公开(公告)号:US20210147587A1
公开(公告)日:2021-05-20
申请号:US16633191
申请日:2018-08-03
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: ROBERTA MARCHINI , STEFANO SPATARO , ROBERTA PICA
IPC: C08F10/08 , C09J123/20
Abstract: A butene-1 polymer having: a) a Melt Flow Rate value of from 100 to 300 g/10 min., measured according to ISO 1133 at 190° C. with a load of 2.16 kg; b) an intrinsic viscosity (IV) measured in tetrahydronaphthalene (THN) at 135° C. equal to lower than 0.70 dl/g; c) a Mw/Mn value equal to or lower than 2.8 and a lower limit of 1.5; d) a Mz value of 90,000 g/mol or higher; and e) optionally, a comonomer content of up to 10% by mole.
-
公开(公告)号:US10894849B2
公开(公告)日:2021-01-19
申请号:US15750123
申请日:2016-07-19
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Paola Massari , Fabrizio Piemontesi , Gianni Vitale , Caroline Cathelin , Giampiero Morini , Claudio Cavalieri , Marco Ciarafoni , Roberto Pantaleoni
IPC: C08J9/00 , C08F210/06 , C08J5/18 , C08L23/14
Abstract: A polyolefin composition made from or containing: A) from about 19 wt % to about 50 wt % of a propylene ethylene copolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt % B) from about 50 wt % to about 81 wt % of a propylene ethylene 1-butene terpolymer having an ethylene derived units content ranging from about 1.5 wt % to about 6.0 wt % and 1-butene derived units content between about 4.8 wt % and about 12.4 wt %; the sum of the amount of component A) and B) being 100; the polyolefin composition being characterized by the following features: molecular weight distribution (MWD), expressed in terms of Mw/Mn, greater than about 4.0; the creep and recovery curve measured on the polymer fuse at 200° C. shows a maximum value between 600 and 1200 seconds, lower than about 53×10−4 1/Pa.
-
公开(公告)号:US20200339796A1
公开(公告)日:2020-10-29
申请号:US16758758
申请日:2018-11-05
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: ROBERTO DE PALO , CLAUDIO CAVALIERI
Abstract: A polyolefin composition made from or containing:T1) 70-95 wt %, a polyolefin component containing: a1) from 30 wt % to 70 wt % of a propylene based polymer; and a2) from 30 wt % to 70 wt % of an ethylene based polymer; the sum of a1) and a2), being referred to the total weight of a1) and a2), being 100; and T2) 5-30 wt % of a propylene ethylene copolymer containing from 2.0 wt % to 10.0 wt %; of ethylene derived units and having a melt flow rate (230° C./2.16 kg) ranging from 0.5 to 20.0 g/10 min, and having a fraction soluble in xylene at 25° C. lower than 20 wt %. the sum of the amount of T1) and T2), being referred to the total weight of T1) and T2), being 100.
-
公开(公告)号:US10767036B2
公开(公告)日:2020-09-08
申请号:US16629104
申请日:2018-06-20
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Monica Galvan , Claudio Cavalieri , Jaume Marti Porqueres , Renaud Lemaire , Roberto De Palo
Abstract: A polyolefinic fiber made from or containing from 2 wt % to 20 wt % relative to the total weight of the fiber of a polyolefin composition made from or containing: A) 5-35% by weight of a propylene homopolymer or a propylene ethylene copolymer; B) 20-50% by weight of a copolymer of ethylene and a C3-C8 alpha-olefin containing from 0.1% to 20% by weight of alpha-olefin units and containing 25% by weight or less of a fraction soluble in xylene at 25° C.; and C) 30-60% by weight of a copolymer of ethylene and propylene containing from 25% to 75% by weight of ethylene units and containing from 40% to 95% by weight of a fraction soluble in xylene at 25° C.; the amounts of (A), (B) and (C) being referred to the total weight of (A)+(B)+(C), the sum of the amount of (A)+(B)+(C) being 100.
-
公开(公告)号:US20200263013A1
公开(公告)日:2020-08-20
申请号:US16758767
申请日:2018-11-05
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: ROBERTO DE PALO , CLAUDIO CAVALIERI
Abstract: A polyolefin composition made from or containing: T1) 70-95 wt %, a polyolefin component containing: a1) from 30 wt % to 70 wt % of a propylene based polymer; and a2) from 30 wt % to 70 wt % of an ethylene based polymer; and T2) 5-30 wt % of an heterophasic propylene ethylene copolymer.
-
公开(公告)号:US20200255609A1
公开(公告)日:2020-08-13
申请号:US16758763
申请日:2018-10-31
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: PAOLA MASSARI , ANDREA FELISATI , MARCO IZZI , PAOLO BASSI , CLAUDIO CAVALIERI
IPC: C08J5/18
Abstract: A heat-shrinkable label made from or containing a terpolymer film containing propylene, ethylene and 1-hexene, wherein the terpolymer has: (i) a content of ethylene derived units ranging from 0.5 wt % to 5.0 wt %, (ii) a content of 1-hexene derived units ranging from 1.0 wt % to 6.0 wt %, (iii) a melt flow rate (MFR) (ISO 1133 230° C., 2.16 kg) ranging from 0.5 to 20 g/10 min, and (iv) a polydispersity index (P.I.) ranging from 2.0 to 7.0.
-
公开(公告)号:US20200231723A1
公开(公告)日:2020-07-23
申请号:US16632175
申请日:2018-07-03
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: PAOLA MASSARI , CAROLINE CATHELIN , CLAUDIO CAVALIERI , MARCO CIARAFONI , ROBERTO PANTALEONI , GIAMPIERO MORINI , GIANNI VITALE , FABRIZIO PIEMONTESI , GIANNI COLLINA , BENEDETTA GADDI
IPC: C08F210/06 , C08J5/18
Abstract: A propylene 1-hexene copolymer containing from 5.7 to 7.7% by weight of 1-hexene derived units, based upon the total weight of the propylene 1-hexene copolymer, having:a) a solubility in xylene at 25° C. ranging from 7.0 wt % to 15.0 wt %, based upon the total weight of the propylene 1-hexene copolymer; b) a melting temperature, measured by DSC ranging from 143.0° C. to 148.0° C.; c) a Melt Flow Rate (MFR, measured according to ASTM D 1238, 230° C./2.16 kg) from 3.5 to 8.0 g/10 min.; and d) a content of 1-hexene derived units in the fraction soluble in xylene at 25° C. ranging from 13.5 wt % to 18.5 wt %, based upon the total weight of the soluble fraction.
-
358.
公开(公告)号:US20200231716A1
公开(公告)日:2020-07-23
申请号:US16647766
申请日:2018-09-07
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: DIEGO BRITA , NICOLO ARICH DE FINETTI , OFELIA FUSCO , BENEDETTA GADDI
Abstract: A process for the preparation of a solid catalyst component for the polymerization of CH2═CHR olefins, wherein R is hydrogen or hydrocarbyl radical with 1-12 carbon atoms, made from or containing a Ti compound on a Mg chloride based support, including the steps of (a) reacting a Mg based compound with a liquid medium made from or containing a Ti compound, at a temperature ranging from 0 to 150° C., thereby yielding solid particles; and (b) suspending the solid particles coming from step (a) in a liquid medium made from or containing hydrocarbons at a temperature ranging from 10 to 100° C., wherein step (a) or (b) is carried out in the presence of 0.2 to 20.0% by weight, with respect to the amount of Mg compound, of particles of a solid compound containing more than 50% by weight of SiO2 units and having average particle size from 1 to 100 μm.
-
公开(公告)号:US20200216588A1
公开(公告)日:2020-07-09
申请号:US16649044
申请日:2018-09-13
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: ANTONIO MAZZUCCO , ENRICO BALESTRA , ROBERTO PANTALEONI , DAVIDE TARTARI , RICCARDO RINALDI
IPC: C08F210/06 , B01J8/26 , B01J8/22
Abstract: A process for the polymerization of olefins in gas phase carried out in a reactor having two interconnected polymerization zones, a first zone (riser) and a second zone (downcomer), wherein growing polymer particles: a) flow through the riser under fast fluidization conditions established by feeding a mixture of gas and liquid; b) leave the riser and enter the downcomer, through which the growing polymer particles flow downward in a densified form; and c) leave the downcomer and are reintroduced into the riser, thereby establishing a circulation of polymer between the riser and the downcomer; the reactor is operated at a temperature between 0° C. and 5° C. above the dew point of the riser gas at the operating pressure, and in the riser, besides the growing polymer particles and gas flow, an amount of liquid is present.
-
公开(公告)号:US10661540B2
公开(公告)日:2020-05-26
申请号:US16301799
申请日:2017-05-09
Applicant: BASELL POLIOLEFINE ITALIA S.R.L.
Inventor: Monica Galvan , Gianni Perdomi , Claudio Cavalieri
Abstract: The disclosure provides a multilayer blown film for stretch hood made from or containing a layer made from or containing a first polyolefin composition made from or containing from 20 wt % to 80 wt %, based upon the total weight of the first polyolefin composition, of Component A) and from 20 wt % to 80 wt %, based upon the total weight of the first polyolefin composition, of Component B); wherein Component A) is an ethylene copolymer and Component B) is a polyolefin composition made from or containing: (i) 5-35% by weight, based upon the total weight of Component B, of a propylene homopolymer or a propylene ethylene copolymer (ii) 20-50% by weight, based upon the total weight of Component B, of a copolymer of ethylene and a C3-C8 alpha-olefin; and (iii) 30-60% by weight, based upon the total weight of Component B, of a copolymer of ethylene and propylene.
-
-
-
-
-
-
-
-
-