The present invention relates to a recording apparatus that includes a recording head capable of performing dot recording, a main scanner for scanning the recording head, and a data storage for storing data sent from a host computer. The apparatus can make a record according to stored data by performing a plurality of main scans, and further comprises a restorer for restoring data, which has been subjected to given processing by the host computer, to another data in line with the given processing. The present invention further relates to a record data processing method. According to the present invention, an amount of sent data to be held can be reduced by reducing an amount of data to be transferred from the host computer. Moreover, a record with irregular concentration suppressed can be made in substantially the same recording area by performing a plurality of rounds of main scan as conventionally, while a reduction in cost can be achieved.
摘要:
A high strength hot-rolled steel sheet has a tensile strength of not less than 780 MPa and exhibits excellent stretch flangeability and excellent fatigue resistance. A steel has a composition containing C at 0.05 to 0.15%, Si at 0.2 to 1.2%, Mn at 1.0 to 2.0%, P at not more than 0.04%, S at not more than 0.005%, Ti at 0.05 to 0.15%, Al at 0.005 to 0.10% and N at not more than 0.007%.
摘要:
A steel having a composition that includes C: 0.05 to 0.15%, Si: 0.2 to 1.2%, Mn: 1.0 to 2.0%, Al: 0.005 to 0.10%, N: 0.006% or less, and at least one selected from Ti: 0.03 to 0.13%, Nb: 0.02 to 0.10%, and V: 0.02 to 0.15% is subjected to rough rolling at a reduction of 80% or more and finish rolling at a finish rolling delivery temperature in the range of 800 to 950° C. The finish rolled sheet is subjected to cooling including cooling the finish rolled sheet from the finish rolling delivery temperature to a cooling end temperature in the range of 550 to 610° C. at an average cooling rate of 25° C./sec. or more and cooling the finish rolled sheet from the cooling end temperature of the previous process to a coiling temperature at an average cooling rate of 100° C./sec. or more.
摘要:
A body structure for rolling stock is disclosed. The body structure may include an outside sheathing of a side construction, and a plurality of reinforcement members joined to said outside sheathing interiorly of said outside sheathing. Each of said plurality of reinforcement members may include a U-shaped part which is substantially U-shaped in cross-section and two fitting flange parts extending continuously from end edges of the U-shaped part in opposite directions. The fitting flange parts may be joined to said outside sheathing by laser welding, and the U-shaped part of at least one of said plurality of reinforcement members may be smaller in width than the U-shaped part of another of said plurality of reinforcement members provided on another part of said outside sheathing.
摘要:
A laser-welding head is capable of applying a fixed pressure to parts to be welded of workpieces regardless of the undulation of the surfaces of the parts to be welded. The laser-welding head includes a pressing device (12) having a roller (16) which rolls along parts of workpieces near a weld line (40) to press together the same parts of the workpieces, a pressing unit (6) for applying a predetermined pressure to the pressing device (12) to press the pressing device (12) toward the parts of the workpieces near the weld line (40), and a laser beam projecting unit (17) mounted on the pressing unit (6) for movement together with the pressing device (12). The pressing unit (6) is provided with a pneumatic cylinder actuator for applying the predetermined pressure to the pressing device (12).
摘要:
This invention has as its object to improve the net processing speed by appropriately assigning the DMA processing time for attaining high-speed processing using hardware, and the software execution time of a CPU. By interrupting the operation of one of a CPU and a DMA processor only when a device such as an external D-RAM shared by processors such as the CPU, DMA processor, and the like, is to be accessed, the CPU operation and the DMA processing are substantially parallelly executed, thereby improving the net processing speed.
摘要:
Provided is a consumable electrode type arc welding method and device in which stable welding can be performed at a high speed for a welding gap greater than a thickness of a base metal and the like, and welding conditions are automatically changed according to the welding gap along a welding line to perform the stable welding. A first base metal extended vertically and a second base metal which has an upper end positioned in a middle portion of the first base metal and is provided along the first base metal are welded together. The first and second base metals have a thickness of 2.8 mm, and an arc is generated toward an upper end portion of the second base metal from obliquely above on a side opposite to the first base metal. The second base metal is melted to be a part of a weld metal. An amount of the second base metal to be melted is increased or decreased according to a welding gap detected by a laser sensor.
摘要:
A steel sheet including C at 0.05 to 0.15%, Si at 0.2 to 1.2%, Mn at 1.0 to 2.0%, P at not more than 0.04%, S at not more than 0.0030%, Al at 0.005 to 0.10%, N at not more than 0.005% and Ti at 0.03 to 0.13%, the balance being Fe and inevitable impurities, includes surface regions having an area fraction of bainite of less than 80% and an area fraction of a ferrite phase with a grain diameter of 2 to 15 μm of not less than 10%, the surface regions extending from both surfaces of the steel sheet each to a depth of 1.5 to 3.0% relative to a total sheet thickness, as well as an inner region other than the surface regions having an area fraction of a bainite phase of more than 95%, and has a tensile strength of not less than 780 MPa.
摘要:
A steel sheet including C at 0.05 to 0.15%, Si at 0.2 to 1.2%, Mn at 1.0 to 2.0%, P at not more than 0.04%, S at not more than 0.0030%, Al at 0.005 to 0.10%, N at not more than 0.005% and Ti at 0.03 to 0.13%, the balance being Fe and inevitable impurities, includes surface regions having an area fraction of bainite of less than 80% and an area fraction of a ferrite phase with a grain diameter of 2 to 15 μm of not less than 10%, the surface regions extending from both surfaces of the steel sheet each to a depth of 1.5 to 3.0% relative to a total sheet thickness, as well as an inner region other than the surface regions having an area fraction of a bainite phase of more than 95%, and has a tensile strength of not less than 780 MPa.
摘要:
A side construction 302 has an outside sheathing 306 and outside sheathing reinforcement members 307A and 307B joined to the outside sheathing 306 interiorly of the outside sheathing 306. The reinforcement member 307A (307B) is shaped like a hat in section. The reinforcement members 307A provided in the vicinity of a window opening portion have a laser welding spacing L1 of 80 mm and each have a hat width of 50 mm, while the reinforcement members 307B provided on other part have a laser welding spacing L1 of 100 mm and each have a hat width of 70 mm. The reinforcement members 307A and 307B each have a height of 25 mm.