Abstract:
The present invention relates to a water-resistant organic thin film obtained by crosslinking, with organic nitrogen compounds, an organic thin film comprising an organic dye having an anionic group, wherein the organic nitrogen compounds are first, second, and third acyclic organic nitrogen compounds each having two or more nitrogen atoms per molecule, wherein the nitrogen atoms of each of the first, second, and third organic nitrogen compounds are each in a cationic group, and the relation A≦0.4 nm
Abstract:
A method for manufacturing a water resistant optically anisotropic film capable of suppressing the generation of a defect such as a crack or separation is provided. The method for manufacturing the water resistant optically anisotropic of the present invention includes a water resistant treatment step of bringing an optically anisotropic film containing an organic dye having an anionic group into contact with a water resistant treatment liquid containing a multivalent cationic compound and a monovalent cationic compound, and the mass ratio of the multivalent cationic compound and the monovalent cationic compound contained in the water resistant treatment liquid, monovalent cationic compound/multivalent cationic compound, is 0.01 to 2.
Abstract:
A pressure-sensitive adhesive sheet comprises a support and a transparent pressure-sensitive adhesive layer on the support. The pressure-sensitive adhesive layer comprises a base adhesive zone made essentially of a transparent base pressure-sensitive adhesive material and formed over a given range from a first principal surface of the pressure-sensitive adhesive layer in a thickness direction of the pressure-sensitive adhesive layer, and a transparent, adherent, refractive index-adjusting zone formed over a given range from a second principal surface of the pressure-sensitive adhesive layer in the thickness direction, and wherein the refractive index-adjusting zone has a refractive index greater than a refractive index of the base pressure-sensitive adhesive material.
Abstract:
Provided are a double-sided transparent conductive film which has blocking resistance and a low reflectance, and is inhibited from scattering reflected light to exhibit good visibility; a roll thereof; and a touch panel. The double-sided transparent conductive film of the present invention includes a base material film with an optical adjusting layer laminate and a transparent conductive layer formed in this order on each of both sides, the optical adjusting layer laminate including two or more optical adjusting layers, wherein the optical adjusting layers have different refractive indexes in each of the optical adjusting layer laminates, an anti-blocking layer containing particles is formed between the base material film and at least one of the optical adjusting layer laminates, the anti-blocking layer includes a flat portion, and a protrusion portion resulting from the particles, a value obtained by subtracting a value of a thickness of the flat portion of the anti-blocking layer from a value of a mode diameter of the particles is larger than a value of a thickness of the optical adjusting layer laminate, and the optical adjusting layer laminates each have a thickness of not less than 60 nm and not more than 250 nm.
Abstract:
A double-sided transparent conductive film including a base material film, having an anti-blocking layer, an optical adjusting layer and a transparent conductive layer formed in this order on each of both sides of the base material film, wherein an anti-blocking layer containing particles is formed at least one of: a location between the base material film and one optical adjusting layer; and a location between the base material film and the other optical adjusting layer, the anti-blocking layer has a flat portion and protrusion portions caused by the particles, and a value obtained by subtracting a thickness of the flat portion of the anti-blocking layer from a mode diameter of the particles is larger than a thickness of the optical adjusting layer.
Abstract:
A touchscreen sensor includes a transparent base material, a first index-matching layer, a first transparent electrode pattern, a second index-matching layer and a first adhesive layer disposed in this order at one side of the transparent base material, and a third index-matching layer, a second transparent electrode pattern, a fourth index-matching layer and a second adhesive layer disposed in this order at another side of the transparent base material. Each of the first, second, third and fourth index-matching layers has a refractive index of 1.6 to 1.8 and a thickness of 50 nm to 150 nm.
Abstract:
A touchscreen sensor includes a transparent base material, a first transparent electrode pattern, a first index-matching layer and a first adhesive layer disposed in this order at one side of the transparent base material, and a second transparent electrode pattern, a second index-matching layer and a second adhesive layer disposed in this order at another side of the transparent base material. The first index-matching layer has a refractive index greater than a refractive index of the first adhesive layer. The second index-matching layer has a refractive index greater than a refractive index of the second adhesive layer. Each of the first index-matching layer and the second index-matching layer has a thickness of 85 nm to 120 nm.
Abstract:
Provided are a double-sided transparent conductive film which is good in appearance even when its transparent conductive layers are patterned, and has anti-blocking property, thereby being producible at low costs; a wound body thereof; and a touch panel. The double-sided transparent conductive film includes a base material film, and a base material film, and an optical adjusting layer and a transparent conductive layer which are formed in this order on each of both sides of the base material film, wherein an anti-blocking layer containing particles is formed at least one of: a location between the base material film and one optical adjusting layer; and a location between the base material film and the other optical adjusting layer, the anti-blocking layer has a flat portion and protrusion portions caused by the particles, and a value obtained by subtracting a thickness of the flat portion of the anti-blocking layer from a mode diameter of the particles is larger than a thickness of the optical adjusting layer.