Poly(arylene ether)-polysiloxane composition and method
    11.
    发明授权
    Poly(arylene ether)-polysiloxane composition and method 有权
    聚(亚芳基醚) - 聚硅氧烷组合物和方法

    公开(公告)号:US08669332B2

    公开(公告)日:2014-03-11

    申请号:US13169137

    申请日:2011-06-27

    Abstract: A thermoplastic composition that includes a poly(arylene ether)-polysiloxane block copolymer is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The oxidative polymerization includes a monohydric phenol addition period characterized by a first temperature, a build period following the addition period and characterized by a second temperature greater than the first temperature, and a temperature ramp period between the addition period and the build period. During the temperature ramp period, the temperature is increased at an average rate of about 0.01 to about 0.35° C. per minute, which improves the efficiency with which the hydroxyaryl-terminated polysiloxane is incorporated into the poly(arylene ether)-polysiloxane block copolymer.

    Abstract translation: 包括聚(亚芳基醚) - 聚硅氧烷嵌段共聚物的热塑性组合物通过包括使一元酚和羟基芳基封端的聚硅氧烷氧化共聚的方法制备。 氧化聚合包括一元酚添加时间,其特征在于第一温度,加入时间之后的生成周期,并且特征在于大于第一温度的第二温度,以及添加周期和构建周期之间的温度斜坡期间。 在温度升高期间,温度以每分钟约0.01至约0.35℃的平均速率增加,这提高了聚(亚芳基醚) - 聚硅氧烷嵌段共聚物中加入羟基芳基封端的聚硅氧烷的效率 。

    POLY(ARYLENE ETHER)-POLYSILOXANE COMPOSITION AND METHOD
    12.
    发明申请
    POLY(ARYLENE ETHER)-POLYSILOXANE COMPOSITION AND METHOD 有权
    聚(亚乙基醚) - 聚硅氧烷组合物和方法

    公开(公告)号:US20120329961A1

    公开(公告)日:2012-12-27

    申请号:US13169137

    申请日:2011-06-27

    Abstract: A thermoplastic composition that includes a poly(arylene ether)-polysiloxane block copolymer is prepared by a method that includes oxidatively copolymerizing a monohydric phenol and a hydroxyaryl-terminated polysiloxane. The oxidative polymerization includes a monohydric phenol addition period characterized by a first temperature, a build period following the addition period and characterized by a second temperature greater than the first temperature, and a temperature ramp period between the addition period and the build period. During the temperature ramp period, the temperature is increased at an average rate of about 0.01 to about 0.35° C. per minute, which improves the efficiency with which the hydroxyaryl-terminated polysiloxane is incorporated into the poly(arylene ether)-polysiloxane block copolymer.

    Abstract translation: 包含聚(亚芳基醚) - 聚硅氧烷嵌段共聚物的热塑性组合物通过包括使一元酚和羟基芳基封端的聚硅氧烷氧化共聚的方法制备。 氧化聚合包括一元酚添加时间,其特征在于第一温度,加入时间之后的生成周期,并且特征在于大于第一温度的第二温度,以及添加周期和构建周期之间的温度斜坡期间。 在温度升高期间,温度以每分钟约0.01至约0.35℃的平均速率增加,这提高了聚(亚芳基醚) - 聚硅氧烷嵌段共聚物中加入羟基芳基封端的聚硅氧烷的效率 。

    Morpholine-substituted poly(arylene ether) and method for the preparation thereof
    14.
    发明授权
    Morpholine-substituted poly(arylene ether) and method for the preparation thereof 有权
    吗啉取代的聚(亚芳基醚)及其制备方法

    公开(公告)号:US08017716B2

    公开(公告)日:2011-09-13

    申请号:US12495980

    申请日:2009-07-01

    CPC classification number: C08G65/46

    Abstract: A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.

    Abstract translation: 使用含吗啉的聚合催化剂制备的聚(2,6-二甲基-1,4-亚苯基醚)具有单分子分子量分布,具有非常高的分子量物质含量降低。 它还表现出高分子量级分中增加的吗啉掺入。 与使用含有二正丁胺的聚合催化剂制备的市售聚(2,6-二甲基-1,4-亚苯基醚)相比,聚(2,6-二甲基-1,4-亚苯基醚) 发明显示减少的气味。 与使用含吗啉的聚合催化剂制备的其它聚(2,6-二甲基-1,4-亚苯基醚)相比,本发明的聚(2,6-二甲基-1,4-亚苯基醚)表现出改善的分子量 在复合期间建立并改善与聚酰胺的相容性。

    MORPHOLINE-SUBSTITUTED POLY(ARYLENE ETHER) AND METHOD FOR THE PREPARATION THEREOF
    15.
    发明申请
    MORPHOLINE-SUBSTITUTED POLY(ARYLENE ETHER) AND METHOD FOR THE PREPARATION THEREOF 有权
    吗啉取代的聚(亚乙基醚)及其制备方法

    公开(公告)号:US20110003962A1

    公开(公告)日:2011-01-06

    申请号:US12495980

    申请日:2009-07-01

    CPC classification number: C08G65/46

    Abstract: A poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst has a monomodal molecular weight distribution with a reduced content of very high molecular weight species. It also exhibits increased morpholine incorporation in the high molecular weight fraction. Compared to commercially available poly(2,6-dimethyl-1,4-phenylene ether) prepared using a di-n-butylamine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits reduced odor. Compared to other poly(2,6-dimethyl-1,4-phenylene ether) prepared using a morpholine-containing polymerization catalyst, the poly(2,6-dimethyl-1,4-phenylene ether) of the invention exhibits improved molecular weight build during compounding and improved compatibilization with polyamides.

    Abstract translation: 使用含吗啉的聚合催化剂制备的聚(2,6-二甲基-1,4-亚苯基醚)具有单分子分子量分布,具有非常高的分子量物质含量降低。 它还表现出高分子量级分中增加的吗啉掺入。 与使用含有二正丁胺的聚合催化剂制备的市售聚(2,6-二甲基-1,4-亚苯基醚)相比,聚(2,6-二甲基-1,4-亚苯基醚) 发明显示减少的气味。 与使用含吗啉的聚合催化剂制备的其它聚(2,6-二甲基-1,4-亚苯基醚)相比,本发明的聚(2,6-二甲基-1,4-亚苯基醚)表现出改善的分子量 在复合期间建立并改善与聚酰胺的相容性。

    POLY(ARYLENE ETHER) COMPOSITION AND ARTICLE
    17.
    发明申请
    POLY(ARYLENE ETHER) COMPOSITION AND ARTICLE 审中-公开
    POLY(ARYLENE ETHER)组合物和文章

    公开(公告)号:US20080071000A1

    公开(公告)日:2008-03-20

    申请号:US11532164

    申请日:2006-09-15

    Abstract: A cured composition is prepared by curing a composition that includes an alkyl styrene and a low molecular weight, bifunctional poly(arylene ether). The curable composition can be prepared and processed at substantially lower temperatures than prior art poly(arylene ether) thermosets. The cured composition exhibits an improved balance of heat resistance, impact strength, and dielectric properties, making it particularly suitable for the fabrication of electronic components.

    Abstract translation: 通过固化包含烷基苯乙烯和低分子量双官能聚(亚芳基醚)的组合物来制备固化的组合物。 可固化组合物可以在比现有技术的聚(亚芳基醚)热固性材料低得多的温度下制备和加工。 固化的组合物表现出改善的耐热性,冲击强度和介电性能的平衡,使其特别适用于电子部件的制造。

    Poly(arylene ether) blends having low melt viscosity in the absence of plasticizer
    20.
    发明授权
    Poly(arylene ether) blends having low melt viscosity in the absence of plasticizer 失效
    在不存在增塑剂的情况下具有低熔体粘度的聚(亚芳基醚)共混物

    公开(公告)号:US07183350B2

    公开(公告)日:2007-02-27

    申请号:US10777436

    申请日:2004-02-12

    CPC classification number: C08L71/123 C08L71/12 C08L2666/22

    Abstract: A poly(arylene ether) composition comprises a first poly(arylene ether) resin having an intrinsic viscosity greater than or equal to about 0.3 dl/g, as measured in chloroform at 25° C. and a second viscosity poly(arylene ether) resin having an intrinsic viscosity less than or equal to about 0.17 dl/g, as measured in chloroform at 25° C. wherein the composition is essentially free of plasticizers.

    Abstract translation: 聚(亚芳基醚)组合物包含在25℃的氯仿中测定的特性粘度大于或等于约0.3dl / g的第一聚亚芳基醚树脂和第二粘度聚(亚芳基醚)树脂 其特性粘度小于或等于约0.17dl / g,如在25℃下在氯仿中测得的,其中组合物基本上不含增塑剂。