Abstract:
The optical film with a pressure sensitive adhesive on both sides includes a first pressure sensitive adhesive layer having a thickness of 3 μm to 30 μm on first main surface of an optical film, and a second pressure sensitive adhesive layer having a thickness of 50 μm or more on second main surface of the optical film. A first protective sheet and a second protective sheet are releasably attached on the first pressure sensitive adhesive layer and the second pressure sensitive adhesive layer, respectively. The residual stress of the second pressure sensitive adhesive layer S2 (N/cm2), the thickness of the first protective sheet Y (μm); and the thickness of the second protective sheet Z (μm) satisfy the following relationship: 20≦Y≦80; 45≦Z; and Y+0.17 Z+10.6 S2≧63.
Abstract translation:具有两面的压敏粘合剂的光学膜包括在光学膜的第一主表面上具有3μm至30μm的厚度的第一压敏粘合剂层和厚度为50μm的第二压敏粘合剂层或 更多在光学膜的第二主表面上。 第一保护片和第二保护片分别可剥离地附接在第一压敏粘合剂层和第二压敏粘合剂层上。 第二压敏粘合剂层S2的残余应力(N / cm 2),第一保护片Y的厚度(μm); 并且第二保护片Z(μm)的厚度满足以下关系:20≦̸ Y≦̸ 80; 45≦̸ Z; Y + 0.17Z +10.6S2≥63。
Abstract:
The pressure sensitive adhesive of the present invention includes an acryl-based base polymer and a hydrogenated terpene phenolic resin having a softening point of 70° C. to 150° C. The hydrogenated terpene phenolic resin preferably has a terpene molar ratio of 0.1 to 0.7. The content of acryl-based base polymer is preferably 45 to 95 parts by weight based on total 100 parts by weight of the pressure sensitive adhesive composition. In addition, total content of the acryl-based base polymer and the hydrogenated terpene phenolic resin is preferably 70 parts by weight or more. The pressure sensitive adhesive of the present invention is hardly clouded even under a high-temperature and high-humidity environment, and has level difference followability, thus can be used by disposing between a front transparent plate and a touch panel, between a front transparent plate and an image display panel or between a touch panel and an image display panel.
Abstract:
Provided is a PSA sheet having a PSA layer. The PSA layer includes a layer A forming at least one surface thereof. The PSA sheet has an adhesive strength N0 of 2.0 N/10 mm or greater, after one day at room temperature following application of the layer A side to a surface of an alkaline float glass plate as an adherend having a contact angle of 5°-10° with distilled water; has an N1 to N0 reduction rate of 30% or lower, wherein N1 is a water-resistant adhesive strength measured after stored at room temperature for one day, immersed in water for 30 minutes, taken out from the water and then residual water is wiped off, and has an N2 to N0 reduction rate of 40% or higher, wherein N2 is a water-peel strength measured after stored at room temperature for one day, 20 μL distilled water is dropped onto the adherend and is allowed to enter a PSA layer/adherend interfacial edge. N2 is measured at a tensile speed of 300 mm/min at a peel angle of 180°.
Abstract:
Provided is a method for peeling a PSA sheet adhered on a polarizing plate. The PSA sheet has a PSA layer. The PSA layer includes a layer A forming at least one surface of the PSA layer. Of the polarizing plate, the surface to which the PSA sheet is adhered is corona-treated or plasma-treated. The peeling method includes a water-peel step in which the PSA sheet is peeled from the polarizing plate, in a state where an aqueous liquid exits at the interface between the polarizing plate and the PSA sheet at the front line of peeling the PSA sheet from the polarizing plate, with the aqueous liquid allowed to further enter the interface following the movement of the peel front line.
Abstract:
The pressure sensitive adhesive sheet is a sheet shaped pressure sensitive adhesive including an acryl-based base polymer. The acryl-based base polymer contains an acryl-based segment and a urethane-based segment, and a content of the urethane-based segment is 3 to 30 parts by weight based on 100 parts by weight of the acryl-based segment. The urethane-based segment includes at least one urethane chain selected from the group consisting of a polyether urethane and a polyester urethane. The content of the urethane-based segment other than the polyether urethane-based segment is 15 parts by weight or less based on 100 parts by weight of the acryl-based segment.
Abstract:
The optical film with pressure sensitive adhesive comprises an optical film and a front-side pressure sensitive adhesive sheet. The front-side pressure sensitive adhesive sheet is a laminated pressure sensitive adhesive sheet and includes a first pressure sensitive adhesive layer disposed in contact with the optical film, and a second pressure sensitive adhesive layer disposed at the furthest from the optical film. The first pressure sensitive adhesive layer has a storage elastic modulus of 9×103 Pa or less at 150° C., and a ratio G′20/G′150 of 20 or more, where G′20 is a storage elastic modulus at 20° C. and G′150 is a storage elastic modulus at 150° C. The second pressure sensitive adhesive layer has a storage elastic modulus of 4×105 Pa or less at 20° C., and a storage elastic modulus of 1×104 Pa or more at 150° C.
Abstract:
The present invention provides an optical pressure-sensitive adhesive sheet which can control the change in capacitance, which cause malfunction, when the optical pressure-sensitive adhesive sheet is applied to an optical member. The present invention provides an optical pressure-sensitive adhesive sheet including a pressure-sensitive adhesive layer, wherein a relative dielectric constant at a frequency of 1 MHz is 2 to 8, and a dielectric tangent at a frequency of 1 MHz is more than 0 and 0.2 or less.