公告)号:US20230265246A1
公开(公告)日:2023-08-24
申请号:US18171644
申请日:2023-02-20
Applicant: FUJIFILM Corporation
Inventor: Shohei YAMAZAKI , Yasuyuki SASADA
IPC: C08G69/44 , C08G63/685 , H05K1/03
CPC classification number: C08G69/44 , C08G63/685 , H05K1/0346 , H05K2201/0145
Abstract: Provided are a film which includes at least a first resin layer containing aromatic polyester amide, and a second resin layer disposed on the first resin layer, and an elastic modulus of the second resin layer at 160° C. is less than 1.0 GPa.
-
公开(公告)号:US20230242818A1
公开(公告)日:2023-08-03
申请号:US18154876
申请日:2023-01-16
Applicant: FUJIFILM Corporation
Inventor: Miyoko HARA , Yasuyuki SASADA
CPC classification number: C09K19/3814 , C08K7/28 , C08K3/36 , C08L77/12 , C08L2203/16
Abstract: Provided are a film which includes at least an a liquid crystal polymer and a filler, and has a melting calorie equal to or greater than 0.5 J/g; a laminate which includes at least the film and a metal layer or a metal wire which is disposed on at least one surface of the film; and applications of the film.
-
公开(公告)号:US20150131038A1
公开(公告)日:2015-05-14
申请号:US14558044
申请日:2014-12-02
Applicant: FUJIFILM Corporation
Inventor: Makoto ISHIGURO , Yasuyuki SASADA , Kazuya HISANAGA
IPC: G02F1/1335 , G02F1/1343
CPC classification number: G02F1/133528 , G02B5/3033 , G02F1/134363 , G02F2001/133531
Abstract: A liquid crystal display includes a liquid crystal cell having a liquid crystal layer provided between two glass substrates having a thickness of 0.5 mm or less, polarization plates provided on both surfaces of the liquid crystal cell in which absorption axes of the polarization plates provided on both surfaces of the liquid crystal cell are disposed to be orthogonal with each other, and a back light provided on a rear side of the liquid crystal cell, and a difference (D-H) between a contractive force D in an absorption axis direction of the front side polarization plate, and a contractive force H in a transmission axis direction of the rear side polarization plate is 365×10 N/m or less.
Abstract translation: 液晶显示器包括具有设置在两个厚度为0.5mm以下的两个玻璃基板之间的液晶层的液晶单元,设置在液晶单元的两个表面上的偏振板,其中设置在两者上的偏振板的吸收轴 液晶单元的表面被配置为彼此正交,并且设置在液晶单元的后侧的背光以及前侧的吸收轴方向上的收缩力D之间的差(DH) 偏振板,后侧偏振板的透射轴方向的收缩力H为365×10 N / m以下。
-
公开(公告)号:US20250074039A1
公开(公告)日:2025-03-06
申请号:US18953084
申请日:2024-11-20
Applicant: FUJIFILM Corporation
Inventor: Yasuyuki SASADA , Miyoko HARA
Abstract: Provided are a film having a plane A consisting of a composition A and a plane B consisting of a composition B as two imaginary planes perpendicular to a thickness direction, in which a content of at least one component A contained in the composition A is decreased from the plane A toward the plane B, a content of at least one component B contained in the composition B is decreased from the plane B toward the plane A, and a dielectric loss tangent is 0.010 or less, and an application thereof.
-
公开(公告)号:US20250034453A1
公开(公告)日:2025-01-30
申请号:US18915299
申请日:2024-10-14
Applicant: FUJIFILM Corporation
Inventor: Shohei YAMAZAKI , Yasuyuki SASADA
IPC: C09K19/38
Abstract: Provided is a film including a phase-separated structure having at least two phases, in which in a case where a glass transition temperature of a first phase, which is one of the at least two phases, is denoted by Tg1, a second phase which is one of the at least two phases and is different from the first phase does not have an inflection point of a storage elastic modulus in a temperature range of 25° C. or higher and the Tg1 or lower.
-
公开(公告)号:US20250026957A1
公开(公告)日:2025-01-23
申请号:US18900839
申请日:2024-09-29
Applicant: FUJIFILM Corporation
Inventor: Miyoko HARA , Yasuyuki SASADA
IPC: C09D177/12 , C08L77/12 , H05K1/03
Abstract: Provided are a film including a layer A, and a layer B provided on at least one surface of the layer A, in which an elastic modulus of the layer A at 160° C. is 100 MPa to 2,500 MPa, and a value of a difference LA-LB between a value LA obtained by subtracting a weight residual rate of the layer A at 900° C. from a weight residual rate of the layer A at 440° C. and a value LB obtained by subtracting a weight residual rate of the layer B at 900° C. from a weight residual rate of the layer B at 440° C. is 80% or less.
-
公开(公告)号:US20230125850A1
公开(公告)日:2023-04-27
申请号:US17896015
申请日:2022-08-25
Applicant: FUJIFILM Corporation
Inventor: Yasuyuki SASADA
IPC: C08L23/30 , C09J123/30 , C09J7/38 , C09J7/28
Abstract: Provided are a film including a matrix material, and a particle having an elastic modulus at 25° C. which is higher than an elastic modulus of the matrix material, in which the film has a region A at at least a part between the matrix material and the particle, and the region A contains a compound having a loss tangent of 0.1 or greater at 25° C.; and a laminate formed of the film.
-
-
-
-
-
-
-
-
-