摘要:
The invention relates to a method of preparing a composite or porous composite used as a biodegradable scaffold, the composite prepared therefrom and the use of the composite. In particular, the composite is a calcium sulfate-polylactic acid composite or porous composite and the composite can be especially used as an in situ pore forming scaffold.
摘要:
The present invention relates to a process of using a heat responsive mixture to produce inorganic interconnected 3D open-cell bone substitutes which can be applied in the orthopedic or dental field for treatment of bone damage. The invention provides a simple and easily-controlled process of preparing porous inorganic bone substitute materials.
摘要:
A bio-implant having a screw body selectively formed with nanoporous channels structure in a spiral groove and the method of making the same are disclosed. Nanoporous channels structure formed into the spiral groove of the bio-implant is carried out by the heat treatment in vacuum firstly and anodic treatment secondly. Thereafter, bioactive material is filled into the nanoporous and deposited on the implant surface by an electro-deposition process so as to increase the bioactivity and biocompatibility of the bio-implant.
摘要:
A method for preparing amorphous calcium phosphate (ACP) and oral care composition containing ACP prepared by the same are disclosed, wherein the method comprises the following steps: (a) cleaning and pulverizing the oyster shells; (b) sintering the oyster shells to obtain a calcium-containing powder; (c) dissolving the calcium-containing powder in water to obtain a calcium-containing solution; and (d) mixing the calcium-containing solution with a other phosphate-containing solution, to produce amorphous calcium phosphate.The method of the present invention not only can simplify the process and reduce the cost, but also can solve the problem of environment pollution resulting from wasted oyster shells. In addition, the ACP prepared in accordance with the method of the present invention further comprises some trace elements, such as strontium (Sr) and fluoride (F), which can improve dental health.
摘要:
The invention provides a process for preparing α-calcium sulfate hemihydrate which comprises the following steps: adding aqueous solutions containing sulfate ions and calcium ions to calcium chloride solution with a range of concentration; reacting the mixture of a) at a range of temperature for an appropriate time; filtering and washing the reaction products of b) with a rising solvent to isolate the solid and liquid phases; and d) collecting and drying the solid phase to obtain α-calcium sulfate hemihydrate with high purity; wherein the relationship between the range of the concentration of calcium chloride (y) and the range of the reaction temperature (x) is shown as the following formula: −0.4x5+7.33x4−52.83x3+187.17x2−328.27x+316
摘要:
The invention relates to a simple and high yield process for producing a regenerated silk fibroin which does not need dialysis. Particularly, a process of the invention is characterized in that the silk fibroin is precipitated by applying a shear stress and/or changing the solvent power of the fibroin solution. The process of the invention simplifies the process of producing silk fibroin and greatly shortens the process time to 1 to 2 hours, whereas the conventional dialysis process is complex and needs around 2 to 3 days. In addition to reducing the time needed, the process of the invention can increase productivity of silk fibroin by at least 8%.
摘要:
A composite bio-ceramic dental implant and fabricating method thereof are disclosed. The composite bio-ceramic is sintered at a temperature between 1000 and 1800° C. using the nearly inert bio-ceramic powder and the active bio-ceramic powder or the completely resorbable bio-ceramic powder. The bioactive bio-ceramic material is dispersed in the inert bio-ceramic material. Therefore, the composite bio-ceramic has enough mechanical strength and good bioactivity for dental implant.
摘要:
The invention provides a process for preparing α-calcium sulfate hemihydrate which comprises the following steps: adding aqueous solutions containing sulfate ions and calcium ions to calcium chloride solution with a range of concentration; reacting the mixture of a) at a range of temperature for an appropriate time; filtering and washing the reaction products of b) with a rising solvent to isolate the solid and liquid phases; and d) collecting and drying the solid phase to obtain α-calcium sulfate hemihydrate with high purity; wherein the relationship between the range of the concentration of calcium chloride (y) and the range of the reaction temperature (x) is shown as the following formula: −0.4x5+7.33x4−52.83x3+187.17x2−328.27x+316
摘要:
The invention provides an anion-containing calcium phosphate compound, composition and dental patch comprising the same and their use in remineralizing teeth. The anion-containing calcium phosphate compound has the following formula: (Ca+2)x(anion−a)y(PO4−3)z wherein 2x=(a*y+3z); a is an integer of 1 to 3; and each of x, y and z is not 0.
摘要:
This invention is related to a kind of teeth bleaching formulation containing the vegetative enzymes extracted from plant tubers with extensively applications in cosmetic dentistry. The enzymes are susceptible to promote the decomposition (dissociation) of peroxide compounds, thus the intermediate hydroxyl free radicals are generated to turn the unpleasant stained tooth into light or colorless appearance effectively. The composition of a whitening gel may comprising 2˜50 wt % of hydrogen peroxide, 0.003˜3 wt % vegetative enzyme extract, and transferring to alkalinity approximately pH 8˜13 to achieve the high efficiency dental bleaching usage.