MAGNETIC ALLOY RIBBON, LAMINATE, AND MAGNETIC CORE

    公开(公告)号:US20230085009A1

    公开(公告)日:2023-03-16

    申请号:US17893502

    申请日:2022-08-23

    Abstract: A specific depth at which a concentration of Fe reaches 10 at % is 18 nm or more and 500 nm or less from the first surface, and from the first surface to the specific depth, the concentration of Fe is less than 10 at %, and a positive increase region is present in which the concentration of Fe increases with a substantially positive concentration gradient, in a case where the concentration of Fe is measured in a depth direction from a first surface of a ribbon.

    MAGNETIC CORE, METHOD OF MANUFACTURING SAME, AND COIL COMPONENT

    公开(公告)号:US20210005364A1

    公开(公告)日:2021-01-07

    申请号:US16977738

    申请日:2019-03-01

    Abstract: A magnetic core and the like having a stable soft magnetic property, including a plurality of soft magnetic layers which are laminated, wherein a crack is formed in the soft magnetic layers. The soft magnetic layers include Fe as a principal component. The soft magnetic layers include a composition formula (Fe(1−(α+β))X1αX2β)(1−(a+b+c+d+e+f))MaBbPcSidCeSf, wherein: X1 is one or more selected from the group consisting of Co and Ni, X2 is one or more selected from the group consisting of Al, Mn, Ag, Zn, Sn, As, Sb, Cu, Cr, Bi, N, and O and rare-earth elements, M is one or more selected from the group consisting of Nb, Hf, Zr, Ta, Mo, V, and W; and a to f and α and β are in predetermined ranges. A structure including a nanoheterostructure or an Fe-group nanocrystal is observed in the soft magnetic layers.

Patent Agency Ranking