Abstract:
The present disclosure relates to a propylene-1-hexene copolymer having: i) a content of 1-hexene derived units ranging from 0.6 wt % to 3.0 wt %; ii) a melt flow rate (MFR) measured according to the method ISO 1133 (230° C., 5 kg) ranging from 0.5 g/10 min to 5.0 g/10 min; iii) a polydispersity (PI) ranges from 4.5 to 10 and the distribution of molecular weight is of multimodal type; iv) a melting point ranging from 160° C. to 145° C.; and v) a differential scanning calorimetry (DSC) curve (temperature/heat of fusion) that shows at least two peaks.
Abstract:
A polypropylene composition made from or containing: A) from 71 wt % to 91 wt % of a propylene homopolymer, B) from 5 wt % to 15 wt % of a copolymer of propylene and ethylene containing from 18 wt % to 32.0 wt % of ethylene derived units; and C) from 4 wt % to 15 wt % of a copolymer of propylene and ethylene containing from 75 wt % to 90.0 wt % of ethylene derived units.
Abstract:
A propylene 1-hexene copolymer containing from 5.7 to 7.7% by weight of 1-hexene derived units, based upon the total weight of the propylene 1-hexene copolymer, having: a) a solubility in xylene at 25° C. ranging from 7.0 wt % to 15.0 wt %, based upon the total weight of the propylene 1-hexene copolymer; b) a melting temperature, measured by DSC ranging from 143.0° C. to 148.0° C.; c) a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg) from 3.5 to 8.0 g/10 min.; and d) a content of 1-hexene derived units in the fraction soluble in xylene at 25° C. ranging from 13.5 wt % to 18.5 wt %, based upon the total weight of the soluble fraction.
Abstract:
A polyolefin composition made from or containing: A) from about 19 wt % to about 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt % B) from about 50 wt % to about 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt % and 1-butene derived units content between about 4.8 wt % and about 12.4 wt %; the sum of the amount of component A) and B) being 100; the polyolefin composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than about 4.0; the creep and recovery curve measured on the polymer fuse at 200° C. shows a maximum value between 600 and 1200 seconds, lower than about 53×10−4 1/Pa.
Abstract:
A film made from or containing a polyolefin composition made from or containing: A) from about 19 wt % to about 50 wt %, based upon the total weight of the polyolefin composition, of a propylene ethylene copolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt %, based upon the total weight of the propylene ethylene copolymer; and B) from about 50 wt % to about 81 wt %, based upon the total weight of the polyolefin composition, of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt %, based upon the total weight of the propylene ethylene 1-butene terpolymer, and 1-butene derived units content of between about 4.8 wt % and about 12.4 wt %, based upon the total weight of the propylene ethylene 1-butene terpolymer; the sum of the amount of component A) and B) being 100.
Abstract:
Extruded or molded profiles comprising a polyolefin composition consisting of 85% by weight or more of a copolymer of 1-butene with ethylene (A) having an ethylene copolymerized content up to 18% by mol, and having Mw/Mn lower than 3, hardness shore A (measured according to ISO 868) lower than 90, no melting point (TmII) detectable at the DSC after cancelling the thermal history, melting enthalpy (ΔHf), measured by DSC after 10 days of aging at room temperature, comprised between 4 and 15 J/g; and up to 15% by weight of a propylene copolymer or a composition of copolymers of propylene (B) having a melting point from about 126° C. to 200° C., isotactic index greater than 90%.