BEAD FOAM MOLDINGS COMPOSED OF EXPANDABLE ACRYLONITRILE COPOLYMERS
    13.
    发明申请
    BEAD FOAM MOLDINGS COMPOSED OF EXPANDABLE ACRYLONITRILE COPOLYMERS 审中-公开
    由可膨胀的丙烯腈共聚物组成的泡沫泡沫塑料

    公开(公告)号:US20100190877A1

    公开(公告)日:2010-07-29

    申请号:US12666956

    申请日:2008-06-26

    IPC分类号: B29C44/34

    摘要: Bead foam moldings obtainable by fusing prefoamed foam beads composed of expandable thermoplastic polymer granules, comprisingfrom 5 to 100% by weight of a component (A) comprising a1) from 5 to 100% by weight (based on (A)) of an α-methylstyrene/acrylonitrile copolymer and/or α-methylstyrene/styrene/acrylonitrile terpolymer and a2) from 0 to 95% by weight (based on (A)) of a styrene/acrylonitrile copolymer; from 0 to 95% by weight of polystyrene (B) and from 0 to 95% by weight of a thermoplastic polymer (C) other than (A) and (B), feature good thermal and solvent stability.

    摘要翻译: 珠粒发泡成型品可通过将由可发性热塑性聚合物颗粒组成的预发泡泡沫珠粒熔融而成,该组合物包含5至100重量%的组分(A),其包含a1)5-100重量%(基于(A))α α-甲基苯乙烯/丙烯腈共聚物和/或α-甲基苯乙烯/苯乙烯/丙烯腈三元共聚物和a2)0至95重量%(基于(A))苯乙烯/丙烯腈共聚物; 0至95重量%的聚苯乙烯(B)和0至95重量%的除(A)和(B)之外的热塑性聚合物(C)具有良好的热和溶剂稳定性。

    ELASTIC EXPANDED POLYMER FOAM BASED ON POLYOLEFIN/STYRENE POLYMER MIXTURES
    16.
    发明申请
    ELASTIC EXPANDED POLYMER FOAM BASED ON POLYOLEFIN/STYRENE POLYMER MIXTURES 失效
    基于聚烯烃/苯乙烯聚合物混合物的弹性膨胀聚合物泡沫

    公开(公告)号:US20110316198A1

    公开(公告)日:2011-12-29

    申请号:US13254174

    申请日:2010-03-01

    IPC分类号: C08L25/06

    摘要: The invention relates to elastic expanded polymer foams and also a process for producing expanded polymer foams by sintering a mixture comprising foam particles P1 and P2 composed of different thermoplastic polymers or polymer blends, wherein the foam particles P1 are obtained by prefoaming expandable, thermoplastic polymer particles comprising A) from 45 to 97.9 percent by weight of a styrene polymer, B1) from 1 to 45 percent by weight of a polyolefin having a melting point in the range from 105 to 140° C., B2) from 0 to 25 percent by weight of a polyolefin having a melting point below 105° C., C1) from 0.1 to 25 percent by weight of a styrene-butadiene or styrene-isoprene block copolymer, C2) from 0.0 to 10 percent by weight of a styrene-ethylene-butylene block copolymer, D) from 1 to 15 percent by weight of a blowing agent, E) from 0 to 5 percent by weight of a nucleating agent, where the sum of A) to E) is 100% by weight.

    摘要翻译: 本发明涉及弹性膨胀聚合物泡沫,还涉及通过烧结由不同的热塑性聚合物或聚合物共混物组成的泡沫颗粒P1和P2的混合物来生产发泡聚合物泡沫的方法,其中泡沫颗粒P1是通过预发泡的可发泡热塑性聚合物颗粒 包括A)45至97.9重量%的苯乙烯聚合物,B1)1至45重量%的熔点在105-140℃的聚烯烃,B2)0-25重量% 熔点低于105℃的聚烯烃的重量,C1)0.1至25重量%的苯乙烯 - 丁二烯或苯乙烯 - 异戊二烯嵌段共聚物,C2)0.0至10重量%的苯乙烯 - 乙烯 - 丁烯嵌段共聚物,D)1〜15重量%的发泡剂,E)0〜5重量%的成核剂,其中A)与E)之和为100重量%。

    ELASTIC MOLDED FOAM BASED ON POLYOLEFIN/STYRENE POLYMER MIXTURES
    17.
    发明申请
    ELASTIC MOLDED FOAM BASED ON POLYOLEFIN/STYRENE POLYMER MIXTURES 审中-公开
    基于聚烯烃/苯乙烯聚合物混合物的弹性模制泡沫

    公开(公告)号:US20110269858A1

    公开(公告)日:2011-11-03

    申请号:US13143029

    申请日:2009-12-16

    摘要: Expandable, thermoplastic polymer bead material, comprising A) from 45 to 97.8 percent by weight of a styrene polymer, B1) from 1 to 45 percent by weight of a polyolefin with a melting point in the range from 105 to 140° C., B2) from 0 to 25 percent by weight of a polyolefin with a melting point below 105° C., C1) from 0.1 to 25 percent by weight of a block or graft copolymer with weight-average molar mass Mw of at least 100,000 g/mol, comprising a) at least one block S composed of from 95 to 100% by weight of vinylaromatic monomers and from 0 to 5% by weight of dienes, and b) at least one copolymer block (S/B)A composed of from 63 to 80% by weight of vinylaromatic monomers and from 20 to 37% by weight of dienes, with glass transition temperature TgA in the range from 5 to 30° C., where the proportion by weight of the entirety of all of the blocks S is in the range from 50 to 70% by weight, based on the block or graft copolymer A, C2) from 0 to 20 percent by weight of a styrene-butadiene or styrene-isoprene block copolymer different from C1, C3) from 0.1 to 9.9 percent by weight of a styrene-ethylene-butylene block copolymer, D) from 1 to 15 percent by weight of a blowing agent, and E) from 0 to 5 percent by weight of a nucleating agent, where the entirety composed of A) to E) gives 100% by weight.

    摘要翻译: 可膨胀的热塑性聚合物珠粒材料,其包含A)45至97.8重量%的苯乙烯聚合物,B1)1至45重量%的熔点为105-140℃的聚烯烃,B2 )0至25重量%的熔点低于105℃的聚烯烃,C1)0.1至25重量%的重均摩尔质量Mw至少为100,000克/摩尔的嵌段或接枝共聚物 包括a)至少一种由95-100%重量的乙烯基芳族单体和0-5%重量二烯组成的嵌段S,和b)至少一种由63组成的共聚物嵌段(S / B)A 至80重量%的乙烯基芳族单体和20至37重量%的二烯,玻璃化转变温度TgA在5至30℃的范围内,其中全部块S的重量比为 基于嵌段或接枝共聚物A在50至70重量%的范围内,C2)0至20重量%的苯乙烯 - 丁 二烯或苯乙烯 - 异戊二烯嵌段共聚物,不同于C1,C3)0.1至9.9重量%的苯乙烯 - 乙烯 - 丁烯嵌段共聚物,D)1至15重量%的发泡剂,E)0至 5重量%的成核剂,其中由A)至E)组成的整体得到100重量%。

    Method for producing polyoxymethlenes
    19.
    发明授权
    Method for producing polyoxymethlenes 失效
    生产聚甲烯的方法

    公开(公告)号:US07906609B2

    公开(公告)日:2011-03-15

    申请号:US11996235

    申请日:2006-07-13

    IPC分类号: C08G2/10 C08G2/06 C08G2/00

    CPC分类号: C08L59/04 C08G2/18

    摘要: Process for preparing polyoxymethylene copolymers (POMs) by a) polymerizing a reaction mixture comprising suitable main monomers and comonomers and also a polymerization initiator and, if appropriate, a regulator, b) adding a deactivator and c) removing the residual monomers, wherein the amount of compounds whose melting point at 1013 hPa is below 60° C. present in the reaction mixture at any point in time during the process is not more than 0.1% by weight, with the POM, the monomers, comonomers, polymerization initiators, deactivators and regulators not being included in the calculation.

    摘要翻译: 通过以下方法制备聚甲醛共聚物(POM)的方法:a)聚合包含合适的主要单体和共聚单体的反应混合物以及聚合引发剂,如果合适的话,聚合引发剂,如果合适的话,调节剂,b)加入失活剂和c)除去残余单体, 的化合物,其熔点为1013hPa,低于60℃,反应混合物中任何时间点在该过程中不超过0.1重量%,POM,单体,共聚单体,聚合引发剂,失活剂和 监管机构不包括在计算中。

    Method for Producing Polyoxymethlenes
    20.
    发明申请
    Method for Producing Polyoxymethlenes 失效
    生产聚氧甲烯的方法

    公开(公告)号:US20080207865A1

    公开(公告)日:2008-08-28

    申请号:US11996235

    申请日:2006-07-13

    IPC分类号: C08G2/10

    CPC分类号: C08L59/04 C08G2/18

    摘要: Process for preparing polyoxymethylene copolymers (POMs) by a) polymerizing a reaction mixture comprising suitable main monomers and comonomers and also a polymerization initiator and, if appropriate, a regulator, b) adding a deactivator and c) removing the residual monomers, wherein the amount of compounds whose melting point at 1013 hPa is below 60° C. present in the reaction mixture at any point in time during the process is not more than 0.1% by weight, with the POM, the monomers, comonomers, polymerization initiators, deactivators and regulators not being included in the calculation.

    摘要翻译: 通过以下方法制备聚甲醛共聚物(POM)的方法:a)聚合包含合适的主要单体和共聚单体的反应混合物以及聚合引发剂,如果合适的话,聚合引发剂,如果合适的话,调节剂,b)加入失活剂和c)除去残余单体, 的化合物,其熔点为1013hPa,低于60℃,反应混合物中任何时间点在该过程中不超过0.1重量%,POM,单体,共聚单体,聚合引发剂,失活剂和 监管机构不包括在计算中。