POLYOLEFINS COMPOSITIONS OBTAINED FROM RECYCLED POLYOLEFINS

    公开(公告)号:US20230250266A1

    公开(公告)日:2023-08-10

    申请号:US18013481

    申请日:2021-06-17

    CPC classification number: C08L23/12 C08L2205/03

    Abstract: A polypropylene composition made from or containing:

    (a) 65 to 85 weight % of a crystalline propylene polymer having an amount of isotactic pentads (mmmm), measured by 13C-MNR on the fraction insoluble in xylene at 25° C. higher than 97.0 molar% and a polydispersity index from 3 to 15;
    (b) 5 to 25 weight % of an elastomeric copolymer of ethylene and propylene, having an amount of recurring units deriving from ethylene ranging from 30 to 70 weight %, and being partially soluble in xylene at ambient temperature; wherein the fraction soluble in xylene at ambient temperature having an intrinsic viscosity value from 3 to 10 dl/g; and
    (c) 5 to 25 weight % of recycled polyethylene (r-PE) having a melt flow rate (190° C./2.16 Kg) from 0.1 to 10 g/10 min,

    wherein the polypropylene composition having a melt flow rate (ISO 1133 230° C./2.16 kg) higher than 3.0 to 15 g/10 min.

    PROPYLENE POLYMER COMPOSITION
    243.
    发明公开

    公开(公告)号:US20230151196A1

    公开(公告)日:2023-05-18

    申请号:US17911938

    申请日:2021-03-08

    Inventor: DAVIDE TARTARI

    CPC classification number: C08L23/12 C08L2205/025 C08L2203/30

    Abstract: A polypropylene composition made from or containing:

    A) From 96 wt % to 80 wt %; of a propylene homopolymer having a fraction insoluble in xylene at 25° C. greater than 90 wt %, based upon the total weight of the propylene homopolymer; and a melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg between 80.0 g/10 min and 300.0 g/10 min; and
    B) From 4 wt % to 20 wt %; of a propylene ethylene copolymer having an ethylene derived units content ranging from 18 wt % to 38 wt %, based upon the total weight of the propylene ethylene copolymer;
    wherein the polypropylene composition having:
    a melt flow rate, MFR, measured according to ISO 1133 at 230° C. with a load of 2.16 kg, between 80.0 g/10 min and 150.0 g/10 min;
    the sum of the amounts of A) and B) being 100 wt %.

    IMPROVED ASPHALT MATERIAL
    245.
    发明申请

    公开(公告)号:US20230118146A1

    公开(公告)日:2023-04-20

    申请号:US17915426

    申请日:2021-04-19

    Abstract: Asphalt product made from or containing Z1) from 90 wt % to 98 wt % of mineral aggregate; and Z2) from 2 wt % to 10 wt % of a bitumen composition made from or containing T1) from 99 wt % to 75 wt % of bitumen, and T2) from 1 wt % to 25 wt % of a polymer composition made from or containing A) 5-35% by weight of a propylene homopolymer; B) 20-50% by weight of an ethylene homopolymer; and C) 30-60% by weight of a terpolymer of ethylene, propylene and 1-butene derived units.

    COMPOSITIONS OBTAINED FROM RECYCLED POLYOLEFINS

    公开(公告)号:US20230099166A1

    公开(公告)日:2023-03-30

    申请号:US17801310

    申请日:2021-02-04

    Abstract: A polypropylene composition made from or containing: T1) 35-65 wt % of a recycled polypropylene mixture containing at least 80 wt % of rigid polypropylene items and having a purity of at least 90 wt %; T2) 20-50 wt % of an ethylene/propylene copolymer; T3) 5-20 wt % of a propylene/ethylene heterophasic copolymer composition made from or containing a) from 12 wt % to 52 wt % of a propylene homopolymer or a propylene/ethylene copolymer; and b) from 48 wt % to 88 wt % of a propylene/ethylene copolymer having a content of ethylene derived units ranging from 15 wt % to 42 wt %; wherein the propylene composition has a melt flow rate (ISO 1133 230° C./2.16 kg) ranging from 0.5 to 20 g/10 min.

    CATATLYST COMPONENTS FOR THE POLYMERIZATION OF OLEFINS

    公开(公告)号:US20220332856A1

    公开(公告)日:2022-10-20

    申请号:US17620968

    申请日:2020-06-24

    Abstract: A solid catalyst component for the polymerization of olefins made from or containing Mg, Ti and an electron donor of formula (I) where the R1 and R5 groups, equal to or different from each other, are selected from C1-C15 hydrocarbon groups, R2 group is selected from C2-C10 hydrocarbon groups, R3 to R4 groups, independently, are selected from hydrogen or C1-C20 hydrocarbon groups, optionally fused together to form one or more cycles, with the proviso that at least one of R3 to R4 groups is a C1-C20 alkyl group.

    CORE-SKIN FIBER COMPRISING PROPYLENE ETHYLENE RANDOM COPOLYMER

    公开(公告)号:US20220251745A1

    公开(公告)日:2022-08-11

    申请号:US17617427

    申请日:2020-05-26

    Abstract: A skin-core fiber having a skin of a propylene ethylene copolymer having: i) xylene soluble fraction from 14 wt % to 27 wt %; ii) intrinsic viscosity of the fraction soluble in xylene at 25° C. from 1.0 to 2.4 dl/g; iii) melt flow rate, MFR, from 12 g/10 min to 60 g/10 min; iv) an ethylene derived units content from 5.0 wt % to 12.0 wt %; v) the ethylene derived units content of the fraction insoluble in xylene from 2.5 wt % to 6.0 wt %; vi) the ethylene derived units content of the fraction soluble in xylene ranging from 15.2. wt % to 30.2 wt %; vii) C13 NMR sequences PEP on the fraction insoluble in xylene from 3.5 mol % to 5.5 mol %; and viii) C13 NMR sequences PEP on the fraction soluble in xylene from 11.0 mol % to 14.2 mol %; and a core of a polyethylene having a density between 0.940 g/cm3 to 0.975 g/cm3.