Abstract:
An ethylene-based polymer, e.g., LDPE, with a low dissipation factor is made by a process comprising the step of contacting at polymerization conditions ethylene and, optionally, one or more comonomers, e.g., an alpha-olefin, with at least one carbon-carbon (C—C) hydrocarbyl, free-radical initiator of Structure 1: wherein R1, R2, R3, R4, R5 and R6, are each, independently, hydrogen or a hydrocarbyl group and wherein, optionally, two or more R groups (R1, R2, R3, R4, R5 and R6) form a ring structure, with the provisos that at least one of R2 and R5, and at least one of R3 and R6 is a hydrocarbyl group of at least two carbon atoms, e.g., an alkaryl of at least seven carbon atoms.
Abstract:
Disclosed is an ethylene-based polymer with a density from about 0.90 to about 0.94 in grams per cubic centimeter, with a molecular weight distribution (Mw/Mn) from about 2 to about 30, a melt index (I2) from about 0.1 to about 50 grams per 10 minutes, and further comprising sulfur from about 5 to about 4000 parts per million. The amount of sulfur is also determined based upon the total weight of the ethylene-based polymer. Also disclosed is process for making an ethylene-based polymer which includes the steps of splitting a process fluid for delivery into a tubular reactor; feeding an upstream process feed stream into a first reaction zone and at least one downstream process feed stream into at least one other reaction zone, where the process fluid has an average velocity of at least 10 meters per second; and initiating a free-radical polymerization reaction.
Abstract:
An insulated wire or cable is made by a process comprising the steps of: (A) extruding onto a covered or uncovered metal conductor or optical fiber a composition having a DF measured at 130° C. (60 Hz, 2 kV) or 120° C. (60 Hz, 8 kV) or 100° C. (60 Hz, 8 kV) of
Abstract:
A process to form an ethylene-based polymer comprising, in polymerized form, ethylene and at least one acid comonomer, said process comprising polymerizing a reaction mixture comprising the ethylene and the acid comonomer, in a reactor configuration comprising at least one Secondary compressor, at least one pressurization device, and at least one reactor selected from the following: at least one autoclave reactor, at least one tubular reactor, or a combination thereof; and wherein the reaction mixture is polymerized in the presence of at least one free-radical initiator, and at a pressure of at least 1000 Bar; and wherein at least a portion of a comonomer composition comprising at least a portion of the acid comonomer used in the polymerization, is compressed, to form a compressed comonomer composition, in the pressurization device, up to a discharge pressure ranging from 1000 Bar to 4000 Bar, and at a discharge temperature (DT) from 10 C to 100 C; and wherein the compressed comonomer composition bypasses the Secondary compressor, and is fed, downstream from the Secondary compressor, into the reactor, and/or into one or more feed streams to the reactor.
Abstract:
The invention provides a process to form an ethylene-based polymer, said process comprising polymerizing ethylene and at least one asymmetrical polyene, comprising an “alpha, beta unsaturated—carbonyl end” and a “C—C double bond end,” and wherein the polymerization takes place in the presence of at least one free-radical initiator, and wherein the polymerization takes place in a reactor configuration comprising at least two reaction zones, reaction zone I and reaction zone i (i>2), wherein reaction zone I is downstream from reaction zone I; and wherein at least one chain transfer agent (CTA) is added to the polymerization, and wherein the CTA is a saturated hydrocarbon or an unsaturated hydrocarbon.
Abstract:
A composition comprising an ethylene-based polymer, the ethylene-based polymer having the following properties: a) at least one incorporated structure derived from a polyene selected from the group consisting of i) through x), as described herein; N and b) a Mw(abs) versus I2 relationship: Mw(abs)
Abstract:
A process to form an ethylene-based polymer including polymerizing ethylene and at least one asymmetrical polyene comprising an “alpha, beta unsaturated-carbonyl end” (“α,β unsaturated-carbonyl end”) and a “C—C double bond end,” wherein the polymerization takes place in the presence of at least one free-radical initiator; and wherein the polymerization takes place in a reactor configuration comprising at least two reaction zones, reaction zone 1 and reaction zone i (i≧2), wherein reaction zone i is downstream from reaction zone 1.
Abstract:
An ethylenic polymer comprising amyl groups from about 0.1 to about 2.0 units per 1000 carbon atoms as determined by Nuclear Magnetic Resonance and both a peak melting temperature, Tm, in ° C., and a heat of fusion, Hf, in J/g, as determined by DSC Crystallinity, where the numerical values of Tm and Hf correspond to the relationship Tm≧(0.2143*Hf)+79.643. An ethylenic polymer comprising at least one preparative TREF fraction that elutes at 95° C. or greater using a Preparative Temperature Rising Elution Fractionation method, where at least one preparative TREF fraction that elutes at 95° C. or greater has a gpcBR value greater than 0.05 and less than 5 as determined by gpcBR Branching Index by 3D-GPC, and where at least 5% of the ethylenic polymer elutes at a temperature of 95° C. or greater based upon the total weight of the ethylenic polymer.