摘要:
An oxidation resistant component is disclosed comprising a substrate and a protective layer. The protective layer consists of an inner MCrAlY layer contiguous with the substrate and an outer layer consisting of at least Ni and Al and having a β-NiAl structure
摘要:
The invention relates to a component having a substrate and a protective layer, which consists of an intermediate NiCoCrAlY layer zone on or near the substrate and an outer layer zone which is arranged on the intermediate NiCoCrAlY layer zone, which is characterized in that the intermediate NiCoCrAlY layer zone comprises of (in wt %): 24-26% Co, 16-18% Cr, 9.5-11% Al, 0.3-0.5 Y, 1-1.8% Re and Ni balance.
摘要:
MCrAl layers according to prior art often display chipping of the thermally grown aluminum oxide layer (TGO) as a result of thermally induced stresses, which significantly reduces the oxidation behavior or the bonding behavior of ceramic heat insulating layers. An inventive MCrAl layer is designed in such a way that the TGO created thereon is microporous and thus allows expansion. The microporosity of the TGO is ensured by adding elements into the MCrAl layer in a targeted manner.
摘要:
An oxidation resistant component is disclosed comprising a substrate and a protective layer. The protective layer consists of an inner MCrAlY layer contiguous with the substrate and an outer layer. The outer layer is characterized by having an Al content of up to 6.5 wt. % and having the structure of a pure γ-Ni phase.
摘要:
Known protective layers having a high Cr-content and a silicone in addition, form brittle phases that embrittle further under the influence of carbon during use. The protective layer according to the invention is composed of 22% to 26% cobalt (Co), 10.5% to 12% aluminum (Al), 0.2% to 0.4% Yttrium (Y) and/or at least one equivalent metal from the group comprising Scandium and the rare earth elements, 15% to 16% chrome (Cr), optionally 0.3% to 1.5% tantal, the remainder nickel (Ni).
摘要:
Known protective coatings having a high Cr content, as well as silicon, have brittle phases that become additionally brittle under the influence of carbon during use. A protective coating is provided. The protective coating includes the composition of 24% to 26% cobalt, 10% to 12% aluminum, 0.2% to 0.5% yttrium, 12% to 14% chromium, and the remainder nickel.
摘要:
Ceramic coatings for a component that is subjected to high temperatures, especially for a turbine blade are provided. The ceramic coatings contain one or more compounds that are selected from alkaline earth silicates, ZrV2O7 and Mg3(VO4)2. A layer system including at least one coating of the ceramic coating is also provided.
摘要:
A nickel-based coating or alloy is provided. The coating includes tantalum preferably without rhenium. The coating or alloy has stabilized the formation of phases γ/γ′ at high temperatures leading to a reduction of local stresses. A component is also provided. The substrate of the component includes a nickel-based or cobalt-based superalloy.
摘要:
Protective layers, according to the prior art, achieve their protective function b depletion of a defined element that forms a protective oxide layer or that is exhausted as a sacrificial material. Once said material is exhausted, the protective function cannot be maintained. The invention is characterized by using particles (1) that contain a sustained-release depot of the exhaustible material. For this purpose, the material is present in a superstoichiometric form.
摘要:
A two-ply MCrAlX layer is provided. The two-ply MCrAlX layer includes nickel and cobalt, but also Cr, Al and Y, differ significantly, in order to improve both oxidation resistance and thermal-mechanical strength. A layer system including a substrate and the two-ply MCrAlX layer is also provided. The MCrAlX layer includes an inner layer and an outer layer.