Hydrogen bond induced high stability porous covalent organic gel material and preparation method thereof

    公开(公告)号:US11897972B2

    公开(公告)日:2024-02-13

    申请号:US17317217

    申请日:2021-05-11

    IPC分类号: C08F132/04

    CPC分类号: C08F132/04

    摘要: A hydrogen bond induced high stability porous covalent organic gel material and a preparation method thereof are provided. The method comprises: dissolving tetrakis(4-carboxyphenyl)silane in methanol to obtain solution A; adding concentrated sulfuric acid to the solution A, then water-bath heating and re-flowing to obtain a solution B; evaporating the solution B, dissolving remaining powder with an ethyl acetate, washing and drying, filtering and then evaporating the filtrate until crystallization to obtain a colorless solid C; dissolving the colorless solid C and hydrazine hydrate in methanol, water-bath re-fluxing, filtering and collecting white powder, washing and drying to obtain a white solid D; adding the white solid D and 1,4-Phthalaldehyde to N,N-dimethyl-formamide, adding trifluoroacetic acid, and then getting the desired material. The material is has high synthesis efficiency, abundant functional groups, a large specific surface area, a good adsorption performance, and excellent chemical stability and thermal stability.

    Isomerized terpene tackifier resins
    6.
    发明授权
    Isomerized terpene tackifier resins 失效
    异构萜烯增粘剂树脂

    公开(公告)号:US4879351A

    公开(公告)日:1989-11-07

    申请号:US232024

    申请日:1988-08-15

    IPC分类号: C08F8/48

    摘要: A novel copolymer resin which has excellent tackifying properties for selected elastomers useful in hot melt and pressure sensitive adhesives is produced by the copolymerization of beta-pinene with other terpenes or hydrocarbon monomers, followed by thermal catalytic isomerization of the resin produced. Typically, beta-pinene and styrene (80/20) are copolymerized at a temperature between 0.degree. to 60.degree. C. under anhydrous conditions with a Lewis acid catalyst in a solvent. After catalyst removal, the copolymer resin is isomerized with iodine as a catalyst at a temperature between 200.degree. to 260.degree. C. Excellent yields of high softening point tackifier resins are produced.