Abstract:
A surface treatment method includes: contacting a substrate with a treatment material, the substrate comprising a metallic element, the treatment material comprising an alkaline earth metal element, an alkali metal element, or any combination thereof; and forming on the substrate a surface layer comprising a first oxide of the alkaline earth metal element, the alkali metal element, or any combination thereof and a second oxide of the metallic element. A device has: a substrate layer comprising a metallic element; and a surface layer comprising a first oxide of an alkaline earth metal element, an alkali metal element, or any combination thereof, and a second oxide of the metallic element.
Abstract:
A method for cracking hydrocarbon includes providing a feedstock comprising steam and hydrocarbon, and feeding the feedstock into a device having an inner surface accessible to the feedstock. The inner surface includes a compound of formula An+1BnO3n+1, wherein A includes at least one alkaline earth metal, B includes at least one transition metal, O is oxygen, and 1≦n≦20.
Abstract:
A material is described of formula NaxMyAlaSibOδ with Face Centered Cubic (fcc) lattices forming F-4 3 m cubic structure, wherein M is at least one of lithium, potassium, rubidium, caesium, vanadium, chromium, iron, cobalt, nickel, ruthenium, rhodium, palladium, silver, osmium, iridium, platinum, gold, and cerium; 0 0; 1≦a≦3; 1≦b≦3; and 0
Abstract:
A coating precursor slurry is provided, along with its methods of formation and use. The coating precursor slurry may include an organic binder comprising a polymeric component and a hardening reagent; an inorganic binder comprising an aluminum-nitrogen compound, a barium-containing organic compound, a nickel-containing organic compound, an ammonia polyphosphate, and phosphorus pentoxide; active components comprising Mo, Te, and graphite; and a solvent.
Abstract:
A method for cracking hydrocarbon includes providing a feedstock comprising steam and hydrocarbon, and feeding the feedstock into a device having an inner surface accessible to the feedstock. The inner surface includes a compound of formula An+1BnO3n+1, wherein A includes at least one alkaline earth metal, B includes at least one transition metal, O is oxygen, and 1≤n≤20.
Abstract:
A method for converting carbon into a carbon oxide, comprises: contacting carbon with steam in presence of a carnegieite-like material of formula (Na2O)xNa2[Al2Si2O8], wherein 0
Abstract:
A method for converting carbon into a carbon oxide, comprises: contacting carbon with steam in presence of a carnegieite-like material of formula (Na2O)xNa2[Al2Si2)8], wherein 0
Abstract translation:一种将碳转化成碳氧化物的方法,包括:在碳酸钙类材料(Na 2 O)x Na 2 [Al 2 Si 2] 8]存在下使碳与蒸汽接触,其中0